Process for Heap Leaching of Nickeliferous Oxidic Ores
A process for the recovery of nickel and cobalt from a nickeliferous oxidic ore by heap leaching and/or atmospheric agitation leaching, the process including the steps of: mixing a sulfur containing reductant selected from reductants that do not include copper into a nickeliferous oxidic ore; leachi...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | LIU HOUYUAN |
description | A process for the recovery of nickel and cobalt from a nickeliferous oxidic ore by heap leaching and/or atmospheric agitation leaching, the process including the steps of: mixing a sulfur containing reductant selected from reductants that do not include copper into a nickeliferous oxidic ore; leaching the reductant/ore mixture with an acidic leach reagent to produce a pregnant leach solution including nickel, cobalt, iron substantially in a ferrous form and other acid soluble impurities; and recovering the nickel and cobalt from the pregnant leach solution. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2011150729A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2011150729A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2011150729A13</originalsourceid><addsrcrecordid>eNrjZDALKMpPTi0uVkjLL1LwSE0sUPBJTUzOyMxLV8hPU_DLTM5OzclMSy3KLy1W8K_ITMlMVvAvSi3mYWBNS8wpTuWF0twMym6uIc4euqkF-fGpxQWJyal5qSXxocFGBoaGhqYG5kaWjobGxKkCAAAfLck</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Process for Heap Leaching of Nickeliferous Oxidic Ores</title><source>esp@cenet</source><creator>LIU HOUYUAN</creator><creatorcontrib>LIU HOUYUAN</creatorcontrib><description>A process for the recovery of nickel and cobalt from a nickeliferous oxidic ore by heap leaching and/or atmospheric agitation leaching, the process including the steps of: mixing a sulfur containing reductant selected from reductants that do not include copper into a nickeliferous oxidic ore; leaching the reductant/ore mixture with an acidic leach reagent to produce a pregnant leach solution including nickel, cobalt, iron substantially in a ferrous form and other acid soluble impurities; and recovering the nickel and cobalt from the pregnant leach solution.</description><language>eng</language><subject>CHEMISTRY ; CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION ORPROCESSING OF GOODS ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC ; GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS ; INORGANIC CHEMISTRY ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS ; TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2011</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20110623&DB=EPODOC&CC=US&NR=2011150729A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20110623&DB=EPODOC&CC=US&NR=2011150729A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU HOUYUAN</creatorcontrib><title>Process for Heap Leaching of Nickeliferous Oxidic Ores</title><description>A process for the recovery of nickel and cobalt from a nickeliferous oxidic ore by heap leaching and/or atmospheric agitation leaching, the process including the steps of: mixing a sulfur containing reductant selected from reductants that do not include copper into a nickeliferous oxidic ore; leaching the reductant/ore mixture with an acidic leach reagent to produce a pregnant leach solution including nickel, cobalt, iron substantially in a ferrous form and other acid soluble impurities; and recovering the nickel and cobalt from the pregnant leach solution.</description><subject>CHEMISTRY</subject><subject>CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION ORPROCESSING OF GOODS</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</subject><subject>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</subject><subject>TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2011</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDALKMpPTi0uVkjLL1LwSE0sUPBJTUzOyMxLV8hPU_DLTM5OzclMSy3KLy1W8K_ITMlMVvAvSi3mYWBNS8wpTuWF0twMym6uIc4euqkF-fGpxQWJyal5qSXxocFGBoaGhqYG5kaWjobGxKkCAAAfLck</recordid><startdate>20110623</startdate><enddate>20110623</enddate><creator>LIU HOUYUAN</creator><scope>EVB</scope></search><sort><creationdate>20110623</creationdate><title>Process for Heap Leaching of Nickeliferous Oxidic Ores</title><author>LIU HOUYUAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2011150729A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2011</creationdate><topic>CHEMISTRY</topic><topic>CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION ORPROCESSING OF GOODS</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</topic><topic>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</topic><topic>TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU HOUYUAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU HOUYUAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Process for Heap Leaching of Nickeliferous Oxidic Ores</title><date>2011-06-23</date><risdate>2011</risdate><abstract>A process for the recovery of nickel and cobalt from a nickeliferous oxidic ore by heap leaching and/or atmospheric agitation leaching, the process including the steps of: mixing a sulfur containing reductant selected from reductants that do not include copper into a nickeliferous oxidic ore; leaching the reductant/ore mixture with an acidic leach reagent to produce a pregnant leach solution including nickel, cobalt, iron substantially in a ferrous form and other acid soluble impurities; and recovering the nickel and cobalt from the pregnant leach solution.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US2011150729A1 |
source | esp@cenet |
subjects | CHEMISTRY CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION ORPROCESSING OF GOODS COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F FERROUS OR NON-FERROUS ALLOYS GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS INORGANIC CHEMISTRY METALLURGY PRETREATMENT OF RAW MATERIALS PRODUCTION AND REFINING OF METALS TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Process for Heap Leaching of Nickeliferous Oxidic Ores |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T12%3A53%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20HOUYUAN&rft.date=2011-06-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2011150729A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |