Process for coating a hot- or cold- rolled steel strip containing 6 - 30% by weight of MN with a metallic protective layer
A method for coating hot-rolled or cold-rolled steel strip containing 6-30 wt %. Mn with a metallic protective layer, includes annealing the steel strip at a temperature of 800-1100° C. under an annealing atmosphere containing nitrogen, water and hydrogen and then subjecting the steel strip to hot d...