Heat-resistant sintered material having excellent high-temperature wear resistance and salt damage resistance and method for producing same
This heat-resistant sintered material has, as an overall composition, a composition including, in terms of % by mass, Cr: 15% to 30%, Ni: 8% to 30%, Si: 2.0% to 6.0%, and C: 0.5% to 2.5% with a remainder being Fe and inevitable impurities, wherein the heat-resistant sintered material has a structure...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | This heat-resistant sintered material has, as an overall composition, a composition including, in terms of % by mass, Cr: 15% to 30%, Ni: 8% to 30%, Si: 2.0% to 6.0%, and C: 0.5% to 2.5% with a remainder being Fe and inevitable impurities, wherein the heat-resistant sintered material has a structure in which hard phases are dispersed in a matrix, the matrix includes Fe, Cr, Ni, and Si, the hard phase includes Fe, Cr, and C, and a porosity is 2.0% or less. |
---|