COMPOSITE BALLISTIC RESISTANT LAMINATE

An unconsolidated impact and penetration resistant laminate comprises a plurality of cross-plied sheets, each cross-plied sheet further comprising (i) first and second layers of fibrous or non-fibrous ultra-high molecular weight polyethylene and (ii) first and second layers of thermoplastic adhesive...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KAMPERT William George, SAUER Bryan Benedict, SINGLETARY James Neal, LIBERT Timothy A, CARBAJAL Leopoldo Alejandro
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KAMPERT William George
SAUER Bryan Benedict
SINGLETARY James Neal
LIBERT Timothy A
CARBAJAL Leopoldo Alejandro
description An unconsolidated impact and penetration resistant laminate comprises a plurality of cross-plied sheets, each cross-plied sheet further comprising (i) first and second layers of fibrous or non-fibrous ultra-high molecular weight polyethylene and (ii) first and second layers of thermoplastic adhesive, each adhesive layer having a basis weight of no greater than 5 gsm, wherein (a) the layers of polyethylene and thermoplastic adhesive alternate within the sheet, (b) at least 50 percent of the polyethylene layers are arranged such that the orientation of the first polyethylene layer is offset with respect to the orientation of the second polyethylene layer, and (c) the plurality of cross-plied sheets form a stack that, when subjected to compaction at a pressure of 255 bar and a temperature of 132 degrees C., will not suffer a pressure loss greater than 8 bar within the first two minutes as measured by Test Method B.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2016265882A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2016265882A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2016265882A13</originalsourceid><addsrcrecordid>eNrjZFBz9vcN8A_2DHFVcHL08fEMDvF0VghyDQYyHP1CFHwcfT39HENceRhY0xJzilN5oTQ3g7Kba4izh25qQX58anFBYnJqXmpJfGiwkYGhmZGZqYWFkaOhMXGqAGvOJMM</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>COMPOSITE BALLISTIC RESISTANT LAMINATE</title><source>esp@cenet</source><creator>KAMPERT William George ; SAUER Bryan Benedict ; SINGLETARY James Neal ; LIBERT Timothy A ; CARBAJAL Leopoldo Alejandro</creator><creatorcontrib>KAMPERT William George ; SAUER Bryan Benedict ; SINGLETARY James Neal ; LIBERT Timothy A ; CARBAJAL Leopoldo Alejandro</creatorcontrib><description>An unconsolidated impact and penetration resistant laminate comprises a plurality of cross-plied sheets, each cross-plied sheet further comprising (i) first and second layers of fibrous or non-fibrous ultra-high molecular weight polyethylene and (ii) first and second layers of thermoplastic adhesive, each adhesive layer having a basis weight of no greater than 5 gsm, wherein (a) the layers of polyethylene and thermoplastic adhesive alternate within the sheet, (b) at least 50 percent of the polyethylene layers are arranged such that the orientation of the first polyethylene layer is offset with respect to the orientation of the second polyethylene layer, and (c) the plurality of cross-plied sheets form a stack that, when subjected to compaction at a pressure of 255 bar and a temperature of 132 degrees C., will not suffer a pressure loss greater than 8 bar within the first two minutes as measured by Test Method B.</description><language>eng</language><subject>ARMOUR ; ARMOURED OR ARMED VEHICLES ; ARMOURED TURRETS ; BLASTING ; HEATING ; INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES ; LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; LIGHTING ; MEANS OF ATTACK OR DEFENCE, e.g. CAMOUFLAGE, IN GENERAL ; MEASURING ; MECHANICAL ENGINEERING ; PERFORMING OPERATIONS ; PHYSICS ; TESTING ; TRANSPORTING ; WEAPONS</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160915&amp;DB=EPODOC&amp;CC=US&amp;NR=2016265882A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160915&amp;DB=EPODOC&amp;CC=US&amp;NR=2016265882A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KAMPERT William George</creatorcontrib><creatorcontrib>SAUER Bryan Benedict</creatorcontrib><creatorcontrib>SINGLETARY James Neal</creatorcontrib><creatorcontrib>LIBERT Timothy A</creatorcontrib><creatorcontrib>CARBAJAL Leopoldo Alejandro</creatorcontrib><title>COMPOSITE BALLISTIC RESISTANT LAMINATE</title><description>An unconsolidated impact and penetration resistant laminate comprises a plurality of cross-plied sheets, each cross-plied sheet further comprising (i) first and second layers of fibrous or non-fibrous ultra-high molecular weight polyethylene and (ii) first and second layers of thermoplastic adhesive, each adhesive layer having a basis weight of no greater than 5 gsm, wherein (a) the layers of polyethylene and thermoplastic adhesive alternate within the sheet, (b) at least 50 percent of the polyethylene layers are arranged such that the orientation of the first polyethylene layer is offset with respect to the orientation of the second polyethylene layer, and (c) the plurality of cross-plied sheets form a stack that, when subjected to compaction at a pressure of 255 bar and a temperature of 132 degrees C., will not suffer a pressure loss greater than 8 bar within the first two minutes as measured by Test Method B.</description><subject>ARMOUR</subject><subject>ARMOURED OR ARMED VEHICLES</subject><subject>ARMOURED TURRETS</subject><subject>BLASTING</subject><subject>HEATING</subject><subject>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES</subject><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>LIGHTING</subject><subject>MEANS OF ATTACK OR DEFENCE, e.g. CAMOUFLAGE, IN GENERAL</subject><subject>MEASURING</subject><subject>MECHANICAL ENGINEERING</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICS</subject><subject>TESTING</subject><subject>TRANSPORTING</subject><subject>WEAPONS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFBz9vcN8A_2DHFVcHL08fEMDvF0VghyDQYyHP1CFHwcfT39HENceRhY0xJzilN5oTQ3g7Kba4izh25qQX58anFBYnJqXmpJfGiwkYGhmZGZqYWFkaOhMXGqAGvOJMM</recordid><startdate>20160915</startdate><enddate>20160915</enddate><creator>KAMPERT William George</creator><creator>SAUER Bryan Benedict</creator><creator>SINGLETARY James Neal</creator><creator>LIBERT Timothy A</creator><creator>CARBAJAL Leopoldo Alejandro</creator><scope>EVB</scope></search><sort><creationdate>20160915</creationdate><title>COMPOSITE BALLISTIC RESISTANT LAMINATE</title><author>KAMPERT William George ; SAUER Bryan Benedict ; SINGLETARY James Neal ; LIBERT Timothy A ; CARBAJAL Leopoldo Alejandro</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2016265882A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2016</creationdate><topic>ARMOUR</topic><topic>ARMOURED OR ARMED VEHICLES</topic><topic>ARMOURED TURRETS</topic><topic>BLASTING</topic><topic>HEATING</topic><topic>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES</topic><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>LIGHTING</topic><topic>MEANS OF ATTACK OR DEFENCE, e.g. CAMOUFLAGE, IN GENERAL</topic><topic>MEASURING</topic><topic>MECHANICAL ENGINEERING</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICS</topic><topic>TESTING</topic><topic>TRANSPORTING</topic><topic>WEAPONS</topic><toplevel>online_resources</toplevel><creatorcontrib>KAMPERT William George</creatorcontrib><creatorcontrib>SAUER Bryan Benedict</creatorcontrib><creatorcontrib>SINGLETARY James Neal</creatorcontrib><creatorcontrib>LIBERT Timothy A</creatorcontrib><creatorcontrib>CARBAJAL Leopoldo Alejandro</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KAMPERT William George</au><au>SAUER Bryan Benedict</au><au>SINGLETARY James Neal</au><au>LIBERT Timothy A</au><au>CARBAJAL Leopoldo Alejandro</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>COMPOSITE BALLISTIC RESISTANT LAMINATE</title><date>2016-09-15</date><risdate>2016</risdate><abstract>An unconsolidated impact and penetration resistant laminate comprises a plurality of cross-plied sheets, each cross-plied sheet further comprising (i) first and second layers of fibrous or non-fibrous ultra-high molecular weight polyethylene and (ii) first and second layers of thermoplastic adhesive, each adhesive layer having a basis weight of no greater than 5 gsm, wherein (a) the layers of polyethylene and thermoplastic adhesive alternate within the sheet, (b) at least 50 percent of the polyethylene layers are arranged such that the orientation of the first polyethylene layer is offset with respect to the orientation of the second polyethylene layer, and (c) the plurality of cross-plied sheets form a stack that, when subjected to compaction at a pressure of 255 bar and a temperature of 132 degrees C., will not suffer a pressure loss greater than 8 bar within the first two minutes as measured by Test Method B.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2016265882A1
source esp@cenet
subjects ARMOUR
ARMOURED OR ARMED VEHICLES
ARMOURED TURRETS
BLASTING
HEATING
INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES
LAYERED PRODUCTS
LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
LIGHTING
MEANS OF ATTACK OR DEFENCE, e.g. CAMOUFLAGE, IN GENERAL
MEASURING
MECHANICAL ENGINEERING
PERFORMING OPERATIONS
PHYSICS
TESTING
TRANSPORTING
WEAPONS
title COMPOSITE BALLISTIC RESISTANT LAMINATE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T14%3A48%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KAMPERT%20William%20George&rft.date=2016-09-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2016265882A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true