SE354266

Process to strengthen the glass and increase its resistance to surface abrasion, characterized by comprising: A) the treatment of the surface of the glass with a compound containing a metal from the group consisting of tin, titanium and zirconium, the compound of which is pyrolyzable to form a metal...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: POOLE J,US, SNYDER H,US, BOSCHINI M,US
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator POOLE J,US
SNYDER H,US
BOSCHINI M,US
description Process to strengthen the glass and increase its resistance to surface abrasion, characterized by comprising: A) the treatment of the surface of the glass with a compound containing a metal from the group consisting of tin, titanium and zirconium, the compound of which is pyrolyzable to form a metal oxide on the surface of the glass while said surface is at a temperature at least as high as the pyrolyzing temperature of the compound, B) a subsequent spraying of said surface with an aqueous solution of a potassium salt to form a continuous coating layer thereon while said glass is still at an elevated temperature in the field near the point of tension of the glass, C) the maintenance of glass at an elevated temperature below the glass tension point for a sufficient period of time to achieve a significant exchange of sodium ions and potassium ions from the glass to a sufficient depth to produce a significant compression stress, although not for a sufficient time to produce a relaxation of tension, D) the cooling of the glass and its subsequent washing to remove any excess potassium salt from the surface of the glass, and. E) a further spraying on the glass surface of an olefin polymer in an amount sufficient to form an adherent and transparent coating on said surface. (Machine-translation by Google Translate, not legally binding)
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_SE354266B</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>SE354266B</sourcerecordid><originalsourceid>FETCH-epo_espacenet_SE354266B3</originalsourceid><addsrcrecordid>eNrjZOAIdjU2NTEyM-NhYE1LzClO5YXS3Axybq4hzh66qQX58anFBYnJqXmpJfEw5U7GBBUAAGBTGZ8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SE354266</title><source>esp@cenet</source><creator>POOLE J,US ; SNYDER H,US ; BOSCHINI M,US</creator><creatorcontrib>POOLE J,US ; SNYDER H,US ; BOSCHINI M,US</creatorcontrib><description>Process to strengthen the glass and increase its resistance to surface abrasion, characterized by comprising: A) the treatment of the surface of the glass with a compound containing a metal from the group consisting of tin, titanium and zirconium, the compound of which is pyrolyzable to form a metal oxide on the surface of the glass while said surface is at a temperature at least as high as the pyrolyzing temperature of the compound, B) a subsequent spraying of said surface with an aqueous solution of a potassium salt to form a continuous coating layer thereon while said glass is still at an elevated temperature in the field near the point of tension of the glass, C) the maintenance of glass at an elevated temperature below the glass tension point for a sufficient period of time to achieve a significant exchange of sodium ions and potassium ions from the glass to a sufficient depth to produce a significant compression stress, although not for a sufficient time to produce a relaxation of tension, D) the cooling of the glass and its subsequent washing to remove any excess potassium salt from the surface of the glass, and. E) a further spraying on the glass surface of an olefin polymer in an amount sufficient to form an adherent and transparent coating on said surface. (Machine-translation by Google Translate, not legally binding)</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>1973</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19730305&amp;DB=EPODOC&amp;CC=SE&amp;NR=354266B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19730305&amp;DB=EPODOC&amp;CC=SE&amp;NR=354266B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>POOLE J,US</creatorcontrib><creatorcontrib>SNYDER H,US</creatorcontrib><creatorcontrib>BOSCHINI M,US</creatorcontrib><title>SE354266</title><description>Process to strengthen the glass and increase its resistance to surface abrasion, characterized by comprising: A) the treatment of the surface of the glass with a compound containing a metal from the group consisting of tin, titanium and zirconium, the compound of which is pyrolyzable to form a metal oxide on the surface of the glass while said surface is at a temperature at least as high as the pyrolyzing temperature of the compound, B) a subsequent spraying of said surface with an aqueous solution of a potassium salt to form a continuous coating layer thereon while said glass is still at an elevated temperature in the field near the point of tension of the glass, C) the maintenance of glass at an elevated temperature below the glass tension point for a sufficient period of time to achieve a significant exchange of sodium ions and potassium ions from the glass to a sufficient depth to produce a significant compression stress, although not for a sufficient time to produce a relaxation of tension, D) the cooling of the glass and its subsequent washing to remove any excess potassium salt from the surface of the glass, and. E) a further spraying on the glass surface of an olefin polymer in an amount sufficient to form an adherent and transparent coating on said surface. (Machine-translation by Google Translate, not legally binding)</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1973</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZOAIdjU2NTEyM-NhYE1LzClO5YXS3Axybq4hzh66qQX58anFBYnJqXmpJfEw5U7GBBUAAGBTGZ8</recordid><startdate>19730305</startdate><enddate>19730305</enddate><creator>POOLE J,US</creator><creator>SNYDER H,US</creator><creator>BOSCHINI M,US</creator><scope>EVB</scope></search><sort><creationdate>19730305</creationdate><title>SE354266</title><author>POOLE J,US ; SNYDER H,US ; BOSCHINI M,US</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_SE354266B3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1973</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>POOLE J,US</creatorcontrib><creatorcontrib>SNYDER H,US</creatorcontrib><creatorcontrib>BOSCHINI M,US</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>POOLE J,US</au><au>SNYDER H,US</au><au>BOSCHINI M,US</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SE354266</title><date>1973-03-05</date><risdate>1973</risdate><abstract>Process to strengthen the glass and increase its resistance to surface abrasion, characterized by comprising: A) the treatment of the surface of the glass with a compound containing a metal from the group consisting of tin, titanium and zirconium, the compound of which is pyrolyzable to form a metal oxide on the surface of the glass while said surface is at a temperature at least as high as the pyrolyzing temperature of the compound, B) a subsequent spraying of said surface with an aqueous solution of a potassium salt to form a continuous coating layer thereon while said glass is still at an elevated temperature in the field near the point of tension of the glass, C) the maintenance of glass at an elevated temperature below the glass tension point for a sufficient period of time to achieve a significant exchange of sodium ions and potassium ions from the glass to a sufficient depth to produce a significant compression stress, although not for a sufficient time to produce a relaxation of tension, D) the cooling of the glass and its subsequent washing to remove any excess potassium salt from the surface of the glass, and. E) a further spraying on the glass surface of an olefin polymer in an amount sufficient to form an adherent and transparent coating on said surface. (Machine-translation by Google Translate, not legally binding)</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_SE354266B
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title SE354266
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T01%3A08%3A46IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=POOLE%20J,US&rft.date=1973-03-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ESE354266B%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true