METHOD OF PRODUCING CERAMIC MEMBRANES FOR FILTRATION WATER TREATMENT

A method for producing ceramic membranes for filtration water treatment, wherein a powdered mixture comprising a ceramic base, a powder-forming agent and a binder is mixed, formed by pressing, preheated and finally sintered to obtain the final product. The ceramic base consists of Silicon Carbide an...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Lapinskyi Andrii Viktorovych, Yanushevska Olena Ivanivna, Dontsova Tetiana Anatoliivna, Molchan Yuliia Mykolaivna, Kyryi Svitlana Oleksandrivna
Format: Patent
Sprache:eng ; ukr
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Lapinskyi Andrii Viktorovych
Yanushevska Olena Ivanivna
Dontsova Tetiana Anatoliivna
Molchan Yuliia Mykolaivna
Kyryi Svitlana Oleksandrivna
description A method for producing ceramic membranes for filtration water treatment, wherein a powdered mixture comprising a ceramic base, a powder-forming agent and a binder is mixed, formed by pressing, preheated and finally sintered to obtain the final product. The ceramic base consists of Silicon Carbide and Aluminum Oxide and its share in the mixture is 55 and 26 wt. %, respectively, the proportion of the powder-forming agent in the mixture is 10 wt. %, and the binder is borax (Na2B4O7-10H2O) and its share in the mixture is 9 wt. Preheating is carried out at a temperature of 95±2 °C for 30-60 minutes to remove moisture at a rate of 1 degree per minute. Further heating to a temperature of 350 ± 5 °C is carried out at a rate of 3 degrees per minute, from a temperature of 350 ± 5 °C to a temperature of 950 ± 10 °C is carried out at a rate of 2 degrees per minute, and final sintering is carried out by holding the mixture at a temperature of 950 ± 10 °C for 60-65 minutes. Self-cooling of the resulting membrane occurs naturally. Спосіб отримання керамічних мембран для фільтраційного очищення води, в якому порошкоподібну суміш, до якої входять керамічна основа, речовина-пороутворювач та в'яжуча речовина, перемішують, створюють формовану заготовку пресуванням, яку попередньо нагрівають та остаточно спікають до отримання кінцевого продукту. Керамічна основа складається з Силіцій карбіду та Алюміній оксиду та її доля у суміші складає 55 та 26 мас. %, відповідно, доля речовини-пороутворювача в суміші складає 10 мас. %, а в'яжуча речовина є бурою (Na2B4O7*10H2O) і її доля в суміші складає 9 мас. %, попереднє нагрівання проводять за температури 95±2 °С протягом 30-60 хвилин для видалення вологи зі швидкістю 1 градус за хвилину. Подальше прогрівання до температури 350±5 °C відбувається зі швидкістю 3 градуси за хвилину, від температури 350±5 °C до температури 950±10 °C здійснюється зі швидкістю 2 градуси за хвилину, і остаточне спікання відбувається шляхом витримування суміші за температури 950±10 °С протягом 60-65 хвилин. Самоохолодження отриманої мембрани відбувається природним шляхом.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_UA155806UU</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>UA155806UU</sourcerecordid><originalsourceid>FETCH-epo_espacenet_UA155806UU3</originalsourceid><addsrcrecordid>eNqFyrEKwjAQANAsDqJ-g_cDgiIV1zO52IDJyXmhYylyTqKF-v-4uDu95c1dyKQtB-AIV-FQfSpn8CSYk4dM-SRY6AaRBWK6qKAmLtChkoAKoWYqunSzx_CcbPVz4daR1LcbG9-9TeNwt5d9-oq7pjluD7Xu_48vu0Irfg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF PRODUCING CERAMIC MEMBRANES FOR FILTRATION WATER TREATMENT</title><source>esp@cenet</source><creator>Lapinskyi Andrii Viktorovych ; Yanushevska Olena Ivanivna ; Dontsova Tetiana Anatoliivna ; Molchan Yuliia Mykolaivna ; Kyryi Svitlana Oleksandrivna</creator><creatorcontrib>Lapinskyi Andrii Viktorovych ; Yanushevska Olena Ivanivna ; Dontsova Tetiana Anatoliivna ; Molchan Yuliia Mykolaivna ; Kyryi Svitlana Oleksandrivna</creatorcontrib><description>A method for producing ceramic membranes for filtration water treatment, wherein a powdered mixture comprising a ceramic base, a powder-forming agent and a binder is mixed, formed by pressing, preheated and finally sintered to obtain the final product. The ceramic base consists of Silicon Carbide and Aluminum Oxide and its share in the mixture is 55 and 26 wt. %, respectively, the proportion of the powder-forming agent in the mixture is 10 wt. %, and the binder is borax (Na2B4O7-10H2O) and its share in the mixture is 9 wt. Preheating is carried out at a temperature of 95±2 °C for 30-60 minutes to remove moisture at a rate of 1 degree per minute. Further heating to a temperature of 350 ± 5 °C is carried out at a rate of 3 degrees per minute, from a temperature of 350 ± 5 °C to a temperature of 950 ± 10 °C is carried out at a rate of 2 degrees per minute, and final sintering is carried out by holding the mixture at a temperature of 950 ± 10 °C for 60-65 minutes. Self-cooling of the resulting membrane occurs naturally. Спосіб отримання керамічних мембран для фільтраційного очищення води, в якому порошкоподібну суміш, до якої входять керамічна основа, речовина-пороутворювач та в'яжуча речовина, перемішують, створюють формовану заготовку пресуванням, яку попередньо нагрівають та остаточно спікають до отримання кінцевого продукту. Керамічна основа складається з Силіцій карбіду та Алюміній оксиду та її доля у суміші складає 55 та 26 мас. %, відповідно, доля речовини-пороутворювача в суміші складає 10 мас. %, а в'яжуча речовина є бурою (Na2B4O7*10H2O) і її доля в суміші складає 9 мас. %, попереднє нагрівання проводять за температури 95±2 °С протягом 30-60 хвилин для видалення вологи зі швидкістю 1 градус за хвилину. Подальше прогрівання до температури 350±5 °C відбувається зі швидкістю 3 градуси за хвилину, від температури 350±5 °C до температури 950±10 °C здійснюється зі швидкістю 2 градуси за хвилину, і остаточне спікання відбувається шляхом витримування суміші за температури 950±10 °С протягом 60-65 хвилин. Самоохолодження отриманої мембрани відбувається природним шляхом.</description><language>eng ; ukr</language><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240410&amp;DB=EPODOC&amp;CC=UA&amp;NR=155806U$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240410&amp;DB=EPODOC&amp;CC=UA&amp;NR=155806U$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Lapinskyi Andrii Viktorovych</creatorcontrib><creatorcontrib>Yanushevska Olena Ivanivna</creatorcontrib><creatorcontrib>Dontsova Tetiana Anatoliivna</creatorcontrib><creatorcontrib>Molchan Yuliia Mykolaivna</creatorcontrib><creatorcontrib>Kyryi Svitlana Oleksandrivna</creatorcontrib><title>METHOD OF PRODUCING CERAMIC MEMBRANES FOR FILTRATION WATER TREATMENT</title><description>A method for producing ceramic membranes for filtration water treatment, wherein a powdered mixture comprising a ceramic base, a powder-forming agent and a binder is mixed, formed by pressing, preheated and finally sintered to obtain the final product. The ceramic base consists of Silicon Carbide and Aluminum Oxide and its share in the mixture is 55 and 26 wt. %, respectively, the proportion of the powder-forming agent in the mixture is 10 wt. %, and the binder is borax (Na2B4O7-10H2O) and its share in the mixture is 9 wt. Preheating is carried out at a temperature of 95±2 °C for 30-60 minutes to remove moisture at a rate of 1 degree per minute. Further heating to a temperature of 350 ± 5 °C is carried out at a rate of 3 degrees per minute, from a temperature of 350 ± 5 °C to a temperature of 950 ± 10 °C is carried out at a rate of 2 degrees per minute, and final sintering is carried out by holding the mixture at a temperature of 950 ± 10 °C for 60-65 minutes. Self-cooling of the resulting membrane occurs naturally. Спосіб отримання керамічних мембран для фільтраційного очищення води, в якому порошкоподібну суміш, до якої входять керамічна основа, речовина-пороутворювач та в'яжуча речовина, перемішують, створюють формовану заготовку пресуванням, яку попередньо нагрівають та остаточно спікають до отримання кінцевого продукту. Керамічна основа складається з Силіцій карбіду та Алюміній оксиду та її доля у суміші складає 55 та 26 мас. %, відповідно, доля речовини-пороутворювача в суміші складає 10 мас. %, а в'яжуча речовина є бурою (Na2B4O7*10H2O) і її доля в суміші складає 9 мас. %, попереднє нагрівання проводять за температури 95±2 °С протягом 30-60 хвилин для видалення вологи зі швидкістю 1 градус за хвилину. Подальше прогрівання до температури 350±5 °C відбувається зі швидкістю 3 градуси за хвилину, від температури 350±5 °C до температури 950±10 °C здійснюється зі швидкістю 2 градуси за хвилину, і остаточне спікання відбувається шляхом витримування суміші за температури 950±10 °С протягом 60-65 хвилин. Самоохолодження отриманої мембрани відбувається природним шляхом.</description><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqFyrEKwjAQANAsDqJ-g_cDgiIV1zO52IDJyXmhYylyTqKF-v-4uDu95c1dyKQtB-AIV-FQfSpn8CSYk4dM-SRY6AaRBWK6qKAmLtChkoAKoWYqunSzx_CcbPVz4daR1LcbG9-9TeNwt5d9-oq7pjluD7Xu_48vu0Irfg</recordid><startdate>20240410</startdate><enddate>20240410</enddate><creator>Lapinskyi Andrii Viktorovych</creator><creator>Yanushevska Olena Ivanivna</creator><creator>Dontsova Tetiana Anatoliivna</creator><creator>Molchan Yuliia Mykolaivna</creator><creator>Kyryi Svitlana Oleksandrivna</creator><scope>EVB</scope></search><sort><creationdate>20240410</creationdate><title>METHOD OF PRODUCING CERAMIC MEMBRANES FOR FILTRATION WATER TREATMENT</title><author>Lapinskyi Andrii Viktorovych ; Yanushevska Olena Ivanivna ; Dontsova Tetiana Anatoliivna ; Molchan Yuliia Mykolaivna ; Kyryi Svitlana Oleksandrivna</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_UA155806UU3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; ukr</language><creationdate>2024</creationdate><toplevel>online_resources</toplevel><creatorcontrib>Lapinskyi Andrii Viktorovych</creatorcontrib><creatorcontrib>Yanushevska Olena Ivanivna</creatorcontrib><creatorcontrib>Dontsova Tetiana Anatoliivna</creatorcontrib><creatorcontrib>Molchan Yuliia Mykolaivna</creatorcontrib><creatorcontrib>Kyryi Svitlana Oleksandrivna</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Lapinskyi Andrii Viktorovych</au><au>Yanushevska Olena Ivanivna</au><au>Dontsova Tetiana Anatoliivna</au><au>Molchan Yuliia Mykolaivna</au><au>Kyryi Svitlana Oleksandrivna</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF PRODUCING CERAMIC MEMBRANES FOR FILTRATION WATER TREATMENT</title><date>2024-04-10</date><risdate>2024</risdate><abstract>A method for producing ceramic membranes for filtration water treatment, wherein a powdered mixture comprising a ceramic base, a powder-forming agent and a binder is mixed, formed by pressing, preheated and finally sintered to obtain the final product. The ceramic base consists of Silicon Carbide and Aluminum Oxide and its share in the mixture is 55 and 26 wt. %, respectively, the proportion of the powder-forming agent in the mixture is 10 wt. %, and the binder is borax (Na2B4O7-10H2O) and its share in the mixture is 9 wt. Preheating is carried out at a temperature of 95±2 °C for 30-60 minutes to remove moisture at a rate of 1 degree per minute. Further heating to a temperature of 350 ± 5 °C is carried out at a rate of 3 degrees per minute, from a temperature of 350 ± 5 °C to a temperature of 950 ± 10 °C is carried out at a rate of 2 degrees per minute, and final sintering is carried out by holding the mixture at a temperature of 950 ± 10 °C for 60-65 minutes. Self-cooling of the resulting membrane occurs naturally. Спосіб отримання керамічних мембран для фільтраційного очищення води, в якому порошкоподібну суміш, до якої входять керамічна основа, речовина-пороутворювач та в'яжуча речовина, перемішують, створюють формовану заготовку пресуванням, яку попередньо нагрівають та остаточно спікають до отримання кінцевого продукту. Керамічна основа складається з Силіцій карбіду та Алюміній оксиду та її доля у суміші складає 55 та 26 мас. %, відповідно, доля речовини-пороутворювача в суміші складає 10 мас. %, а в'яжуча речовина є бурою (Na2B4O7*10H2O) і її доля в суміші складає 9 мас. %, попереднє нагрівання проводять за температури 95±2 °С протягом 30-60 хвилин для видалення вологи зі швидкістю 1 градус за хвилину. Подальше прогрівання до температури 350±5 °C відбувається зі швидкістю 3 градуси за хвилину, від температури 350±5 °C до температури 950±10 °C здійснюється зі швидкістю 2 градуси за хвилину, і остаточне спікання відбувається шляхом витримування суміші за температури 950±10 °С протягом 60-65 хвилин. Самоохолодження отриманої мембрани відбувається природним шляхом.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; ukr
recordid cdi_epo_espacenet_UA155806UU
source esp@cenet
title METHOD OF PRODUCING CERAMIC MEMBRANES FOR FILTRATION WATER TREATMENT
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T09%3A54%3A06IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Lapinskyi%20Andrii%20Viktorovych&rft.date=2024-04-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUA155806UU%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true