Nickel-cobalt-manganese complex hydroxide particles and method for producing same, positive electrode active material for nonaqueous electrolyte secondary battery and method for producing same, and nonaqueous electrolyte second battery
A method for producing a nickel cobalt manganese composite hydroxide by a crystallization reaction is provided. The method includes: a nucleation step of performing nucleation by controlling a pH of an aqueous solution for nucleation including metal compounds containing nickel, cobalt and manganese,...
Gespeichert in:
Hauptverfasser: | , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | Nagai, Hiroki Ryoshi, Kazuomi Imaizumi, Shin Osako, Toshiyuki Mori, Kensaku Ikeuchi, Kenji Toya, Hiroyuki Fukui, Atsushi |
description | A method for producing a nickel cobalt manganese composite hydroxide by a crystallization reaction is provided. The method includes: a nucleation step of performing nucleation by controlling a pH of an aqueous solution for nucleation including metal compounds containing nickel, cobalt and manganese, and an ammonium ion donor to 12.0 to 14.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard; and a particle growth step of growing nuclei by controlling a pH of an aqueous solution for particle growth containing nuclei formed in the nucleation step to 10.5 to 12.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US10490815B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US10490815B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US10490815B23</originalsourceid><addsrcrecordid>eNqNjTFPQkEQhF9DYdT_sPa-BEQTbTESKxuxJsveABfubo-7fYT3m_0TApEWrSaZ-Wbmqvn-8LJBaEUXHKyNnFacUEGiMQfsad27onvvQJmLeQmoxMlRhK3V0VIL5aKuE59WVDninrJWb34HQoDYIQSxnIzIhuI5nGpJE287aFfPYOgNVCGaHJeeFmwHvP_r7hhf3DoP3TSDJYeK21-9bu6mb7PX9xZZ56iZBQk2__ocDR9fhs-jp8nD-D_MD3bpc44</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Nickel-cobalt-manganese complex hydroxide particles and method for producing same, positive electrode active material for nonaqueous electrolyte secondary battery and method for producing same, and nonaqueous electrolyte second battery</title><source>esp@cenet</source><creator>Nagai, Hiroki ; Ryoshi, Kazuomi ; Imaizumi, Shin ; Osako, Toshiyuki ; Mori, Kensaku ; Ikeuchi, Kenji ; Toya, Hiroyuki ; Fukui, Atsushi</creator><creatorcontrib>Nagai, Hiroki ; Ryoshi, Kazuomi ; Imaizumi, Shin ; Osako, Toshiyuki ; Mori, Kensaku ; Ikeuchi, Kenji ; Toya, Hiroyuki ; Fukui, Atsushi</creatorcontrib><description>A method for producing a nickel cobalt manganese composite hydroxide by a crystallization reaction is provided. The method includes: a nucleation step of performing nucleation by controlling a pH of an aqueous solution for nucleation including metal compounds containing nickel, cobalt and manganese, and an ammonium ion donor to 12.0 to 14.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard; and a particle growth step of growing nuclei by controlling a pH of an aqueous solution for particle growth containing nuclei formed in the nucleation step to 10.5 to 12.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; ELECTRICITY ; INORGANIC CHEMISTRY ; METALLURGY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20191126&DB=EPODOC&CC=US&NR=10490815B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20191126&DB=EPODOC&CC=US&NR=10490815B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Nagai, Hiroki</creatorcontrib><creatorcontrib>Ryoshi, Kazuomi</creatorcontrib><creatorcontrib>Imaizumi, Shin</creatorcontrib><creatorcontrib>Osako, Toshiyuki</creatorcontrib><creatorcontrib>Mori, Kensaku</creatorcontrib><creatorcontrib>Ikeuchi, Kenji</creatorcontrib><creatorcontrib>Toya, Hiroyuki</creatorcontrib><creatorcontrib>Fukui, Atsushi</creatorcontrib><title>Nickel-cobalt-manganese complex hydroxide particles and method for producing same, positive electrode active material for nonaqueous electrolyte secondary battery and method for producing same, and nonaqueous electrolyte second battery</title><description>A method for producing a nickel cobalt manganese composite hydroxide by a crystallization reaction is provided. The method includes: a nucleation step of performing nucleation by controlling a pH of an aqueous solution for nucleation including metal compounds containing nickel, cobalt and manganese, and an ammonium ion donor to 12.0 to 14.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard; and a particle growth step of growing nuclei by controlling a pH of an aqueous solution for particle growth containing nuclei formed in the nucleation step to 10.5 to 12.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjTFPQkEQhF9DYdT_sPa-BEQTbTESKxuxJsveABfubo-7fYT3m_0TApEWrSaZ-Wbmqvn-8LJBaEUXHKyNnFacUEGiMQfsad27onvvQJmLeQmoxMlRhK3V0VIL5aKuE59WVDninrJWb34HQoDYIQSxnIzIhuI5nGpJE287aFfPYOgNVCGaHJeeFmwHvP_r7hhf3DoP3TSDJYeK21-9bu6mb7PX9xZZ56iZBQk2__ocDR9fhs-jp8nD-D_MD3bpc44</recordid><startdate>20191126</startdate><enddate>20191126</enddate><creator>Nagai, Hiroki</creator><creator>Ryoshi, Kazuomi</creator><creator>Imaizumi, Shin</creator><creator>Osako, Toshiyuki</creator><creator>Mori, Kensaku</creator><creator>Ikeuchi, Kenji</creator><creator>Toya, Hiroyuki</creator><creator>Fukui, Atsushi</creator><scope>EVB</scope></search><sort><creationdate>20191126</creationdate><title>Nickel-cobalt-manganese complex hydroxide particles and method for producing same, positive electrode active material for nonaqueous electrolyte secondary battery and method for producing same, and nonaqueous electrolyte second battery</title><author>Nagai, Hiroki ; Ryoshi, Kazuomi ; Imaizumi, Shin ; Osako, Toshiyuki ; Mori, Kensaku ; Ikeuchi, Kenji ; Toya, Hiroyuki ; Fukui, Atsushi</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US10490815B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2019</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>Nagai, Hiroki</creatorcontrib><creatorcontrib>Ryoshi, Kazuomi</creatorcontrib><creatorcontrib>Imaizumi, Shin</creatorcontrib><creatorcontrib>Osako, Toshiyuki</creatorcontrib><creatorcontrib>Mori, Kensaku</creatorcontrib><creatorcontrib>Ikeuchi, Kenji</creatorcontrib><creatorcontrib>Toya, Hiroyuki</creatorcontrib><creatorcontrib>Fukui, Atsushi</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Nagai, Hiroki</au><au>Ryoshi, Kazuomi</au><au>Imaizumi, Shin</au><au>Osako, Toshiyuki</au><au>Mori, Kensaku</au><au>Ikeuchi, Kenji</au><au>Toya, Hiroyuki</au><au>Fukui, Atsushi</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Nickel-cobalt-manganese complex hydroxide particles and method for producing same, positive electrode active material for nonaqueous electrolyte secondary battery and method for producing same, and nonaqueous electrolyte second battery</title><date>2019-11-26</date><risdate>2019</risdate><abstract>A method for producing a nickel cobalt manganese composite hydroxide by a crystallization reaction is provided. The method includes: a nucleation step of performing nucleation by controlling a pH of an aqueous solution for nucleation including metal compounds containing nickel, cobalt and manganese, and an ammonium ion donor to 12.0 to 14.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard; and a particle growth step of growing nuclei by controlling a pH of an aqueous solution for particle growth containing nuclei formed in the nucleation step to 10.5 to 12.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US10490815B2 |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS CHEMISTRY COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ELECTRICITY INORGANIC CHEMISTRY METALLURGY PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY |
title | Nickel-cobalt-manganese complex hydroxide particles and method for producing same, positive electrode active material for nonaqueous electrolyte secondary battery and method for producing same, and nonaqueous electrolyte second battery |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-10T09%3A23%3A49IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Nagai,%20Hiroki&rft.date=2019-11-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS10490815B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |