Glass Forming Hardbanding Material

A drill pipe and a method of applying hardbanding thereto. A hardbanding alloy comprising iron and manganese present in the range of 67 to 87 weight percent (wt. %), niobium and chromium present in the range of 9 to 29 wt. %, and boron, carbon and silicon present in the range of 3 to 6.5 wt. % may b...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KIILUNEN WILLIAM D, MERKLE BRIAN D, BRANAGAN DANIEL JAMES, MILLOWAY JAMES N, MEACHAM BRIAN E
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KIILUNEN WILLIAM D
MERKLE BRIAN D
BRANAGAN DANIEL JAMES
MILLOWAY JAMES N
MEACHAM BRIAN E
description A drill pipe and a method of applying hardbanding thereto. A hardbanding alloy comprising iron and manganese present in the range of 67 to 87 weight percent (wt. %), niobium and chromium present in the range of 9 to 29 wt. %, and boron, carbon and silicon present in the range of 3 to 6.5 wt. % may be welded around at least a portion of a tool joint circumference. The hardbanding alloy may exhibit a hardness of 45 Rc to 70 Rc and a wear rate in the range of 0.08 grams to 1.60 grams of mass loss after 6,000 cycles as measured using ASTM G65-04, Procedure A.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2011100720A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2011100720A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2011100720A13</originalsourceid><addsrcrecordid>eNrjZFByz0ksLlZwyy_KzcxLV_BILEpJSsxLAbF9E0tSizITc3gYWNMSc4pTeaE0N4Oym2uIs4duakF-fGpxQWJyal5qSXxosJGBoaGhgYG5kYGjoTFxqgAjECaG</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Glass Forming Hardbanding Material</title><source>esp@cenet</source><creator>KIILUNEN WILLIAM D ; MERKLE BRIAN D ; BRANAGAN DANIEL JAMES ; MILLOWAY JAMES N ; MEACHAM BRIAN E</creator><creatorcontrib>KIILUNEN WILLIAM D ; MERKLE BRIAN D ; BRANAGAN DANIEL JAMES ; MILLOWAY JAMES N ; MEACHAM BRIAN E</creatorcontrib><description>A drill pipe and a method of applying hardbanding thereto. A hardbanding alloy comprising iron and manganese present in the range of 67 to 87 weight percent (wt. %), niobium and chromium present in the range of 9 to 29 wt. %, and boron, carbon and silicon present in the range of 3 to 6.5 wt. % may be welded around at least a portion of a tool joint circumference. The hardbanding alloy may exhibit a hardness of 45 Rc to 70 Rc and a wear rate in the range of 0.08 grams to 1.60 grams of mass loss after 6,000 cycles as measured using ASTM G65-04, Procedure A.</description><language>eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; EARTH DRILLING ; EARTH DRILLING, e.g. DEEP DRILLING ; FIXED CONSTRUCTIONS ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; MINING ; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2011</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20110505&amp;DB=EPODOC&amp;CC=US&amp;NR=2011100720A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20110505&amp;DB=EPODOC&amp;CC=US&amp;NR=2011100720A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KIILUNEN WILLIAM D</creatorcontrib><creatorcontrib>MERKLE BRIAN D</creatorcontrib><creatorcontrib>BRANAGAN DANIEL JAMES</creatorcontrib><creatorcontrib>MILLOWAY JAMES N</creatorcontrib><creatorcontrib>MEACHAM BRIAN E</creatorcontrib><title>Glass Forming Hardbanding Material</title><description>A drill pipe and a method of applying hardbanding thereto. A hardbanding alloy comprising iron and manganese present in the range of 67 to 87 weight percent (wt. %), niobium and chromium present in the range of 9 to 29 wt. %, and boron, carbon and silicon present in the range of 3 to 6.5 wt. % may be welded around at least a portion of a tool joint circumference. The hardbanding alloy may exhibit a hardness of 45 Rc to 70 Rc and a wear rate in the range of 0.08 grams to 1.60 grams of mass loss after 6,000 cycles as measured using ASTM G65-04, Procedure A.</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>EARTH DRILLING</subject><subject>EARTH DRILLING, e.g. DEEP DRILLING</subject><subject>FIXED CONSTRUCTIONS</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>MINING</subject><subject>OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2011</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFByz0ksLlZwyy_KzcxLV_BILEpJSsxLAbF9E0tSizITc3gYWNMSc4pTeaE0N4Oym2uIs4duakF-fGpxQWJyal5qSXxosJGBoaGhgYG5kYGjoTFxqgAjECaG</recordid><startdate>20110505</startdate><enddate>20110505</enddate><creator>KIILUNEN WILLIAM D</creator><creator>MERKLE BRIAN D</creator><creator>BRANAGAN DANIEL JAMES</creator><creator>MILLOWAY JAMES N</creator><creator>MEACHAM BRIAN E</creator><scope>EVB</scope></search><sort><creationdate>20110505</creationdate><title>Glass Forming Hardbanding Material</title><author>KIILUNEN WILLIAM D ; MERKLE BRIAN D ; BRANAGAN DANIEL JAMES ; MILLOWAY JAMES N ; MEACHAM BRIAN E</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2011100720A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2011</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>EARTH DRILLING</topic><topic>EARTH DRILLING, e.g. DEEP DRILLING</topic><topic>FIXED CONSTRUCTIONS</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>MINING</topic><topic>OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>KIILUNEN WILLIAM D</creatorcontrib><creatorcontrib>MERKLE BRIAN D</creatorcontrib><creatorcontrib>BRANAGAN DANIEL JAMES</creatorcontrib><creatorcontrib>MILLOWAY JAMES N</creatorcontrib><creatorcontrib>MEACHAM BRIAN E</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KIILUNEN WILLIAM D</au><au>MERKLE BRIAN D</au><au>BRANAGAN DANIEL JAMES</au><au>MILLOWAY JAMES N</au><au>MEACHAM BRIAN E</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Glass Forming Hardbanding Material</title><date>2011-05-05</date><risdate>2011</risdate><abstract>A drill pipe and a method of applying hardbanding thereto. A hardbanding alloy comprising iron and manganese present in the range of 67 to 87 weight percent (wt. %), niobium and chromium present in the range of 9 to 29 wt. %, and boron, carbon and silicon present in the range of 3 to 6.5 wt. % may be welded around at least a portion of a tool joint circumference. The hardbanding alloy may exhibit a hardness of 45 Rc to 70 Rc and a wear rate in the range of 0.08 grams to 1.60 grams of mass loss after 6,000 cycles as measured using ASTM G65-04, Procedure A.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2011100720A1
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
EARTH DRILLING
EARTH DRILLING, e.g. DEEP DRILLING
FIXED CONSTRUCTIONS
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
MINING
OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title Glass Forming Hardbanding Material
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-23T01%3A22%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KIILUNEN%20WILLIAM%20D&rft.date=2011-05-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2011100720A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true