METHOD OF PRODUCING POLYAMIDOACID SOLUTION FOR FIBER FORMING

FIELD: chemistry of high-molecular compounds. SUBSTANCE: method involves the additional use at polycondensation of 2,5-bis-(p-aminophenyl)- or 4,4′-p-terphenyl at the mole ratio to 4,4′-diaminodiphenyloxide = (15-50): (50-85). Fiber rupture strength is 27.0-37.8 cH/tex after heating at 450 C for 5 m...