Grain-oriented silicon steel with low core loss and manufacturing method therefore

A grain-oriented silicon steel with low iron loss, wherein the silicon steel is provided with a plurality of grooves on its surface, each of the grooves is 10-60 μm in width and 5-40 μm in depth, and the spacing between adjacent grooves is 1-10 mm. The manufacturing method therefor comprises: scorin...