Primary cooling method in continuously annealing steel strip

In a method of continuously annealing steel strip comprising a heating step (A), a soaking step (B), a primary cooling step (C) including a rapid cooling step at least in a second half thereof, an overaging step (D), and a final cooling step (E), insert atmosphere gas containing H2 gas in the concen...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SAKURAI, KOICHI, WAKABAYASHI, HISAMOTO, SHIBUYA, TATSURU, SUGIYAMA, SEIJI, WAKI, KOUICHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SAKURAI, KOICHI
WAKABAYASHI, HISAMOTO
SHIBUYA, TATSURU
SUGIYAMA, SEIJI
WAKI, KOUICHI
description In a method of continuously annealing steel strip comprising a heating step (A), a soaking step (B), a primary cooling step (C) including a rapid cooling step at least in a second half thereof, an overaging step (D), and a final cooling step (E), insert atmosphere gas containing H2 gas in the concentration of 30-60% is employed as cooling gas for use in the rapid cooling step, the blowoff temperature of the cooling gas is 30-150 DEG C, and the blowoff speed of the cooling gas is 100-150 m/sec. The primary cooling method in continuously annealing steel strip provides the primary cooling step (C) including the rapid cooling step which can be carried out with a high efficiency and a low cost.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_TW420718BB</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>TW420718BB</sourcerecordid><originalsourceid>FETCH-epo_espacenet_TW420718BB3</originalsourceid><addsrcrecordid>eNrjZLAJKMrMTSyqVEjOz8_JzEtXyE0tychPUcjMA4rklWTmleaXFudUKiTm5aUmghUUl6Sm5gDJoswCHgbWtMSc4lReKM3NIO_mGuLsoZtakB-fWlyQmJyal1oSHxJuYmRgbmjh5GRMWAUAeKcv5A</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Primary cooling method in continuously annealing steel strip</title><source>esp@cenet</source><creator>SAKURAI, KOICHI ; WAKABAYASHI, HISAMOTO ; SHIBUYA, TATSURU ; SUGIYAMA, SEIJI ; WAKI, KOUICHI</creator><creatorcontrib>SAKURAI, KOICHI ; WAKABAYASHI, HISAMOTO ; SHIBUYA, TATSURU ; SUGIYAMA, SEIJI ; WAKI, KOUICHI</creatorcontrib><description>In a method of continuously annealing steel strip comprising a heating step (A), a soaking step (B), a primary cooling step (C) including a rapid cooling step at least in a second half thereof, an overaging step (D), and a final cooling step (E), insert atmosphere gas containing H2 gas in the concentration of 30-60% is employed as cooling gas for use in the rapid cooling step, the blowoff temperature of the cooling gas is 30-150 DEG C, and the blowoff speed of the cooling gas is 100-150 m/sec. The primary cooling method in continuously annealing steel strip provides the primary cooling step (C) including the rapid cooling step which can be carried out with a high efficiency and a low cost.</description><edition>7</edition><language>eng</language><subject>CHEMISTRY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><creationdate>2001</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20010201&amp;DB=EPODOC&amp;CC=TW&amp;NR=420718B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20010201&amp;DB=EPODOC&amp;CC=TW&amp;NR=420718B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SAKURAI, KOICHI</creatorcontrib><creatorcontrib>WAKABAYASHI, HISAMOTO</creatorcontrib><creatorcontrib>SHIBUYA, TATSURU</creatorcontrib><creatorcontrib>SUGIYAMA, SEIJI</creatorcontrib><creatorcontrib>WAKI, KOUICHI</creatorcontrib><title>Primary cooling method in continuously annealing steel strip</title><description>In a method of continuously annealing steel strip comprising a heating step (A), a soaking step (B), a primary cooling step (C) including a rapid cooling step at least in a second half thereof, an overaging step (D), and a final cooling step (E), insert atmosphere gas containing H2 gas in the concentration of 30-60% is employed as cooling gas for use in the rapid cooling step, the blowoff temperature of the cooling gas is 30-150 DEG C, and the blowoff speed of the cooling gas is 100-150 m/sec. The primary cooling method in continuously annealing steel strip provides the primary cooling step (C) including the rapid cooling step which can be carried out with a high efficiency and a low cost.</description><subject>CHEMISTRY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2001</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAJKMrMTSyqVEjOz8_JzEtXyE0tychPUcjMA4rklWTmleaXFudUKiTm5aUmghUUl6Sm5gDJoswCHgbWtMSc4lReKM3NIO_mGuLsoZtakB-fWlyQmJyal1oSHxJuYmRgbmjh5GRMWAUAeKcv5A</recordid><startdate>20010201</startdate><enddate>20010201</enddate><creator>SAKURAI, KOICHI</creator><creator>WAKABAYASHI, HISAMOTO</creator><creator>SHIBUYA, TATSURU</creator><creator>SUGIYAMA, SEIJI</creator><creator>WAKI, KOUICHI</creator><scope>EVB</scope></search><sort><creationdate>20010201</creationdate><title>Primary cooling method in continuously annealing steel strip</title><author>SAKURAI, KOICHI ; WAKABAYASHI, HISAMOTO ; SHIBUYA, TATSURU ; SUGIYAMA, SEIJI ; WAKI, KOUICHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_TW420718BB3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2001</creationdate><topic>CHEMISTRY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>SAKURAI, KOICHI</creatorcontrib><creatorcontrib>WAKABAYASHI, HISAMOTO</creatorcontrib><creatorcontrib>SHIBUYA, TATSURU</creatorcontrib><creatorcontrib>SUGIYAMA, SEIJI</creatorcontrib><creatorcontrib>WAKI, KOUICHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SAKURAI, KOICHI</au><au>WAKABAYASHI, HISAMOTO</au><au>SHIBUYA, TATSURU</au><au>SUGIYAMA, SEIJI</au><au>WAKI, KOUICHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Primary cooling method in continuously annealing steel strip</title><date>2001-02-01</date><risdate>2001</risdate><abstract>In a method of continuously annealing steel strip comprising a heating step (A), a soaking step (B), a primary cooling step (C) including a rapid cooling step at least in a second half thereof, an overaging step (D), and a final cooling step (E), insert atmosphere gas containing H2 gas in the concentration of 30-60% is employed as cooling gas for use in the rapid cooling step, the blowoff temperature of the cooling gas is 30-150 DEG C, and the blowoff speed of the cooling gas is 100-150 m/sec. The primary cooling method in continuously annealing steel strip provides the primary cooling step (C) including the rapid cooling step which can be carried out with a high efficiency and a low cost.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_TW420718BB
source esp@cenet
subjects CHEMISTRY
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
title Primary cooling method in continuously annealing steel strip
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T09%3A55%3A49IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SAKURAI,%20KOICHI&rft.date=2001-02-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ETW420718BB%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true