Polymer composition and methods of making and using same

A bimodal polymer composition comprising a lower molecular weight homopolymer and a higher molecular weight copolymer wherein the bimodal polymer composition has a density of from about 0.930 gram per cubic centimeter (g/cc) to about 0.970 g/cc, a ratio of high load melt index:melt index of from abo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Schwerdtfeger, Eric D, Fodor, Jeffrey S, Yu, Youlu, Soules, David A
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Schwerdtfeger, Eric D
Fodor, Jeffrey S
Yu, Youlu
Soules, David A
description A bimodal polymer composition comprising a lower molecular weight homopolymer and a higher molecular weight copolymer wherein the bimodal polymer composition has a density of from about 0.930 gram per cubic centimeter (g/cc) to about 0.970 g/cc, a ratio of high load melt index:melt index of from about 10 to about 150 and an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561. A chromium-catalyzed polymer composition comprising (i) a lower molecular weight homopolymer and (ii) a higher molecular weight copolymer, wherein the bimodal polymer composition has an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US11674023B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US11674023B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US11674023B23</originalsourceid><addsrcrecordid>eNrjZLAIyM-pzE0tUkjOzy3IL84syczPU0jMS1HITS3JyE8pVshPU8hNzM7MSweLlhaDWMWJuak8DKxpiTnFqbxQmptB0c01xNlDN7UgPz61uCAxOTUvtSQ-NNjQ0MzcxMDI2MnImBg1AAzqLlE</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Polymer composition and methods of making and using same</title><source>esp@cenet</source><creator>Schwerdtfeger, Eric D ; Fodor, Jeffrey S ; Yu, Youlu ; Soules, David A</creator><creatorcontrib>Schwerdtfeger, Eric D ; Fodor, Jeffrey S ; Yu, Youlu ; Soules, David A</creatorcontrib><description>A bimodal polymer composition comprising a lower molecular weight homopolymer and a higher molecular weight copolymer wherein the bimodal polymer composition has a density of from about 0.930 gram per cubic centimeter (g/cc) to about 0.970 g/cc, a ratio of high load melt index:melt index of from about 10 to about 150 and an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561. A chromium-catalyzed polymer composition comprising (i) a lower molecular weight homopolymer and (ii) a higher molecular weight copolymer, wherein the bimodal polymer composition has an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561.</description><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230613&amp;DB=EPODOC&amp;CC=US&amp;NR=11674023B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25551,76302</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230613&amp;DB=EPODOC&amp;CC=US&amp;NR=11674023B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Schwerdtfeger, Eric D</creatorcontrib><creatorcontrib>Fodor, Jeffrey S</creatorcontrib><creatorcontrib>Yu, Youlu</creatorcontrib><creatorcontrib>Soules, David A</creatorcontrib><title>Polymer composition and methods of making and using same</title><description>A bimodal polymer composition comprising a lower molecular weight homopolymer and a higher molecular weight copolymer wherein the bimodal polymer composition has a density of from about 0.930 gram per cubic centimeter (g/cc) to about 0.970 g/cc, a ratio of high load melt index:melt index of from about 10 to about 150 and an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561. A chromium-catalyzed polymer composition comprising (i) a lower molecular weight homopolymer and (ii) a higher molecular weight copolymer, wherein the bimodal polymer composition has an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAIyM-pzE0tUkjOzy3IL84syczPU0jMS1HITS3JyE8pVshPU8hNzM7MSweLlhaDWMWJuak8DKxpiTnFqbxQmptB0c01xNlDN7UgPz61uCAxOTUvtSQ-NNjQ0MzcxMDI2MnImBg1AAzqLlE</recordid><startdate>20230613</startdate><enddate>20230613</enddate><creator>Schwerdtfeger, Eric D</creator><creator>Fodor, Jeffrey S</creator><creator>Yu, Youlu</creator><creator>Soules, David A</creator><scope>EVB</scope></search><sort><creationdate>20230613</creationdate><title>Polymer composition and methods of making and using same</title><author>Schwerdtfeger, Eric D ; Fodor, Jeffrey S ; Yu, Youlu ; Soules, David A</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US11674023B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2023</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>Schwerdtfeger, Eric D</creatorcontrib><creatorcontrib>Fodor, Jeffrey S</creatorcontrib><creatorcontrib>Yu, Youlu</creatorcontrib><creatorcontrib>Soules, David A</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Schwerdtfeger, Eric D</au><au>Fodor, Jeffrey S</au><au>Yu, Youlu</au><au>Soules, David A</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Polymer composition and methods of making and using same</title><date>2023-06-13</date><risdate>2023</risdate><abstract>A bimodal polymer composition comprising a lower molecular weight homopolymer and a higher molecular weight copolymer wherein the bimodal polymer composition has a density of from about 0.930 gram per cubic centimeter (g/cc) to about 0.970 g/cc, a ratio of high load melt index:melt index of from about 10 to about 150 and an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561. A chromium-catalyzed polymer composition comprising (i) a lower molecular weight homopolymer and (ii) a higher molecular weight copolymer, wherein the bimodal polymer composition has an Environmental Stress Crack Resistance (ESCR) of from about 25 hours to about 300 hours when measured in accordance with ASTM D1693 or ASTM D2561.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US11674023B2
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title Polymer composition and methods of making and using same
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T18%3A36%3A15IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Schwerdtfeger,%20Eric%20D&rft.date=2023-06-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS11674023B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true