METHOD FOR WASHING BLAST-FURNACE HEARTH
Method for washing blast-furnace hearth includes periodical charging to the ore part the charge of washing materials in amount of 1.5 - 3 % of the total mass of the charge, with its melting. Washing materials are included to the charge in portions between the following cast iron discharges, at that...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | PEFTIIEV YEVHEN IHOROVYCH KOVAL VALENTYN ANDRIIOVYCH KAMARDIN MYKOLA OLEKSIIOVYCH DIDEVYCH ANATOLII VASYLIOVYCH BILYI OLEKSII PETROVYCH OVCHYNNIKOV MYKOLA OLEKSIIOVYCH CHOTYRKYN YEVHEN IVANOVYCH ZOTOV OLEKSII VOLODYMYROVYCH FYLYPPOV OLEKSANDR OLEKSIIOVYCH VASKEVYCH MYKHAILO YAKOVYCH |
description | Method for washing blast-furnace hearth includes periodical charging to the ore part the charge of washing materials in amount of 1.5 - 3 % of the total mass of the charge, with its melting. Washing materials are included to the charge in portions between the following cast iron discharges, at that the mass of each portion is determined by the dependence. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_UA68521A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>UA68521A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_UA68521A3</originalsourceid><addsrcrecordid>eNrjZFD3dQ3x8HdRcPMPUgh3DPbw9HNXcPJxDA7RdQsN8nN0dlXwcHUMCvHgYWBNS8wpTuWF0twMsm6uIc4euqkF-fGpxQWJyal5qSXxoY5mFqZGho7GhOQByy4iGA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR WASHING BLAST-FURNACE HEARTH</title><source>esp@cenet</source><creator>PEFTIIEV YEVHEN IHOROVYCH ; KOVAL VALENTYN ANDRIIOVYCH ; KAMARDIN MYKOLA OLEKSIIOVYCH ; DIDEVYCH ANATOLII VASYLIOVYCH ; BILYI OLEKSII PETROVYCH ; OVCHYNNIKOV MYKOLA OLEKSIIOVYCH ; CHOTYRKYN YEVHEN IVANOVYCH ; ZOTOV OLEKSII VOLODYMYROVYCH ; FYLYPPOV OLEKSANDR OLEKSIIOVYCH ; VASKEVYCH MYKHAILO YAKOVYCH</creator><creatorcontrib>PEFTIIEV YEVHEN IHOROVYCH ; KOVAL VALENTYN ANDRIIOVYCH ; KAMARDIN MYKOLA OLEKSIIOVYCH ; DIDEVYCH ANATOLII VASYLIOVYCH ; BILYI OLEKSII PETROVYCH ; OVCHYNNIKOV MYKOLA OLEKSIIOVYCH ; CHOTYRKYN YEVHEN IVANOVYCH ; ZOTOV OLEKSII VOLODYMYROVYCH ; FYLYPPOV OLEKSANDR OLEKSIIOVYCH ; VASKEVYCH MYKHAILO YAKOVYCH</creatorcontrib><description>Method for washing blast-furnace hearth includes periodical charging to the ore part the charge of washing materials in amount of 1.5 - 3 % of the total mass of the charge, with its melting. Washing materials are included to the charge in portions between the following cast iron discharges, at that the mass of each portion is determined by the dependence.</description><edition>7</edition><language>eng</language><subject>CHEMISTRY ; MANUFACTURE OF IRON OR STEEL ; METALLURGY ; METALLURGY OF IRON</subject><creationdate>2004</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20040816&DB=EPODOC&CC=UA&NR=68521A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20040816&DB=EPODOC&CC=UA&NR=68521A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>PEFTIIEV YEVHEN IHOROVYCH</creatorcontrib><creatorcontrib>KOVAL VALENTYN ANDRIIOVYCH</creatorcontrib><creatorcontrib>KAMARDIN MYKOLA OLEKSIIOVYCH</creatorcontrib><creatorcontrib>DIDEVYCH ANATOLII VASYLIOVYCH</creatorcontrib><creatorcontrib>BILYI OLEKSII PETROVYCH</creatorcontrib><creatorcontrib>OVCHYNNIKOV MYKOLA OLEKSIIOVYCH</creatorcontrib><creatorcontrib>CHOTYRKYN YEVHEN IVANOVYCH</creatorcontrib><creatorcontrib>ZOTOV OLEKSII VOLODYMYROVYCH</creatorcontrib><creatorcontrib>FYLYPPOV OLEKSANDR OLEKSIIOVYCH</creatorcontrib><creatorcontrib>VASKEVYCH MYKHAILO YAKOVYCH</creatorcontrib><title>METHOD FOR WASHING BLAST-FURNACE HEARTH</title><description>Method for washing blast-furnace hearth includes periodical charging to the ore part the charge of washing materials in amount of 1.5 - 3 % of the total mass of the charge, with its melting. Washing materials are included to the charge in portions between the following cast iron discharges, at that the mass of each portion is determined by the dependence.</description><subject>CHEMISTRY</subject><subject>MANUFACTURE OF IRON OR STEEL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2004</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD3dQ3x8HdRcPMPUgh3DPbw9HNXcPJxDA7RdQsN8nN0dlXwcHUMCvHgYWBNS8wpTuWF0twMsm6uIc4euqkF-fGpxQWJyal5qSXxoY5mFqZGho7GhOQByy4iGA</recordid><startdate>20040816</startdate><enddate>20040816</enddate><creator>PEFTIIEV YEVHEN IHOROVYCH</creator><creator>KOVAL VALENTYN ANDRIIOVYCH</creator><creator>KAMARDIN MYKOLA OLEKSIIOVYCH</creator><creator>DIDEVYCH ANATOLII VASYLIOVYCH</creator><creator>BILYI OLEKSII PETROVYCH</creator><creator>OVCHYNNIKOV MYKOLA OLEKSIIOVYCH</creator><creator>CHOTYRKYN YEVHEN IVANOVYCH</creator><creator>ZOTOV OLEKSII VOLODYMYROVYCH</creator><creator>FYLYPPOV OLEKSANDR OLEKSIIOVYCH</creator><creator>VASKEVYCH MYKHAILO YAKOVYCH</creator><scope>EVB</scope></search><sort><creationdate>20040816</creationdate><title>METHOD FOR WASHING BLAST-FURNACE HEARTH</title><author>PEFTIIEV YEVHEN IHOROVYCH ; KOVAL VALENTYN ANDRIIOVYCH ; KAMARDIN MYKOLA OLEKSIIOVYCH ; DIDEVYCH ANATOLII VASYLIOVYCH ; BILYI OLEKSII PETROVYCH ; OVCHYNNIKOV MYKOLA OLEKSIIOVYCH ; CHOTYRKYN YEVHEN IVANOVYCH ; ZOTOV OLEKSII VOLODYMYROVYCH ; FYLYPPOV OLEKSANDR OLEKSIIOVYCH ; VASKEVYCH MYKHAILO YAKOVYCH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_UA68521A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2004</creationdate><topic>CHEMISTRY</topic><topic>MANUFACTURE OF IRON OR STEEL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><toplevel>online_resources</toplevel><creatorcontrib>PEFTIIEV YEVHEN IHOROVYCH</creatorcontrib><creatorcontrib>KOVAL VALENTYN ANDRIIOVYCH</creatorcontrib><creatorcontrib>KAMARDIN MYKOLA OLEKSIIOVYCH</creatorcontrib><creatorcontrib>DIDEVYCH ANATOLII VASYLIOVYCH</creatorcontrib><creatorcontrib>BILYI OLEKSII PETROVYCH</creatorcontrib><creatorcontrib>OVCHYNNIKOV MYKOLA OLEKSIIOVYCH</creatorcontrib><creatorcontrib>CHOTYRKYN YEVHEN IVANOVYCH</creatorcontrib><creatorcontrib>ZOTOV OLEKSII VOLODYMYROVYCH</creatorcontrib><creatorcontrib>FYLYPPOV OLEKSANDR OLEKSIIOVYCH</creatorcontrib><creatorcontrib>VASKEVYCH MYKHAILO YAKOVYCH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>PEFTIIEV YEVHEN IHOROVYCH</au><au>KOVAL VALENTYN ANDRIIOVYCH</au><au>KAMARDIN MYKOLA OLEKSIIOVYCH</au><au>DIDEVYCH ANATOLII VASYLIOVYCH</au><au>BILYI OLEKSII PETROVYCH</au><au>OVCHYNNIKOV MYKOLA OLEKSIIOVYCH</au><au>CHOTYRKYN YEVHEN IVANOVYCH</au><au>ZOTOV OLEKSII VOLODYMYROVYCH</au><au>FYLYPPOV OLEKSANDR OLEKSIIOVYCH</au><au>VASKEVYCH MYKHAILO YAKOVYCH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR WASHING BLAST-FURNACE HEARTH</title><date>2004-08-16</date><risdate>2004</risdate><abstract>Method for washing blast-furnace hearth includes periodical charging to the ore part the charge of washing materials in amount of 1.5 - 3 % of the total mass of the charge, with its melting. Washing materials are included to the charge in portions between the following cast iron discharges, at that the mass of each portion is determined by the dependence.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_UA68521A |
source | esp@cenet |
subjects | CHEMISTRY MANUFACTURE OF IRON OR STEEL METALLURGY METALLURGY OF IRON |
title | METHOD FOR WASHING BLAST-FURNACE HEARTH |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-03T20%3A28%3A31IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=PEFTIIEV%20YEVHEN%20IHOROVYCH&rft.date=2004-08-16&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUA68521A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |