Hollow casting and manufacturing method therefor, and method and apparatus for smoothing internal surface of hollow casting
There is provided a hollow casting in which a surface roughness Ra of a casting wall portion surface forming a hollow portion formed by a wall portion is 10 mum or less. Such a hollow casting can be obtained by a manufacturing method for the hollow casting in which after molten metal is poured into...