A METHOD FOR PREPARING MARKETABLE ELECTRODE PITCHES
A method for preparing marketable electrode pitches by two-stage thermal treatment in delivery of pitch air at the temperature of softening not more than 60 DEGREE C. According to the invention at the first stage of the pitch thermal treatment 2/3 of air amount to the specified one, at the second st...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | KAUFMAN SEMEN ILLICH VLASOV HENNADII OLEKSANDROVYCH PITIULIN IHOR NARKYSOVYCH PECHIN VALENTYN STEPANOVYCH |
description | A method for preparing marketable electrode pitches by two-stage thermal treatment in delivery of pitch air at the temperature of softening not more than 60 DEGREE C. According to the invention at the first stage of the pitch thermal treatment 2/3 of air amount to the specified one, at the second stage 1/3 of air amount to the specified amount is delivered, the obtained high-temperature pitch is mixed with previously refined turbulized high-boiling distillate fraction, at that consumption of high-boiling distillate fraction is equal to 100-250 kg per 1 ton depending on pitch grade being obtained and quality pitch and distillate fraction to be mixed. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_UA72763C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>UA72763C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_UA72763C23</originalsourceid><addsrcrecordid>eNrjZDB2VPB1DfHwd1Fw8w9SCAhyDXAM8vRzV_B1DPJ2DXF08nFVcPVxdQ4J8ndxVQjwDHH2cA3mYWBNS8wpTuWF0twMcm6uQBnd1IL8-NTigsTk1LzUkvhQR3MjczNjZyNjggoAq0AlyA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>A METHOD FOR PREPARING MARKETABLE ELECTRODE PITCHES</title><source>esp@cenet</source><creator>KAUFMAN SEMEN ILLICH ; VLASOV HENNADII OLEKSANDROVYCH ; PITIULIN IHOR NARKYSOVYCH ; PECHIN VALENTYN STEPANOVYCH</creator><creatorcontrib>KAUFMAN SEMEN ILLICH ; VLASOV HENNADII OLEKSANDROVYCH ; PITIULIN IHOR NARKYSOVYCH ; PECHIN VALENTYN STEPANOVYCH</creatorcontrib><description>A method for preparing marketable electrode pitches by two-stage thermal treatment in delivery of pitch air at the temperature of softening not more than 60 DEGREE C. According to the invention at the first stage of the pitch thermal treatment 2/3 of air amount to the specified one, at the second stage 1/3 of air amount to the specified amount is delivered, the obtained high-temperature pitch is mixed with previously refined turbulized high-boiling distillate fraction, at that consumption of high-boiling distillate fraction is equal to 100-250 kg per 1 ton depending on pitch grade being obtained and quality pitch and distillate fraction to be mixed.</description><edition>7</edition><language>eng</language><subject>CHEMISTRY ; FUELS ; LUBRICANTS ; METALLURGY ; PEAT ; PETROLEUM, GAS OR COKE INDUSTRIES ; PYROLIGNEOUS ACID ; TECHNICAL GASES CONTAINING CARBON MONOXIDE ; WORKING-UP PITCH, ASPHALT, BITUMEN, TAR</subject><creationdate>2005</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20050415&DB=EPODOC&CC=UA&NR=72763C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20050415&DB=EPODOC&CC=UA&NR=72763C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KAUFMAN SEMEN ILLICH</creatorcontrib><creatorcontrib>VLASOV HENNADII OLEKSANDROVYCH</creatorcontrib><creatorcontrib>PITIULIN IHOR NARKYSOVYCH</creatorcontrib><creatorcontrib>PECHIN VALENTYN STEPANOVYCH</creatorcontrib><title>A METHOD FOR PREPARING MARKETABLE ELECTRODE PITCHES</title><description>A method for preparing marketable electrode pitches by two-stage thermal treatment in delivery of pitch air at the temperature of softening not more than 60 DEGREE C. According to the invention at the first stage of the pitch thermal treatment 2/3 of air amount to the specified one, at the second stage 1/3 of air amount to the specified amount is delivered, the obtained high-temperature pitch is mixed with previously refined turbulized high-boiling distillate fraction, at that consumption of high-boiling distillate fraction is equal to 100-250 kg per 1 ton depending on pitch grade being obtained and quality pitch and distillate fraction to be mixed.</description><subject>CHEMISTRY</subject><subject>FUELS</subject><subject>LUBRICANTS</subject><subject>METALLURGY</subject><subject>PEAT</subject><subject>PETROLEUM, GAS OR COKE INDUSTRIES</subject><subject>PYROLIGNEOUS ACID</subject><subject>TECHNICAL GASES CONTAINING CARBON MONOXIDE</subject><subject>WORKING-UP PITCH, ASPHALT, BITUMEN, TAR</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2005</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDB2VPB1DfHwd1Fw8w9SCAhyDXAM8vRzV_B1DPJ2DXF08nFVcPVxdQ4J8ndxVQjwDHH2cA3mYWBNS8wpTuWF0twMcm6uQBnd1IL8-NTigsTk1LzUkvhQR3MjczNjZyNjggoAq0AlyA</recordid><startdate>20050415</startdate><enddate>20050415</enddate><creator>KAUFMAN SEMEN ILLICH</creator><creator>VLASOV HENNADII OLEKSANDROVYCH</creator><creator>PITIULIN IHOR NARKYSOVYCH</creator><creator>PECHIN VALENTYN STEPANOVYCH</creator><scope>EVB</scope></search><sort><creationdate>20050415</creationdate><title>A METHOD FOR PREPARING MARKETABLE ELECTRODE PITCHES</title><author>KAUFMAN SEMEN ILLICH ; VLASOV HENNADII OLEKSANDROVYCH ; PITIULIN IHOR NARKYSOVYCH ; PECHIN VALENTYN STEPANOVYCH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_UA72763C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2005</creationdate><topic>CHEMISTRY</topic><topic>FUELS</topic><topic>LUBRICANTS</topic><topic>METALLURGY</topic><topic>PEAT</topic><topic>PETROLEUM, GAS OR COKE INDUSTRIES</topic><topic>PYROLIGNEOUS ACID</topic><topic>TECHNICAL GASES CONTAINING CARBON MONOXIDE</topic><topic>WORKING-UP PITCH, ASPHALT, BITUMEN, TAR</topic><toplevel>online_resources</toplevel><creatorcontrib>KAUFMAN SEMEN ILLICH</creatorcontrib><creatorcontrib>VLASOV HENNADII OLEKSANDROVYCH</creatorcontrib><creatorcontrib>PITIULIN IHOR NARKYSOVYCH</creatorcontrib><creatorcontrib>PECHIN VALENTYN STEPANOVYCH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KAUFMAN SEMEN ILLICH</au><au>VLASOV HENNADII OLEKSANDROVYCH</au><au>PITIULIN IHOR NARKYSOVYCH</au><au>PECHIN VALENTYN STEPANOVYCH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>A METHOD FOR PREPARING MARKETABLE ELECTRODE PITCHES</title><date>2005-04-15</date><risdate>2005</risdate><abstract>A method for preparing marketable electrode pitches by two-stage thermal treatment in delivery of pitch air at the temperature of softening not more than 60 DEGREE C. According to the invention at the first stage of the pitch thermal treatment 2/3 of air amount to the specified one, at the second stage 1/3 of air amount to the specified amount is delivered, the obtained high-temperature pitch is mixed with previously refined turbulized high-boiling distillate fraction, at that consumption of high-boiling distillate fraction is equal to 100-250 kg per 1 ton depending on pitch grade being obtained and quality pitch and distillate fraction to be mixed.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_UA72763C2 |
source | esp@cenet |
subjects | CHEMISTRY FUELS LUBRICANTS METALLURGY PEAT PETROLEUM, GAS OR COKE INDUSTRIES PYROLIGNEOUS ACID TECHNICAL GASES CONTAINING CARBON MONOXIDE WORKING-UP PITCH, ASPHALT, BITUMEN, TAR |
title | A METHOD FOR PREPARING MARKETABLE ELECTRODE PITCHES |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-19T05%3A37%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KAUFMAN%20SEMEN%20ILLICH&rft.date=2005-04-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUA72763C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |