METHOD FOR MELTING STEEL IN BASIC OPEN-HEARTH FURNACE

Method for melting steel in basic open-hearth furnace comprises of loading to the furnace scrap metal, oxidizers and mix of converter slag with limestone, before charging the scrap, with melting and finishing. First of all in separate portion oxidizers are loaded, and after those - mix of converter...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Koval Serhii Oleksiovych, Klimanchuk Vladyslav Vladyslavovych, Boiko Volodymyr Semenovych, Shebanits Eduard Mykolaiovych, Ostroushko Anatolii Viktorovych, Kladiti Heorhii Oleksandrovych, Fentisov Ihor Mykolaiovych, Yakin Mykhailo Mykolaiovych, Alioshyn Oleksandr Oleksandrovch, Prakhnin Viacheslav Leonidovych
Format: Patent
Sprache:eng ; rus ; ukr
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Koval Serhii Oleksiovych
Klimanchuk Vladyslav Vladyslavovych
Boiko Volodymyr Semenovych
Shebanits Eduard Mykolaiovych
Ostroushko Anatolii Viktorovych
Kladiti Heorhii Oleksandrovych
Fentisov Ihor Mykolaiovych
Yakin Mykhailo Mykolaiovych
Alioshyn Oleksandr Oleksandrovch
Prakhnin Viacheslav Leonidovych
description Method for melting steel in basic open-hearth furnace comprises of loading to the furnace scrap metal, oxidizers and mix of converter slag with limestone, before charging the scrap, with melting and finishing. First of all in separate portion oxidizers are loaded, and after those - mix of converter slag with limestone, at ratio 1:(1.5-2.5), at that the ration of the masses of the limestone, converter slag and oxidizers is (7.5- 4.5) : 3 : 1. Способ выплавки стали в основной мартеновской печи включает загрузку в печь металлолома, окислителей и смеси конвертерного шлака с известняком перед завалкой лома, плавление и доводку. Прежде всего засыпают отдельной порцией окислители, а после них - смесь конвертерного шлака с известняком в соотношении 1:(1,5-2,5), при этом соотношение между массами известняка, конвертерного шлака и окислителей составляет (7,5- 4,5) : 3:1. Спосіб виплавки сталі в основній мартенівській печі включає завантаження у піч металобрухту, окисників і суміші конвертерного шлаку із вапняком перед завалкою брухту, плавлення і доведення. Насамперед засипають окремою порцією окисники, а після них - суміш конвертерного шлаку із вапняком у співвідношенні 1:(1,5-2,5), при цьому співвідношення між масами вапняку, конвертерного шлаку і окисників становить (7,5- 4,5) : 3 : 1.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_UA53501A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>UA53501A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_UA53501A3</originalsourceid><addsrcrecordid>eNrjZDD1dQ3x8HdRcPMPUvB19Qnx9HNXCA5xdfVR8PRTcHIM9nRW8A9w9dP1cHUMCvFQcAsN8nN0duVhYE1LzClO5YXS3Ayybq4hzh66qQX58anFBYnJqXmpJfGhjqbGpgaGjsaE5AGcKiWn</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MELTING STEEL IN BASIC OPEN-HEARTH FURNACE</title><source>esp@cenet</source><creator>Koval Serhii Oleksiovych ; Klimanchuk Vladyslav Vladyslavovych ; Boiko Volodymyr Semenovych ; Shebanits Eduard Mykolaiovych ; Ostroushko Anatolii Viktorovych ; Kladiti Heorhii Oleksandrovych ; Fentisov Ihor Mykolaiovych ; Yakin Mykhailo Mykolaiovych ; Alioshyn Oleksandr Oleksandrovch ; Prakhnin Viacheslav Leonidovych</creator><creatorcontrib>Koval Serhii Oleksiovych ; Klimanchuk Vladyslav Vladyslavovych ; Boiko Volodymyr Semenovych ; Shebanits Eduard Mykolaiovych ; Ostroushko Anatolii Viktorovych ; Kladiti Heorhii Oleksandrovych ; Fentisov Ihor Mykolaiovych ; Yakin Mykhailo Mykolaiovych ; Alioshyn Oleksandr Oleksandrovch ; Prakhnin Viacheslav Leonidovych</creatorcontrib><description>Method for melting steel in basic open-hearth furnace comprises of loading to the furnace scrap metal, oxidizers and mix of converter slag with limestone, before charging the scrap, with melting and finishing. First of all in separate portion oxidizers are loaded, and after those - mix of converter slag with limestone, at ratio 1:(1.5-2.5), at that the ration of the masses of the limestone, converter slag and oxidizers is (7.5- 4.5) : 3 : 1. Способ выплавки стали в основной мартеновской печи включает загрузку в печь металлолома, окислителей и смеси конвертерного шлака с известняком перед завалкой лома, плавление и доводку. Прежде всего засыпают отдельной порцией окислители, а после них - смесь конвертерного шлака с известняком в соотношении 1:(1,5-2,5), при этом соотношение между массами известняка, конвертерного шлака и окислителей составляет (7,5- 4,5) : 3:1. Спосіб виплавки сталі в основній мартенівській печі включає завантаження у піч металобрухту, окисників і суміші конвертерного шлаку із вапняком перед завалкою брухту, плавлення і доведення. Насамперед засипають окремою порцією окисники, а після них - суміш конвертерного шлаку із вапняком у співвідношенні 1:(1,5-2,5), при цьому співвідношення між масами вапняку, конвертерного шлаку і окисників становить (7,5- 4,5) : 3 : 1.</description><language>eng ; rus ; ukr</language><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030115&amp;DB=EPODOC&amp;CC=UA&amp;NR=53501A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030115&amp;DB=EPODOC&amp;CC=UA&amp;NR=53501A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Koval Serhii Oleksiovych</creatorcontrib><creatorcontrib>Klimanchuk Vladyslav Vladyslavovych</creatorcontrib><creatorcontrib>Boiko Volodymyr Semenovych</creatorcontrib><creatorcontrib>Shebanits Eduard Mykolaiovych</creatorcontrib><creatorcontrib>Ostroushko Anatolii Viktorovych</creatorcontrib><creatorcontrib>Kladiti Heorhii Oleksandrovych</creatorcontrib><creatorcontrib>Fentisov Ihor Mykolaiovych</creatorcontrib><creatorcontrib>Yakin Mykhailo Mykolaiovych</creatorcontrib><creatorcontrib>Alioshyn Oleksandr Oleksandrovch</creatorcontrib><creatorcontrib>Prakhnin Viacheslav Leonidovych</creatorcontrib><title>METHOD FOR MELTING STEEL IN BASIC OPEN-HEARTH FURNACE</title><description>Method for melting steel in basic open-hearth furnace comprises of loading to the furnace scrap metal, oxidizers and mix of converter slag with limestone, before charging the scrap, with melting and finishing. First of all in separate portion oxidizers are loaded, and after those - mix of converter slag with limestone, at ratio 1:(1.5-2.5), at that the ration of the masses of the limestone, converter slag and oxidizers is (7.5- 4.5) : 3 : 1. Способ выплавки стали в основной мартеновской печи включает загрузку в печь металлолома, окислителей и смеси конвертерного шлака с известняком перед завалкой лома, плавление и доводку. Прежде всего засыпают отдельной порцией окислители, а после них - смесь конвертерного шлака с известняком в соотношении 1:(1,5-2,5), при этом соотношение между массами известняка, конвертерного шлака и окислителей составляет (7,5- 4,5) : 3:1. Спосіб виплавки сталі в основній мартенівській печі включає завантаження у піч металобрухту, окисників і суміші конвертерного шлаку із вапняком перед завалкою брухту, плавлення і доведення. Насамперед засипають окремою порцією окисники, а після них - суміш конвертерного шлаку із вапняком у співвідношенні 1:(1,5-2,5), при цьому співвідношення між масами вапняку, конвертерного шлаку і окисників становить (7,5- 4,5) : 3 : 1.</description><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD1dQ3x8HdRcPMPUvB19Qnx9HNXCA5xdfVR8PRTcHIM9nRW8A9w9dP1cHUMCvFQcAsN8nN0duVhYE1LzClO5YXS3Ayybq4hzh66qQX58anFBYnJqXmpJfGhjqbGpgaGjsaE5AGcKiWn</recordid><startdate>20030115</startdate><enddate>20030115</enddate><creator>Koval Serhii Oleksiovych</creator><creator>Klimanchuk Vladyslav Vladyslavovych</creator><creator>Boiko Volodymyr Semenovych</creator><creator>Shebanits Eduard Mykolaiovych</creator><creator>Ostroushko Anatolii Viktorovych</creator><creator>Kladiti Heorhii Oleksandrovych</creator><creator>Fentisov Ihor Mykolaiovych</creator><creator>Yakin Mykhailo Mykolaiovych</creator><creator>Alioshyn Oleksandr Oleksandrovch</creator><creator>Prakhnin Viacheslav Leonidovych</creator><scope>EVB</scope></search><sort><creationdate>20030115</creationdate><title>METHOD FOR MELTING STEEL IN BASIC OPEN-HEARTH FURNACE</title><author>Koval Serhii Oleksiovych ; Klimanchuk Vladyslav Vladyslavovych ; Boiko Volodymyr Semenovych ; Shebanits Eduard Mykolaiovych ; Ostroushko Anatolii Viktorovych ; Kladiti Heorhii Oleksandrovych ; Fentisov Ihor Mykolaiovych ; Yakin Mykhailo Mykolaiovych ; Alioshyn Oleksandr Oleksandrovch ; Prakhnin Viacheslav Leonidovych</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_UA53501A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus ; ukr</language><creationdate>2003</creationdate><toplevel>online_resources</toplevel><creatorcontrib>Koval Serhii Oleksiovych</creatorcontrib><creatorcontrib>Klimanchuk Vladyslav Vladyslavovych</creatorcontrib><creatorcontrib>Boiko Volodymyr Semenovych</creatorcontrib><creatorcontrib>Shebanits Eduard Mykolaiovych</creatorcontrib><creatorcontrib>Ostroushko Anatolii Viktorovych</creatorcontrib><creatorcontrib>Kladiti Heorhii Oleksandrovych</creatorcontrib><creatorcontrib>Fentisov Ihor Mykolaiovych</creatorcontrib><creatorcontrib>Yakin Mykhailo Mykolaiovych</creatorcontrib><creatorcontrib>Alioshyn Oleksandr Oleksandrovch</creatorcontrib><creatorcontrib>Prakhnin Viacheslav Leonidovych</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Koval Serhii Oleksiovych</au><au>Klimanchuk Vladyslav Vladyslavovych</au><au>Boiko Volodymyr Semenovych</au><au>Shebanits Eduard Mykolaiovych</au><au>Ostroushko Anatolii Viktorovych</au><au>Kladiti Heorhii Oleksandrovych</au><au>Fentisov Ihor Mykolaiovych</au><au>Yakin Mykhailo Mykolaiovych</au><au>Alioshyn Oleksandr Oleksandrovch</au><au>Prakhnin Viacheslav Leonidovych</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MELTING STEEL IN BASIC OPEN-HEARTH FURNACE</title><date>2003-01-15</date><risdate>2003</risdate><abstract>Method for melting steel in basic open-hearth furnace comprises of loading to the furnace scrap metal, oxidizers and mix of converter slag with limestone, before charging the scrap, with melting and finishing. First of all in separate portion oxidizers are loaded, and after those - mix of converter slag with limestone, at ratio 1:(1.5-2.5), at that the ration of the masses of the limestone, converter slag and oxidizers is (7.5- 4.5) : 3 : 1. Способ выплавки стали в основной мартеновской печи включает загрузку в печь металлолома, окислителей и смеси конвертерного шлака с известняком перед завалкой лома, плавление и доводку. Прежде всего засыпают отдельной порцией окислители, а после них - смесь конвертерного шлака с известняком в соотношении 1:(1,5-2,5), при этом соотношение между массами известняка, конвертерного шлака и окислителей составляет (7,5- 4,5) : 3:1. Спосіб виплавки сталі в основній мартенівській печі включає завантаження у піч металобрухту, окисників і суміші конвертерного шлаку із вапняком перед завалкою брухту, плавлення і доведення. Насамперед засипають окремою порцією окисники, а після них - суміш конвертерного шлаку із вапняком у співвідношенні 1:(1,5-2,5), при цьому співвідношення між масами вапняку, конвертерного шлаку і окисників становить (7,5- 4,5) : 3 : 1.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus ; ukr
recordid cdi_epo_espacenet_UA53501A
source esp@cenet
title METHOD FOR MELTING STEEL IN BASIC OPEN-HEARTH FURNACE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T06%3A28%3A29IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Koval%20Serhii%20Oleksiovych&rft.date=2003-01-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUA53501A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true