Glass panel for cathode ray tube, cathode ray tube employing this glass panel and method for producing cathode ray tube
A CRT in its entirety is to be rendered lightweight without detracting from the resistance against pressure of a panel or from characteristics desirable for the CRT. To this end, there is provided a glass panel for a CRT obtained on chemically reinforcing the glass containing 57 to 64 wt% of SiO2, 0...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | OKADA, MASAMICHI SANTOKU, MASATAKA HACHITANI, YOICHI WATANABE, ITARU KURAMOTO, FUMIO |
description | A CRT in its entirety is to be rendered lightweight without detracting from the resistance against pressure of a panel or from characteristics desirable for the CRT. To this end, there is provided a glass panel for a CRT obtained on chemically reinforcing the glass containing 57 to 64 wt% of SiO2, 0.1 to 4 wt% of Al2O3, 5 to 10 wt% of Na2O, 5 to 10 wt% of K2O, 7 to 13 wt% of SrO, 7 to 11 wt% of BaO, 0.1 to 2 wt% of TiO2, 0.1 to 4 wt% of ZrO2 and 0.01 to 1 wt% of CeO2. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_TW492037BB</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>TW492037BB</sourcerecordid><originalsourceid>FETCH-epo_espacenet_TW492037BB3</originalsourceid><addsrcrecordid>eNrjZCh3z0ksLlYoSMxLzVFIyy9SSE4sychPSVUoSqxUKClNStXBEFFIzS3Iya_MzEtXKMnILFZIRzIhMS9FITcVpB5sWEFRfkppMkgluiE8DKxpiTnFqbxQmptB3s01xNlDN7UgPz61uCAxOTUvtSQ-JNzE0sjA2NzJyZiwCgDsqkS7</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Glass panel for cathode ray tube, cathode ray tube employing this glass panel and method for producing cathode ray tube</title><source>esp@cenet</source><creator>OKADA, MASAMICHI ; SANTOKU, MASATAKA ; HACHITANI, YOICHI ; WATANABE, ITARU ; KURAMOTO, FUMIO</creator><creatorcontrib>OKADA, MASAMICHI ; SANTOKU, MASATAKA ; HACHITANI, YOICHI ; WATANABE, ITARU ; KURAMOTO, FUMIO</creatorcontrib><description>A CRT in its entirety is to be rendered lightweight without detracting from the resistance against pressure of a panel or from characteristics desirable for the CRT. To this end, there is provided a glass panel for a CRT obtained on chemically reinforcing the glass containing 57 to 64 wt% of SiO2, 0.1 to 4 wt% of Al2O3, 5 to 10 wt% of Na2O, 5 to 10 wt% of K2O, 7 to 13 wt% of SrO, 7 to 11 wt% of BaO, 0.1 to 2 wt% of TiO2, 0.1 to 4 wt% of ZrO2 and 0.01 to 1 wt% of CeO2.</description><edition>7</edition><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS ; ELECTRICITY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2002</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20020621&DB=EPODOC&CC=TW&NR=492037B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20020621&DB=EPODOC&CC=TW&NR=492037B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>OKADA, MASAMICHI</creatorcontrib><creatorcontrib>SANTOKU, MASATAKA</creatorcontrib><creatorcontrib>HACHITANI, YOICHI</creatorcontrib><creatorcontrib>WATANABE, ITARU</creatorcontrib><creatorcontrib>KURAMOTO, FUMIO</creatorcontrib><title>Glass panel for cathode ray tube, cathode ray tube employing this glass panel and method for producing cathode ray tube</title><description>A CRT in its entirety is to be rendered lightweight without detracting from the resistance against pressure of a panel or from characteristics desirable for the CRT. To this end, there is provided a glass panel for a CRT obtained on chemically reinforcing the glass containing 57 to 64 wt% of SiO2, 0.1 to 4 wt% of Al2O3, 5 to 10 wt% of Na2O, 5 to 10 wt% of K2O, 7 to 13 wt% of SrO, 7 to 11 wt% of BaO, 0.1 to 2 wt% of TiO2, 0.1 to 4 wt% of ZrO2 and 0.01 to 1 wt% of CeO2.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS</subject><subject>ELECTRICITY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2002</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZCh3z0ksLlYoSMxLzVFIyy9SSE4sychPSVUoSqxUKClNStXBEFFIzS3Iya_MzEtXKMnILFZIRzIhMS9FITcVpB5sWEFRfkppMkgluiE8DKxpiTnFqbxQmptB3s01xNlDN7UgPz61uCAxOTUvtSQ-JNzE0sjA2NzJyZiwCgDsqkS7</recordid><startdate>20020621</startdate><enddate>20020621</enddate><creator>OKADA, MASAMICHI</creator><creator>SANTOKU, MASATAKA</creator><creator>HACHITANI, YOICHI</creator><creator>WATANABE, ITARU</creator><creator>KURAMOTO, FUMIO</creator><scope>EVB</scope></search><sort><creationdate>20020621</creationdate><title>Glass panel for cathode ray tube, cathode ray tube employing this glass panel and method for producing cathode ray tube</title><author>OKADA, MASAMICHI ; SANTOKU, MASATAKA ; HACHITANI, YOICHI ; WATANABE, ITARU ; KURAMOTO, FUMIO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_TW492037BB3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2002</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS</topic><topic>ELECTRICITY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>OKADA, MASAMICHI</creatorcontrib><creatorcontrib>SANTOKU, MASATAKA</creatorcontrib><creatorcontrib>HACHITANI, YOICHI</creatorcontrib><creatorcontrib>WATANABE, ITARU</creatorcontrib><creatorcontrib>KURAMOTO, FUMIO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>OKADA, MASAMICHI</au><au>SANTOKU, MASATAKA</au><au>HACHITANI, YOICHI</au><au>WATANABE, ITARU</au><au>KURAMOTO, FUMIO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Glass panel for cathode ray tube, cathode ray tube employing this glass panel and method for producing cathode ray tube</title><date>2002-06-21</date><risdate>2002</risdate><abstract>A CRT in its entirety is to be rendered lightweight without detracting from the resistance against pressure of a panel or from characteristics desirable for the CRT. To this end, there is provided a glass panel for a CRT obtained on chemically reinforcing the glass containing 57 to 64 wt% of SiO2, 0.1 to 4 wt% of Al2O3, 5 to 10 wt% of Na2O, 5 to 10 wt% of K2O, 7 to 13 wt% of SrO, 7 to 11 wt% of BaO, 0.1 to 2 wt% of TiO2, 0.1 to 4 wt% of ZrO2 and 0.01 to 1 wt% of CeO2.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_TW492037BB |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS CHEMISTRY ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS ELECTRICITY GLASS JOINING GLASS TO GLASS OR OTHER MATERIALS METALLURGY MINERAL OR SLAG WOOL SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS SURFACE TREATMENT OF GLASS |
title | Glass panel for cathode ray tube, cathode ray tube employing this glass panel and method for producing cathode ray tube |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T08%3A17%3A06IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=OKADA,%20MASAMICHI&rft.date=2002-06-21&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ETW492037BB%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |