ELECTRODE MATERIAL, SPARK-PLUG ELECTRODE, AND SPARK PLUG

An electrode material contains, on a mass percent basis, Al: 0.005% to 0.2%, Si: 0.2% to 1.6%, Cr: 0.05% to 1.0%, Ti: 0.05% to 0.5%, and Y: 0.2% to 1.0%. The remainder are Ni and inevitable impurities. The Si/Cr mass ratio is 1 or more. Because of the inclusion of specific amounts of Al, Si, Cr, and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YAMAZAKI KAZUO, TOKUDA TAKESHI, TOMITA SHIN, NISHIKAWA TAICHIRO, SAKUTA MASAO, OTA HAJIME, TAKAKI YOSHIYUKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YAMAZAKI KAZUO
TOKUDA TAKESHI
TOMITA SHIN
NISHIKAWA TAICHIRO
SAKUTA MASAO
OTA HAJIME
TAKAKI YOSHIYUKI
description An electrode material contains, on a mass percent basis, Al: 0.005% to 0.2%, Si: 0.2% to 1.6%, Cr: 0.05% to 1.0%, Ti: 0.05% to 0.5%, and Y: 0.2% to 1.0%. The remainder are Ni and inevitable impurities. The Si/Cr mass ratio is 1 or more. Because of the inclusion of specific amounts of Al, Si, Cr, and Y and the Si content higher than the Al content, the electrode material has an oxidation inhibiting effect. The inclusion of the specific amount of Ti can reduce the occurrence of expansion and cracking of the oxide film. Because of the inclusion of the specific amount of Y, the oxide film can maintain the microstructure even at high temperatures and have high resistance to high-temperature oxidation. Having a Si/Cr ratio of 1 or more, the oxide film has improved corrosion resistance and is resistant to corrosion by corrosive liquids.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2014370258A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2014370258A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2014370258A13</originalsourceid><addsrcrecordid>eNrjZLBw9XF1Dgnyd3FV8HUMcQ3ydPTRUQgOcAzy1g3wCXVXgEvrKDj6uUBkFEAyPAysaYk5xam8UJqbQdnNNcTZQze1ID8-tbggMTk1L7UkPjTYyMDQxNjcwMjUwtHQmDhVAOSUKRo</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>ELECTRODE MATERIAL, SPARK-PLUG ELECTRODE, AND SPARK PLUG</title><source>esp@cenet</source><creator>YAMAZAKI KAZUO ; TOKUDA TAKESHI ; TOMITA SHIN ; NISHIKAWA TAICHIRO ; SAKUTA MASAO ; OTA HAJIME ; TAKAKI YOSHIYUKI</creator><creatorcontrib>YAMAZAKI KAZUO ; TOKUDA TAKESHI ; TOMITA SHIN ; NISHIKAWA TAICHIRO ; SAKUTA MASAO ; OTA HAJIME ; TAKAKI YOSHIYUKI</creatorcontrib><description>An electrode material contains, on a mass percent basis, Al: 0.005% to 0.2%, Si: 0.2% to 1.6%, Cr: 0.05% to 1.0%, Ti: 0.05% to 0.5%, and Y: 0.2% to 1.0%. The remainder are Ni and inevitable impurities. The Si/Cr mass ratio is 1 or more. Because of the inclusion of specific amounts of Al, Si, Cr, and Y and the Si content higher than the Al content, the electrode material has an oxidation inhibiting effect. The inclusion of the specific amount of Ti can reduce the occurrence of expansion and cracking of the oxide film. Because of the inclusion of the specific amount of Y, the oxide film can maintain the microstructure even at high temperatures and have high resistance to high-temperature oxidation. Having a Si/Cr ratio of 1 or more, the oxide film has improved corrosion resistance and is resistant to corrosion by corrosive liquids.</description><language>eng</language><subject>ALLOYS ; BASIC ELECTRIC ELEMENTS ; BLASTING ; CHEMISTRY ; COMBUSTION ENGINES ; CORONA DEVICES ; ELECTRICITY ; FERROUS OR NON-FERROUS ALLOYS ; GENERATING IONS TO BE INTRODUCED INTO NON-ENCLOSED GASES ; HEATING ; HOT-GAS OR COMBUSTION-PRODUCT ENGINE PLANTS ; IGNITION, OTHER THAN COMPRESSION IGNITION, FORINTERNAL-COMBUSTION ENGINES ; LIGHTING ; MECHANICAL ENGINEERING ; METALLURGY ; OVERVOLTAGE ARRESTERS USING SPARK GAPS ; SPARK GAPS ; SPARKING PLUGS ; TESTING OF IGNITION TIMING IN COMPRESSION-IGNITION ENGINES ; TREATMENT OF ALLOYS OR NON-FERROUS METALS ; WEAPONS</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20141218&amp;DB=EPODOC&amp;CC=US&amp;NR=2014370258A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20141218&amp;DB=EPODOC&amp;CC=US&amp;NR=2014370258A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YAMAZAKI KAZUO</creatorcontrib><creatorcontrib>TOKUDA TAKESHI</creatorcontrib><creatorcontrib>TOMITA SHIN</creatorcontrib><creatorcontrib>NISHIKAWA TAICHIRO</creatorcontrib><creatorcontrib>SAKUTA MASAO</creatorcontrib><creatorcontrib>OTA HAJIME</creatorcontrib><creatorcontrib>TAKAKI YOSHIYUKI</creatorcontrib><title>ELECTRODE MATERIAL, SPARK-PLUG ELECTRODE, AND SPARK PLUG</title><description>An electrode material contains, on a mass percent basis, Al: 0.005% to 0.2%, Si: 0.2% to 1.6%, Cr: 0.05% to 1.0%, Ti: 0.05% to 0.5%, and Y: 0.2% to 1.0%. The remainder are Ni and inevitable impurities. The Si/Cr mass ratio is 1 or more. Because of the inclusion of specific amounts of Al, Si, Cr, and Y and the Si content higher than the Al content, the electrode material has an oxidation inhibiting effect. The inclusion of the specific amount of Ti can reduce the occurrence of expansion and cracking of the oxide film. Because of the inclusion of the specific amount of Y, the oxide film can maintain the microstructure even at high temperatures and have high resistance to high-temperature oxidation. Having a Si/Cr ratio of 1 or more, the oxide film has improved corrosion resistance and is resistant to corrosion by corrosive liquids.</description><subject>ALLOYS</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>BLASTING</subject><subject>CHEMISTRY</subject><subject>COMBUSTION ENGINES</subject><subject>CORONA DEVICES</subject><subject>ELECTRICITY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERATING IONS TO BE INTRODUCED INTO NON-ENCLOSED GASES</subject><subject>HEATING</subject><subject>HOT-GAS OR COMBUSTION-PRODUCT ENGINE PLANTS</subject><subject>IGNITION, OTHER THAN COMPRESSION IGNITION, FORINTERNAL-COMBUSTION ENGINES</subject><subject>LIGHTING</subject><subject>MECHANICAL ENGINEERING</subject><subject>METALLURGY</subject><subject>OVERVOLTAGE ARRESTERS USING SPARK GAPS</subject><subject>SPARK GAPS</subject><subject>SPARKING PLUGS</subject><subject>TESTING OF IGNITION TIMING IN COMPRESSION-IGNITION ENGINES</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><subject>WEAPONS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLBw9XF1Dgnyd3FV8HUMcQ3ydPTRUQgOcAzy1g3wCXVXgEvrKDj6uUBkFEAyPAysaYk5xam8UJqbQdnNNcTZQze1ID8-tbggMTk1L7UkPjTYyMDQxNjcwMjUwtHQmDhVAOSUKRo</recordid><startdate>20141218</startdate><enddate>20141218</enddate><creator>YAMAZAKI KAZUO</creator><creator>TOKUDA TAKESHI</creator><creator>TOMITA SHIN</creator><creator>NISHIKAWA TAICHIRO</creator><creator>SAKUTA MASAO</creator><creator>OTA HAJIME</creator><creator>TAKAKI YOSHIYUKI</creator><scope>EVB</scope></search><sort><creationdate>20141218</creationdate><title>ELECTRODE MATERIAL, SPARK-PLUG ELECTRODE, AND SPARK PLUG</title><author>YAMAZAKI KAZUO ; TOKUDA TAKESHI ; TOMITA SHIN ; NISHIKAWA TAICHIRO ; SAKUTA MASAO ; OTA HAJIME ; TAKAKI YOSHIYUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2014370258A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2014</creationdate><topic>ALLOYS</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>BLASTING</topic><topic>CHEMISTRY</topic><topic>COMBUSTION ENGINES</topic><topic>CORONA DEVICES</topic><topic>ELECTRICITY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERATING IONS TO BE INTRODUCED INTO NON-ENCLOSED GASES</topic><topic>HEATING</topic><topic>HOT-GAS OR COMBUSTION-PRODUCT ENGINE PLANTS</topic><topic>IGNITION, OTHER THAN COMPRESSION IGNITION, FORINTERNAL-COMBUSTION ENGINES</topic><topic>LIGHTING</topic><topic>MECHANICAL ENGINEERING</topic><topic>METALLURGY</topic><topic>OVERVOLTAGE ARRESTERS USING SPARK GAPS</topic><topic>SPARK GAPS</topic><topic>SPARKING PLUGS</topic><topic>TESTING OF IGNITION TIMING IN COMPRESSION-IGNITION ENGINES</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><topic>WEAPONS</topic><toplevel>online_resources</toplevel><creatorcontrib>YAMAZAKI KAZUO</creatorcontrib><creatorcontrib>TOKUDA TAKESHI</creatorcontrib><creatorcontrib>TOMITA SHIN</creatorcontrib><creatorcontrib>NISHIKAWA TAICHIRO</creatorcontrib><creatorcontrib>SAKUTA MASAO</creatorcontrib><creatorcontrib>OTA HAJIME</creatorcontrib><creatorcontrib>TAKAKI YOSHIYUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YAMAZAKI KAZUO</au><au>TOKUDA TAKESHI</au><au>TOMITA SHIN</au><au>NISHIKAWA TAICHIRO</au><au>SAKUTA MASAO</au><au>OTA HAJIME</au><au>TAKAKI YOSHIYUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>ELECTRODE MATERIAL, SPARK-PLUG ELECTRODE, AND SPARK PLUG</title><date>2014-12-18</date><risdate>2014</risdate><abstract>An electrode material contains, on a mass percent basis, Al: 0.005% to 0.2%, Si: 0.2% to 1.6%, Cr: 0.05% to 1.0%, Ti: 0.05% to 0.5%, and Y: 0.2% to 1.0%. The remainder are Ni and inevitable impurities. The Si/Cr mass ratio is 1 or more. Because of the inclusion of specific amounts of Al, Si, Cr, and Y and the Si content higher than the Al content, the electrode material has an oxidation inhibiting effect. The inclusion of the specific amount of Ti can reduce the occurrence of expansion and cracking of the oxide film. Because of the inclusion of the specific amount of Y, the oxide film can maintain the microstructure even at high temperatures and have high resistance to high-temperature oxidation. Having a Si/Cr ratio of 1 or more, the oxide film has improved corrosion resistance and is resistant to corrosion by corrosive liquids.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2014370258A1
source esp@cenet
subjects ALLOYS
BASIC ELECTRIC ELEMENTS
BLASTING
CHEMISTRY
COMBUSTION ENGINES
CORONA DEVICES
ELECTRICITY
FERROUS OR NON-FERROUS ALLOYS
GENERATING IONS TO BE INTRODUCED INTO NON-ENCLOSED GASES
HEATING
HOT-GAS OR COMBUSTION-PRODUCT ENGINE PLANTS
IGNITION, OTHER THAN COMPRESSION IGNITION, FORINTERNAL-COMBUSTION ENGINES
LIGHTING
MECHANICAL ENGINEERING
METALLURGY
OVERVOLTAGE ARRESTERS USING SPARK GAPS
SPARK GAPS
SPARKING PLUGS
TESTING OF IGNITION TIMING IN COMPRESSION-IGNITION ENGINES
TREATMENT OF ALLOYS OR NON-FERROUS METALS
WEAPONS
title ELECTRODE MATERIAL, SPARK-PLUG ELECTRODE, AND SPARK PLUG
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T16%3A45%3A38IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YAMAZAKI%20KAZUO&rft.date=2014-12-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2014370258A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true