Method for reducing yellowness index of a polyetherimide, polyetherimide having a reduced yellowness index, and compositions and articles comprising the polyetherimide

A method for reducing yellowness of a polyetherimide solution, including exposing a first solution including a solvent and a polyetherimide to light under conditions effective to provide a second solution having a yellowness index that is 1 to 100 units less than the yellowness index of the first so...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Rodriguez Ordonez, Juan Justino, Remacha, Javier Nieves, Quevedo Sanchez, Bernabe
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Rodriguez Ordonez, Juan Justino
Remacha, Javier Nieves
Quevedo Sanchez, Bernabe
description A method for reducing yellowness of a polyetherimide solution, including exposing a first solution including a solvent and a polyetherimide to light under conditions effective to provide a second solution having a yellowness index that is 1 to 100 units less than the yellowness index of the first solution, as determined according to ASTM D1925. Another aspect is a method for reducing yellowness of a polyetherimide solution including acidifying a first solution including a solvent and a polyetherimide to provide a second solution having a pH less than 5 under conditions effective for the second solution to attain a yellowness index that is 1 to 30 units less than the yellowness index of the first solution, as determined according to ASTM D1925. Polyetherimides prepared according to the method, and compositions and articles including the polyetherimide are also described.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US10584211B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US10584211B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US10584211B23</originalsourceid><addsrcrecordid>eNqNzD0OwjAMBeAuDAi4g9mLRAtIzCAQCxMwV1HiUktpXMXhpyfimrSFqSxMlv2ev2H0OmIo2EDOHjyamyZ3hRqt5YdDESBn8Amcg4KKbd2U0VNJBuPeDoW6t7_qw6D5UWJQzoDmsmKhQOykOygfSFuULvEkLdKoPX4cDXJlBSffOYqm-915e5hhxRlKpTQ6DNnllMxX62WaJJt08U_nDZpVWVU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for reducing yellowness index of a polyetherimide, polyetherimide having a reduced yellowness index, and compositions and articles comprising the polyetherimide</title><source>esp@cenet</source><creator>Rodriguez Ordonez, Juan Justino ; Remacha, Javier Nieves ; Quevedo Sanchez, Bernabe</creator><creatorcontrib>Rodriguez Ordonez, Juan Justino ; Remacha, Javier Nieves ; Quevedo Sanchez, Bernabe</creatorcontrib><description>A method for reducing yellowness of a polyetherimide solution, including exposing a first solution including a solvent and a polyetherimide to light under conditions effective to provide a second solution having a yellowness index that is 1 to 100 units less than the yellowness index of the first solution, as determined according to ASTM D1925. Another aspect is a method for reducing yellowness of a polyetherimide solution including acidifying a first solution including a solvent and a polyetherimide to provide a second solution having a pH less than 5 under conditions effective for the second solution to attain a yellowness index that is 1 to 30 units less than the yellowness index of the first solution, as determined according to ASTM D1925. Polyetherimides prepared according to the method, and compositions and articles including the polyetherimide are also described.</description><language>eng</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; GENERAL PROCESSES OF COMPOUNDING ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; WORKING-UP</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200310&amp;DB=EPODOC&amp;CC=US&amp;NR=10584211B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200310&amp;DB=EPODOC&amp;CC=US&amp;NR=10584211B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Rodriguez Ordonez, Juan Justino</creatorcontrib><creatorcontrib>Remacha, Javier Nieves</creatorcontrib><creatorcontrib>Quevedo Sanchez, Bernabe</creatorcontrib><title>Method for reducing yellowness index of a polyetherimide, polyetherimide having a reduced yellowness index, and compositions and articles comprising the polyetherimide</title><description>A method for reducing yellowness of a polyetherimide solution, including exposing a first solution including a solvent and a polyetherimide to light under conditions effective to provide a second solution having a yellowness index that is 1 to 100 units less than the yellowness index of the first solution, as determined according to ASTM D1925. Another aspect is a method for reducing yellowness of a polyetherimide solution including acidifying a first solution including a solvent and a polyetherimide to provide a second solution having a pH less than 5 under conditions effective for the second solution to attain a yellowness index that is 1 to 30 units less than the yellowness index of the first solution, as determined according to ASTM D1925. Polyetherimides prepared according to the method, and compositions and articles including the polyetherimide are also described.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNzD0OwjAMBeAuDAi4g9mLRAtIzCAQCxMwV1HiUktpXMXhpyfimrSFqSxMlv2ev2H0OmIo2EDOHjyamyZ3hRqt5YdDESBn8Amcg4KKbd2U0VNJBuPeDoW6t7_qw6D5UWJQzoDmsmKhQOykOygfSFuULvEkLdKoPX4cDXJlBSffOYqm-915e5hhxRlKpTQ6DNnllMxX62WaJJt08U_nDZpVWVU</recordid><startdate>20200310</startdate><enddate>20200310</enddate><creator>Rodriguez Ordonez, Juan Justino</creator><creator>Remacha, Javier Nieves</creator><creator>Quevedo Sanchez, Bernabe</creator><scope>EVB</scope></search><sort><creationdate>20200310</creationdate><title>Method for reducing yellowness index of a polyetherimide, polyetherimide having a reduced yellowness index, and compositions and articles comprising the polyetherimide</title><author>Rodriguez Ordonez, Juan Justino ; Remacha, Javier Nieves ; Quevedo Sanchez, Bernabe</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US10584211B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2020</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>Rodriguez Ordonez, Juan Justino</creatorcontrib><creatorcontrib>Remacha, Javier Nieves</creatorcontrib><creatorcontrib>Quevedo Sanchez, Bernabe</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Rodriguez Ordonez, Juan Justino</au><au>Remacha, Javier Nieves</au><au>Quevedo Sanchez, Bernabe</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for reducing yellowness index of a polyetherimide, polyetherimide having a reduced yellowness index, and compositions and articles comprising the polyetherimide</title><date>2020-03-10</date><risdate>2020</risdate><abstract>A method for reducing yellowness of a polyetherimide solution, including exposing a first solution including a solvent and a polyetherimide to light under conditions effective to provide a second solution having a yellowness index that is 1 to 100 units less than the yellowness index of the first solution, as determined according to ASTM D1925. Another aspect is a method for reducing yellowness of a polyetherimide solution including acidifying a first solution including a solvent and a polyetherimide to provide a second solution having a pH less than 5 under conditions effective for the second solution to attain a yellowness index that is 1 to 30 units less than the yellowness index of the first solution, as determined according to ASTM D1925. Polyetherimides prepared according to the method, and compositions and articles including the polyetherimide are also described.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US10584211B2
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
GENERAL PROCESSES OF COMPOUNDING
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
WORKING-UP
title Method for reducing yellowness index of a polyetherimide, polyetherimide having a reduced yellowness index, and compositions and articles comprising the polyetherimide
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T07%3A26%3A49IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Rodriguez%20Ordonez,%20Juan%20Justino&rft.date=2020-03-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS10584211B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true