Method of preparing positive electrode active material for secondary battery and secondary battery using the same
Provided is a method of preparing a positive electrode active material, which includes preparing a mixture by mixing a lithium compound, a transition metal precursor, and a metal oxide additive, and sintering the mixture to form a lithium transition metal oxide, wherein the sintering is performed th...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | Eom, Jun Ho Baek, Hyeon Hui Ban, Sung Ho Park, Na Ri |
description | Provided is a method of preparing a positive electrode active material, which includes preparing a mixture by mixing a lithium compound, a transition metal precursor, and a metal oxide additive, and sintering the mixture to form a lithium transition metal oxide, wherein the sintering is performed through two-stage temperature holding sections, a temperature of a first temperature holding section is in a range of 400° C. to 650° C., and a temperature of a second temperature holding section is in a range of 700° C. to 900° C. A positive electrode including a positive electrode active material prepared according to the method, and a lithium secondary battery including the positive electrode is also provided. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US11764347B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US11764347B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US11764347B23</originalsourceid><addsrcrecordid>eNqNzLsKwkAQheE0FqK-w_gAFjHB9IpiY6XWYdw9MQvJzro7Cnl7L1haWB34OPzj7HaAtmJJGgoRgaPzVwqSnLoHCB2MRrEgNh_oWREdd9RIpAQj3nIc6ML68oHY2x96T--otqDEPabZqOEuYfbdSTbfbU-b_QJBaqTABh5an495Xq3KoqzWy-KfzxP3p0Ru</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of preparing positive electrode active material for secondary battery and secondary battery using the same</title><source>esp@cenet</source><creator>Eom, Jun Ho ; Baek, Hyeon Hui ; Ban, Sung Ho ; Park, Na Ri</creator><creatorcontrib>Eom, Jun Ho ; Baek, Hyeon Hui ; Ban, Sung Ho ; Park, Na Ri</creatorcontrib><description>Provided is a method of preparing a positive electrode active material, which includes preparing a mixture by mixing a lithium compound, a transition metal precursor, and a metal oxide additive, and sintering the mixture to form a lithium transition metal oxide, wherein the sintering is performed through two-stage temperature holding sections, a temperature of a first temperature holding section is in a range of 400° C. to 650° C., and a temperature of a second temperature holding section is in a range of 700° C. to 900° C. A positive electrode including a positive electrode active material prepared according to the method, and a lithium secondary battery including the positive electrode is also provided.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; ELECTRICITY ; INORGANIC CHEMISTRY ; METALLURGY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230919&DB=EPODOC&CC=US&NR=11764347B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230919&DB=EPODOC&CC=US&NR=11764347B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Eom, Jun Ho</creatorcontrib><creatorcontrib>Baek, Hyeon Hui</creatorcontrib><creatorcontrib>Ban, Sung Ho</creatorcontrib><creatorcontrib>Park, Na Ri</creatorcontrib><title>Method of preparing positive electrode active material for secondary battery and secondary battery using the same</title><description>Provided is a method of preparing a positive electrode active material, which includes preparing a mixture by mixing a lithium compound, a transition metal precursor, and a metal oxide additive, and sintering the mixture to form a lithium transition metal oxide, wherein the sintering is performed through two-stage temperature holding sections, a temperature of a first temperature holding section is in a range of 400° C. to 650° C., and a temperature of a second temperature holding section is in a range of 700° C. to 900° C. A positive electrode including a positive electrode active material prepared according to the method, and a lithium secondary battery including the positive electrode is also provided.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNzLsKwkAQheE0FqK-w_gAFjHB9IpiY6XWYdw9MQvJzro7Cnl7L1haWB34OPzj7HaAtmJJGgoRgaPzVwqSnLoHCB2MRrEgNh_oWREdd9RIpAQj3nIc6ML68oHY2x96T--otqDEPabZqOEuYfbdSTbfbU-b_QJBaqTABh5an495Xq3KoqzWy-KfzxP3p0Ru</recordid><startdate>20230919</startdate><enddate>20230919</enddate><creator>Eom, Jun Ho</creator><creator>Baek, Hyeon Hui</creator><creator>Ban, Sung Ho</creator><creator>Park, Na Ri</creator><scope>EVB</scope></search><sort><creationdate>20230919</creationdate><title>Method of preparing positive electrode active material for secondary battery and secondary battery using the same</title><author>Eom, Jun Ho ; Baek, Hyeon Hui ; Ban, Sung Ho ; Park, Na Ri</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US11764347B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2023</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>Eom, Jun Ho</creatorcontrib><creatorcontrib>Baek, Hyeon Hui</creatorcontrib><creatorcontrib>Ban, Sung Ho</creatorcontrib><creatorcontrib>Park, Na Ri</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Eom, Jun Ho</au><au>Baek, Hyeon Hui</au><au>Ban, Sung Ho</au><au>Park, Na Ri</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of preparing positive electrode active material for secondary battery and secondary battery using the same</title><date>2023-09-19</date><risdate>2023</risdate><abstract>Provided is a method of preparing a positive electrode active material, which includes preparing a mixture by mixing a lithium compound, a transition metal precursor, and a metal oxide additive, and sintering the mixture to form a lithium transition metal oxide, wherein the sintering is performed through two-stage temperature holding sections, a temperature of a first temperature holding section is in a range of 400° C. to 650° C., and a temperature of a second temperature holding section is in a range of 700° C. to 900° C. A positive electrode including a positive electrode active material prepared according to the method, and a lithium secondary battery including the positive electrode is also provided.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US11764347B2 |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS CHEMISTRY COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ELECTRICITY INORGANIC CHEMISTRY METALLURGY PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY |
title | Method of preparing positive electrode active material for secondary battery and secondary battery using the same |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T20%3A25%3A53IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Eom,%20Jun%20Ho&rft.date=2023-09-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS11764347B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |