Metallic gloss ceramic glaze using basalt as the raw material and its preparation method

A formulation of ceramic glaze with metallic gloss is as follows. The major constituent of a base glaze are basalt and flux controlled at 40 to 55wt%, 45 to 60wt% respectively. The constituents are mixed with water and grind into a slip, then spray coating on the ceramic body. The firing process is...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HSI, CHI-SHIUNG, CHANG, KUN-SEN, HAN, HSIUNG-WEN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HSI, CHI-SHIUNG
CHANG, KUN-SEN
HAN, HSIUNG-WEN
description A formulation of ceramic glaze with metallic gloss is as follows. The major constituent of a base glaze are basalt and flux controlled at 40 to 55wt%, 45 to 60wt% respectively. The constituents are mixed with water and grind into a slip, then spray coating on the ceramic body. The firing process is included oxidation atmosphere control, heating time 4 to 8 hour to temperature 1130 to 1210 DEG C, and maturation time 10 to 30 minute.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_TW201237007A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>TW201237007A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_TW201237007A3</originalsourceid><addsrcrecordid>eNqNyj0KwkAQhuE0FqLeYTyAsCZFagmKjV1Au_C5GZOF_WNnRPD0gngAq5cH3mV1u7DCe2dp8kmELBeEr_BmeoqLE90h8EoQ0pmp4EUBysXBE-JIToVy4YwCdSlSYJ3TuK4WD3jhza-rans69t15xzkNLBmWI-vQX2uzr5vWmPbQ_PN8AH4aOi0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Metallic gloss ceramic glaze using basalt as the raw material and its preparation method</title><source>esp@cenet</source><creator>HSI, CHI-SHIUNG ; CHANG, KUN-SEN ; HAN, HSIUNG-WEN</creator><creatorcontrib>HSI, CHI-SHIUNG ; CHANG, KUN-SEN ; HAN, HSIUNG-WEN</creatorcontrib><description>A formulation of ceramic glaze with metallic gloss is as follows. The major constituent of a base glaze are basalt and flux controlled at 40 to 55wt%, 45 to 60wt% respectively. The constituents are mixed with water and grind into a slip, then spray coating on the ceramic body. The firing process is included oxidation atmosphere control, heating time 4 to 8 hour to temperature 1130 to 1210 DEG C, and maturation time 10 to 30 minute.</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120916&amp;DB=EPODOC&amp;CC=TW&amp;NR=201237007A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120916&amp;DB=EPODOC&amp;CC=TW&amp;NR=201237007A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HSI, CHI-SHIUNG</creatorcontrib><creatorcontrib>CHANG, KUN-SEN</creatorcontrib><creatorcontrib>HAN, HSIUNG-WEN</creatorcontrib><title>Metallic gloss ceramic glaze using basalt as the raw material and its preparation method</title><description>A formulation of ceramic glaze with metallic gloss is as follows. The major constituent of a base glaze are basalt and flux controlled at 40 to 55wt%, 45 to 60wt% respectively. The constituents are mixed with water and grind into a slip, then spray coating on the ceramic body. The firing process is included oxidation atmosphere control, heating time 4 to 8 hour to temperature 1130 to 1210 DEG C, and maturation time 10 to 30 minute.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyj0KwkAQhuE0FqLeYTyAsCZFagmKjV1Au_C5GZOF_WNnRPD0gngAq5cH3mV1u7DCe2dp8kmELBeEr_BmeoqLE90h8EoQ0pmp4EUBysXBE-JIToVy4YwCdSlSYJ3TuK4WD3jhza-rans69t15xzkNLBmWI-vQX2uzr5vWmPbQ_PN8AH4aOi0</recordid><startdate>20120916</startdate><enddate>20120916</enddate><creator>HSI, CHI-SHIUNG</creator><creator>CHANG, KUN-SEN</creator><creator>HAN, HSIUNG-WEN</creator><scope>EVB</scope></search><sort><creationdate>20120916</creationdate><title>Metallic gloss ceramic glaze using basalt as the raw material and its preparation method</title><author>HSI, CHI-SHIUNG ; CHANG, KUN-SEN ; HAN, HSIUNG-WEN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_TW201237007A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2012</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>HSI, CHI-SHIUNG</creatorcontrib><creatorcontrib>CHANG, KUN-SEN</creatorcontrib><creatorcontrib>HAN, HSIUNG-WEN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HSI, CHI-SHIUNG</au><au>CHANG, KUN-SEN</au><au>HAN, HSIUNG-WEN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Metallic gloss ceramic glaze using basalt as the raw material and its preparation method</title><date>2012-09-16</date><risdate>2012</risdate><abstract>A formulation of ceramic glaze with metallic gloss is as follows. The major constituent of a base glaze are basalt and flux controlled at 40 to 55wt%, 45 to 60wt% respectively. The constituents are mixed with water and grind into a slip, then spray coating on the ceramic body. The firing process is included oxidation atmosphere control, heating time 4 to 8 hour to temperature 1130 to 1210 DEG C, and maturation time 10 to 30 minute.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_TW201237007A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Metallic gloss ceramic glaze using basalt as the raw material and its preparation method
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-01T07%3A59%3A00IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HSI,%20CHI-SHIUNG&rft.date=2012-09-16&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ETW201237007A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true