METHOD FOR FORMING LEAD - ACID BATTERIES AND AN INSTALLATION FOR EMBODIMENT OF THE METHOD

A method for forming lead-acid batteries (2) that comprises the following stages: a first electrolyte (7) at a given concentration and constant temperature is collected from a first tank (5); said first electrolyte (7) is distributed to the batteries; said first electrolyte (7) is circulated continu...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: STOCCHIERO, FRANCO
Format: Patent
Sprache:eng ; rus ; ukr
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator STOCCHIERO, FRANCO
description A method for forming lead-acid batteries (2) that comprises the following stages: a first electrolyte (7) at a given concentration and constant temperature is collected from a first tank (5); said first electrolyte (7) is distributed to the batteries; said first electrolyte (7) is circulated continuously at predetermined and substantially constant concentration and temperature for a preset amount of time; said batteries are powered with a direct current during the circulation of said first electrolyte (7) for a given initial charge time; the circulation of said first electrolyte (7) is cut off and a second electrolyte (8) is circulated in said batteries, said second electrolyte being collected from a second tank (6), at a greater concentration than the previous electrolyte and at a preset and substantially constant temperature for a further preset time; said batteries are powered with a direct current during the circulation of said second electrolyte (8) for a preset second charge time. Способ формирования свинцово-кислотных аккумуляторов (2), который включает такие стадии: отбор первого электролита (7) при определенной концентрации и постоянной температуре с первого резервуара (5); распределение упомянутого первого электролита (7) по аккумуляторам; обеспечение беспрерывной циркуляции упомянутого первого электролита (7) при заданных практически постоянных концентрации и температуре в течение заданного времени; питание упомянутых аккумуляторов постоянным током во время циркуляции упомянутого первого электролита (7) в течение заданного времени начального заряда; прекращение циркуляции упомянутого первого электро� Спосіб формування свинцево-кислотних акумуляторів (2), який включає такі стадії: відбирання першого електроліту (7) при певній концентрації та постійній температурі з першого резервуара (5); розподілення згаданого першого електроліту (7) по акумуляторах; забезпечення безперервної циркуляції згаданого першого електроліту (7) при заданих практично постійних концентрації та температурі протягом заданого часу; живлення згаданих акумуляторів постійним струмом під час циркуляції згаданого першого електроліту (7) протягом заданого часу початкового заряджання; припинення циркуляції згаданого першого електроліту (7) та забезпечення циркуляції в згаданих акумуляторах протягом другого заданого часу другого електроліту (8), який відбирають із другого резервуара (6), при заздалегідь визначених та практично постійних концентрації та температурі; живлення згаданих
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_UA83490C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>UA83490C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_UA83490C23</originalsourceid><addsrcrecordid>eNrjZIj0dQ3x8HdRcPMPAmFfTz93BR9XRxcFXQVHZ08XBSfHkBDXIE_XYAVHPxcgVvD0Cw5x9PFxDPH09wPrcvV18nfx9HX1C1Hwd1MI8XBVgBjJw8CalphTnMoLpbkZ5NxcQ5w9dFML8uNTiwsSk1PzUkviQx0tjE0sDZyNjAkqAACT8y-D</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR FORMING LEAD - ACID BATTERIES AND AN INSTALLATION FOR EMBODIMENT OF THE METHOD</title><source>esp@cenet</source><creator>STOCCHIERO, FRANCO</creator><creatorcontrib>STOCCHIERO, FRANCO</creatorcontrib><description>A method for forming lead-acid batteries (2) that comprises the following stages: a first electrolyte (7) at a given concentration and constant temperature is collected from a first tank (5); said first electrolyte (7) is distributed to the batteries; said first electrolyte (7) is circulated continuously at predetermined and substantially constant concentration and temperature for a preset amount of time; said batteries are powered with a direct current during the circulation of said first electrolyte (7) for a given initial charge time; the circulation of said first electrolyte (7) is cut off and a second electrolyte (8) is circulated in said batteries, said second electrolyte being collected from a second tank (6), at a greater concentration than the previous electrolyte and at a preset and substantially constant temperature for a further preset time; said batteries are powered with a direct current during the circulation of said second electrolyte (8) for a preset second charge time. Способ формирования свинцово-кислотных аккумуляторов (2), который включает такие стадии: отбор первого электролита (7) при определенной концентрации и постоянной температуре с первого резервуара (5); распределение упомянутого первого электролита (7) по аккумуляторам; обеспечение беспрерывной циркуляции упомянутого первого электролита (7) при заданных практически постоянных концентрации и температуре в течение заданного времени; питание упомянутых аккумуляторов постоянным током во время циркуляции упомянутого первого электролита (7) в течение заданного времени начального заряда; прекращение циркуляции упомянутого первого электро� Спосіб формування свинцево-кислотних акумуляторів (2), який включає такі стадії: відбирання першого електроліту (7) при певній концентрації та постійній температурі з першого резервуара (5); розподілення згаданого першого електроліту (7) по акумуляторах; забезпечення безперервної циркуляції згаданого першого електроліту (7) при заданих практично постійних концентрації та температурі протягом заданого часу; живлення згаданих акумуляторів постійним струмом під час циркуляції згаданого першого електроліту (7) протягом заданого часу початкового заряджання; припинення циркуляції згаданого першого електроліту (7) та забезпечення циркуляції в згаданих акумуляторах протягом другого заданого часу другого електроліту (8), який відбирають із другого резервуара (6), при заздалегідь визначених та практично постійних концентрації та температурі; живлення згаданих акумуляторів постійним струмом під час циркуляції згаданого другого електроліту (8) протягом заданого часу другого заряджання.</description><language>eng ; rus ; ukr</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2008</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20080725&amp;DB=EPODOC&amp;CC=UA&amp;NR=83490C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20080725&amp;DB=EPODOC&amp;CC=UA&amp;NR=83490C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>STOCCHIERO, FRANCO</creatorcontrib><title>METHOD FOR FORMING LEAD - ACID BATTERIES AND AN INSTALLATION FOR EMBODIMENT OF THE METHOD</title><description>A method for forming lead-acid batteries (2) that comprises the following stages: a first electrolyte (7) at a given concentration and constant temperature is collected from a first tank (5); said first electrolyte (7) is distributed to the batteries; said first electrolyte (7) is circulated continuously at predetermined and substantially constant concentration and temperature for a preset amount of time; said batteries are powered with a direct current during the circulation of said first electrolyte (7) for a given initial charge time; the circulation of said first electrolyte (7) is cut off and a second electrolyte (8) is circulated in said batteries, said second electrolyte being collected from a second tank (6), at a greater concentration than the previous electrolyte and at a preset and substantially constant temperature for a further preset time; said batteries are powered with a direct current during the circulation of said second electrolyte (8) for a preset second charge time. Способ формирования свинцово-кислотных аккумуляторов (2), который включает такие стадии: отбор первого электролита (7) при определенной концентрации и постоянной температуре с первого резервуара (5); распределение упомянутого первого электролита (7) по аккумуляторам; обеспечение беспрерывной циркуляции упомянутого первого электролита (7) при заданных практически постоянных концентрации и температуре в течение заданного времени; питание упомянутых аккумуляторов постоянным током во время циркуляции упомянутого первого электролита (7) в течение заданного времени начального заряда; прекращение циркуляции упомянутого первого электро� Спосіб формування свинцево-кислотних акумуляторів (2), який включає такі стадії: відбирання першого електроліту (7) при певній концентрації та постійній температурі з першого резервуара (5); розподілення згаданого першого електроліту (7) по акумуляторах; забезпечення безперервної циркуляції згаданого першого електроліту (7) при заданих практично постійних концентрації та температурі протягом заданого часу; живлення згаданих акумуляторів постійним струмом під час циркуляції згаданого першого електроліту (7) протягом заданого часу початкового заряджання; припинення циркуляції згаданого першого електроліту (7) та забезпечення циркуляції в згаданих акумуляторах протягом другого заданого часу другого електроліту (8), який відбирають із другого резервуара (6), при заздалегідь визначених та практично постійних концентрації та температурі; живлення згаданих акумуляторів постійним струмом під час циркуляції згаданого другого електроліту (8) протягом заданого часу другого заряджання.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2008</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZIj0dQ3x8HdRcPMPAmFfTz93BR9XRxcFXQVHZ08XBSfHkBDXIE_XYAVHPxcgVvD0Cw5x9PFxDPH09wPrcvV18nfx9HX1C1Hwd1MI8XBVgBjJw8CalphTnMoLpbkZ5NxcQ5w9dFML8uNTiwsSk1PzUkviQx0tjE0sDZyNjAkqAACT8y-D</recordid><startdate>20080725</startdate><enddate>20080725</enddate><creator>STOCCHIERO, FRANCO</creator><scope>EVB</scope></search><sort><creationdate>20080725</creationdate><title>METHOD FOR FORMING LEAD - ACID BATTERIES AND AN INSTALLATION FOR EMBODIMENT OF THE METHOD</title><author>STOCCHIERO, FRANCO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_UA83490C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus ; ukr</language><creationdate>2008</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>STOCCHIERO, FRANCO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>STOCCHIERO, FRANCO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR FORMING LEAD - ACID BATTERIES AND AN INSTALLATION FOR EMBODIMENT OF THE METHOD</title><date>2008-07-25</date><risdate>2008</risdate><abstract>A method for forming lead-acid batteries (2) that comprises the following stages: a first electrolyte (7) at a given concentration and constant temperature is collected from a first tank (5); said first electrolyte (7) is distributed to the batteries; said first electrolyte (7) is circulated continuously at predetermined and substantially constant concentration and temperature for a preset amount of time; said batteries are powered with a direct current during the circulation of said first electrolyte (7) for a given initial charge time; the circulation of said first electrolyte (7) is cut off and a second electrolyte (8) is circulated in said batteries, said second electrolyte being collected from a second tank (6), at a greater concentration than the previous electrolyte and at a preset and substantially constant temperature for a further preset time; said batteries are powered with a direct current during the circulation of said second electrolyte (8) for a preset second charge time. Способ формирования свинцово-кислотных аккумуляторов (2), который включает такие стадии: отбор первого электролита (7) при определенной концентрации и постоянной температуре с первого резервуара (5); распределение упомянутого первого электролита (7) по аккумуляторам; обеспечение беспрерывной циркуляции упомянутого первого электролита (7) при заданных практически постоянных концентрации и температуре в течение заданного времени; питание упомянутых аккумуляторов постоянным током во время циркуляции упомянутого первого электролита (7) в течение заданного времени начального заряда; прекращение циркуляции упомянутого первого электро� Спосіб формування свинцево-кислотних акумуляторів (2), який включає такі стадії: відбирання першого електроліту (7) при певній концентрації та постійній температурі з першого резервуара (5); розподілення згаданого першого електроліту (7) по акумуляторах; забезпечення безперервної циркуляції згаданого першого електроліту (7) при заданих практично постійних концентрації та температурі протягом заданого часу; живлення згаданих акумуляторів постійним струмом під час циркуляції згаданого першого електроліту (7) протягом заданого часу початкового заряджання; припинення циркуляції згаданого першого електроліту (7) та забезпечення циркуляції в згаданих акумуляторах протягом другого заданого часу другого електроліту (8), який відбирають із другого резервуара (6), при заздалегідь визначених та практично постійних концентрації та температурі; живлення згаданих акумуляторів постійним струмом під час циркуляції згаданого другого електроліту (8) протягом заданого часу другого заряджання.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus ; ukr
recordid cdi_epo_espacenet_UA83490C2
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title METHOD FOR FORMING LEAD - ACID BATTERIES AND AN INSTALLATION FOR EMBODIMENT OF THE METHOD
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-09T15%3A04%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=STOCCHIERO,%20FRANCO&rft.date=2008-07-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUA83490C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true