Method and apparatus for controlling flow of molten steel in mold, and method for producing continuous castings

When a molten steel flow velocity (u) on a bath surface is higher than a mold-powder entrainment critical flow velocity of 0.32 m/sec, the molten steel flow velocity (u) is controlled to a predetermined molten steel flow velocity by applying a shifting magnetic field to impart a braking force to a d...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KONDO TSUNEO, MIZUOKA SEISHI, KUBOTA JUN
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KONDO TSUNEO
MIZUOKA SEISHI
KUBOTA JUN
description When a molten steel flow velocity (u) on a bath surface is higher than a mold-powder entrainment critical flow velocity of 0.32 m/sec, the molten steel flow velocity (u) is controlled to a predetermined molten steel flow velocity by applying a shifting magnetic field to impart a braking force to a discharge flow from an immersion nozzle. When the molten steel flow velocity (u) is lower than an inclusion-adherence critical flow velocity of 0.20 m/sec and is higher than or equal to a bath-surface skinning critical flow velocity of 0.10 m/sec, the molten steel flow velocity (u) is control to the range of 0.20-0.32 m/sec by applying a shifting magnetic field to rotate the intra-mold molten steel in a horizontal direction. When the molten steel flow velocity (u) is lower than the inclusion-adherence critical flow velocity, the molten steel flow velocity (u) is controlled to the range of 0.20-0.32 m/sec by applying a shifting magnetic field to impart an accelerating force to the discharge flow from the immersion nozzle.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2005092458A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2005092458A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2005092458A13</originalsourceid><addsrcrecordid>eNqNjEEKwjAQRbNxIeodBtwq1GpBlyKKG1fquoRk0hbSmZBJ8fo26gFcDH8-_Pemim-YWragabwQdNRpEHAcwTClyN531IDz_AJ20LNPSCAJ0UNHudvVh-2_mgyGyHYwGcuKjgYejUbL-DYyVxOnveDilzO1vJwfp-saA9coQRskTPXzXhZFVRzKXbU_brb_rd4Rt0QI</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method and apparatus for controlling flow of molten steel in mold, and method for producing continuous castings</title><source>esp@cenet</source><creator>KONDO TSUNEO ; MIZUOKA SEISHI ; KUBOTA JUN</creator><creatorcontrib>KONDO TSUNEO ; MIZUOKA SEISHI ; KUBOTA JUN</creatorcontrib><description>When a molten steel flow velocity (u) on a bath surface is higher than a mold-powder entrainment critical flow velocity of 0.32 m/sec, the molten steel flow velocity (u) is controlled to a predetermined molten steel flow velocity by applying a shifting magnetic field to impart a braking force to a discharge flow from an immersion nozzle. When the molten steel flow velocity (u) is lower than an inclusion-adherence critical flow velocity of 0.20 m/sec and is higher than or equal to a bath-surface skinning critical flow velocity of 0.10 m/sec, the molten steel flow velocity (u) is control to the range of 0.20-0.32 m/sec by applying a shifting magnetic field to rotate the intra-mold molten steel in a horizontal direction. When the molten steel flow velocity (u) is lower than the inclusion-adherence critical flow velocity, the molten steel flow velocity (u) is controlled to the range of 0.20-0.32 m/sec by applying a shifting magnetic field to impart an accelerating force to the discharge flow from the immersion nozzle.</description><edition>7</edition><language>eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>2005</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050505&amp;DB=EPODOC&amp;CC=US&amp;NR=2005092458A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050505&amp;DB=EPODOC&amp;CC=US&amp;NR=2005092458A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KONDO TSUNEO</creatorcontrib><creatorcontrib>MIZUOKA SEISHI</creatorcontrib><creatorcontrib>KUBOTA JUN</creatorcontrib><title>Method and apparatus for controlling flow of molten steel in mold, and method for producing continuous castings</title><description>When a molten steel flow velocity (u) on a bath surface is higher than a mold-powder entrainment critical flow velocity of 0.32 m/sec, the molten steel flow velocity (u) is controlled to a predetermined molten steel flow velocity by applying a shifting magnetic field to impart a braking force to a discharge flow from an immersion nozzle. When the molten steel flow velocity (u) is lower than an inclusion-adherence critical flow velocity of 0.20 m/sec and is higher than or equal to a bath-surface skinning critical flow velocity of 0.10 m/sec, the molten steel flow velocity (u) is control to the range of 0.20-0.32 m/sec by applying a shifting magnetic field to rotate the intra-mold molten steel in a horizontal direction. When the molten steel flow velocity (u) is lower than the inclusion-adherence critical flow velocity, the molten steel flow velocity (u) is controlled to the range of 0.20-0.32 m/sec by applying a shifting magnetic field to impart an accelerating force to the discharge flow from the immersion nozzle.</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2005</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEEKwjAQRbNxIeodBtwq1GpBlyKKG1fquoRk0hbSmZBJ8fo26gFcDH8-_Pemim-YWragabwQdNRpEHAcwTClyN531IDz_AJ20LNPSCAJ0UNHudvVh-2_mgyGyHYwGcuKjgYejUbL-DYyVxOnveDilzO1vJwfp-saA9coQRskTPXzXhZFVRzKXbU_brb_rd4Rt0QI</recordid><startdate>20050505</startdate><enddate>20050505</enddate><creator>KONDO TSUNEO</creator><creator>MIZUOKA SEISHI</creator><creator>KUBOTA JUN</creator><scope>EVB</scope></search><sort><creationdate>20050505</creationdate><title>Method and apparatus for controlling flow of molten steel in mold, and method for producing continuous castings</title><author>KONDO TSUNEO ; MIZUOKA SEISHI ; KUBOTA JUN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2005092458A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2005</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>KONDO TSUNEO</creatorcontrib><creatorcontrib>MIZUOKA SEISHI</creatorcontrib><creatorcontrib>KUBOTA JUN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KONDO TSUNEO</au><au>MIZUOKA SEISHI</au><au>KUBOTA JUN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method and apparatus for controlling flow of molten steel in mold, and method for producing continuous castings</title><date>2005-05-05</date><risdate>2005</risdate><abstract>When a molten steel flow velocity (u) on a bath surface is higher than a mold-powder entrainment critical flow velocity of 0.32 m/sec, the molten steel flow velocity (u) is controlled to a predetermined molten steel flow velocity by applying a shifting magnetic field to impart a braking force to a discharge flow from an immersion nozzle. When the molten steel flow velocity (u) is lower than an inclusion-adherence critical flow velocity of 0.20 m/sec and is higher than or equal to a bath-surface skinning critical flow velocity of 0.10 m/sec, the molten steel flow velocity (u) is control to the range of 0.20-0.32 m/sec by applying a shifting magnetic field to rotate the intra-mold molten steel in a horizontal direction. When the molten steel flow velocity (u) is lower than the inclusion-adherence critical flow velocity, the molten steel flow velocity (u) is controlled to the range of 0.20-0.32 m/sec by applying a shifting magnetic field to impart an accelerating force to the discharge flow from the immersion nozzle.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2005092458A1
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title Method and apparatus for controlling flow of molten steel in mold, and method for producing continuous castings
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T10%3A01%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KONDO%20TSUNEO&rft.date=2005-05-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2005092458A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true