GLASS FOR CHEMICAL STRENGTHENING AND METHOD FOR MANUFACTURING GLASS FOR CHEMICAL STRENGTHENING, AND CHEMICALLY STRENGTHENED GLASS AND IMAGE DISPLAY DEVICE PROVIDED WITH SAME

A glass for chemical strengthening that is a float-formed glass for chemical strengthening includes, as represented by mass percentage based on oxides, from 65 to 72% of SiO2, from 3.6 to 8.6% of Al2O3, from 3.3 to 6% of MgO, from 6.5 to 9% of CaO, from 13 to 16% of Na2O and from 0 to 0.9% of K2O. I...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MIURA Takenori, KASE Junichiro, MIYASAKA Junko, KAWAKAMI Masamichi
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A glass for chemical strengthening that is a float-formed glass for chemical strengthening includes, as represented by mass percentage based on oxides, from 65 to 72% of SiO2, from 3.6 to 8.6% of Al2O3, from 3.3 to 6% of MgO, from 6.5 to 9% of CaO, from 13 to 16% of Na2O and from 0 to 0.9% of K2O. In the glass for chemical strengthening, (Na2O+K2O)/Al2O3 is from 2.2 to 5. The glass for chemical strengthening has a sheet thickness (t) of 0.1 mm or more and 2 mm or less. A SnO2 amount of a bottom surface in an unpolished state of the glass for chemical strengthening is 6.2 μg/cm2 or less (0.1≦t≦1 mm) or (2t+4.2) μg/cm2 or less (1