Cathode ray tube neck glass

A cathode ray tube with an improved tubular glass neck member having a softening point in the range of 640-650 DEG C, an annealing temperature in the range of 460-472 DEG C, a strain point in the range of 420-425 DEG C, a coefficient of thermal expansion in the range of 94-97x10-7/DEG C., and a line...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: TAMMARO, DAVID ALAN
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A cathode ray tube with an improved tubular glass neck member having a softening point in the range of 640-650 DEG C, an annealing temperature in the range of 460-472 DEG C, a strain point in the range of 420-425 DEG C, a coefficient of thermal expansion in the range of 94-97x10-7/DEG C., and a linear x-ray absorption value of at least 100 cm-1 and a composition, as calculated in weight % on an oxide basis, consisting essentially of 46.5-49.5% SiO2, 1.5-2% Al2O3, 0.5-1.5% Na2O, 10-12% K2O, 2-3% SrO, 1-1.8% BaO, 32-34% PbO, 1-1.5% ZnO and a fining agent.