METHOD FOR DYEING OF POLYESTER THREADS

FIELD: dyeing-finishing production; applicable in dyeing of polyester threads and ropes in course of their production. SUBSTANCE: method for dyeing of polyester threads is effected at thread tensioning of less than 0.3 gf/tex in one dyeing bath in two stages at temperature of 100.5-105.0 C. At the f...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ANDRONOVA A.P, ISAKOV V.F
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ANDRONOVA A.P
ISAKOV V.F
description FIELD: dyeing-finishing production; applicable in dyeing of polyester threads and ropes in course of their production. SUBSTANCE: method for dyeing of polyester threads is effected at thread tensioning of less than 0.3 gf/tex in one dyeing bath in two stages at temperature of 100.5-105.0 C. At the first stage, freshly spun fiber is dyed at constant speed of its transportation in the bath and at the second stage, it is dyed at increasing speed of transportation by 1.5-10 times. In this case, ratio of fiber path at the first stage to that at the second stage equals (1:1)-(2:1). EFFECT: higher efficiency. 1 cl, 3 dwg Использование: в красильно-отделочном производстве для крашения полиэфирных нитей и жгутов в процессе их получения. Сущность изобретения: способ крашения полиэфирных нитей осуществляют при натяжении нити менее 0,3 гс/текс в одной красильной ванне в две стадии при температуре 100,5-105,0°С, при этом на первой стадии крашение свежесформованной нити проводят при постоянной скорости транспортирования нитей в ванне, а на второй стадии - при возрастании скорости транспортирования нитей в 1,5-10 раз, причем отношение длины пути нити на первой стадии к длине пути нити на второй стадии равно 1:1 - 2: 1.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU94031444A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU94031444A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU94031444A3</originalsourceid><addsrcrecordid>eNrjZFDzdQ3x8HdRcPMPUnCJdPX0c1fwd1MI8PeJdA0OcQ1SCPEIcnV0CeZhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoZYmBsaGJiYmjsZEKAEAfB8jQA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR DYEING OF POLYESTER THREADS</title><source>esp@cenet</source><creator>ANDRONOVA A.P ; ISAKOV V.F</creator><creatorcontrib>ANDRONOVA A.P ; ISAKOV V.F</creatorcontrib><description>FIELD: dyeing-finishing production; applicable in dyeing of polyester threads and ropes in course of their production. SUBSTANCE: method for dyeing of polyester threads is effected at thread tensioning of less than 0.3 gf/tex in one dyeing bath in two stages at temperature of 100.5-105.0 C. At the first stage, freshly spun fiber is dyed at constant speed of its transportation in the bath and at the second stage, it is dyed at increasing speed of transportation by 1.5-10 times. In this case, ratio of fiber path at the first stage to that at the second stage equals (1:1)-(2:1). EFFECT: higher efficiency. 1 cl, 3 dwg Использование: в красильно-отделочном производстве для крашения полиэфирных нитей и жгутов в процессе их получения. Сущность изобретения: способ крашения полиэфирных нитей осуществляют при натяжении нити менее 0,3 гс/текс в одной красильной ванне в две стадии при температуре 100,5-105,0°С, при этом на первой стадии крашение свежесформованной нити проводят при постоянной скорости транспортирования нитей в ванне, а на второй стадии - при возрастании скорости транспортирования нитей в 1,5-10 раз, причем отношение длины пути нити на первой стадии к длине пути нити на второй стадии равно 1:1 - 2: 1.</description><language>eng ; rus</language><subject>DYEING LEATHER, FURS, OR SOLID MACROMOLECULAR SUBSTANCES INANY FORM ; DYEING OR PRINTING TEXTILES ; FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR ; LAUNDERING ; TEXTILES ; TREATMENT OF TEXTILES OR THE LIKE</subject><creationdate>1996</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960820&amp;DB=EPODOC&amp;CC=RU&amp;NR=94031444A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960820&amp;DB=EPODOC&amp;CC=RU&amp;NR=94031444A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ANDRONOVA A.P</creatorcontrib><creatorcontrib>ISAKOV V.F</creatorcontrib><title>METHOD FOR DYEING OF POLYESTER THREADS</title><description>FIELD: dyeing-finishing production; applicable in dyeing of polyester threads and ropes in course of their production. SUBSTANCE: method for dyeing of polyester threads is effected at thread tensioning of less than 0.3 gf/tex in one dyeing bath in two stages at temperature of 100.5-105.0 C. At the first stage, freshly spun fiber is dyed at constant speed of its transportation in the bath and at the second stage, it is dyed at increasing speed of transportation by 1.5-10 times. In this case, ratio of fiber path at the first stage to that at the second stage equals (1:1)-(2:1). EFFECT: higher efficiency. 1 cl, 3 dwg Использование: в красильно-отделочном производстве для крашения полиэфирных нитей и жгутов в процессе их получения. Сущность изобретения: способ крашения полиэфирных нитей осуществляют при натяжении нити менее 0,3 гс/текс в одной красильной ванне в две стадии при температуре 100,5-105,0°С, при этом на первой стадии крашение свежесформованной нити проводят при постоянной скорости транспортирования нитей в ванне, а на второй стадии - при возрастании скорости транспортирования нитей в 1,5-10 раз, причем отношение длины пути нити на первой стадии к длине пути нити на второй стадии равно 1:1 - 2: 1.</description><subject>DYEING LEATHER, FURS, OR SOLID MACROMOLECULAR SUBSTANCES INANY FORM</subject><subject>DYEING OR PRINTING TEXTILES</subject><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</subject><subject>LAUNDERING</subject><subject>TEXTILES</subject><subject>TREATMENT OF TEXTILES OR THE LIKE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1996</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFDzdQ3x8HdRcPMPUnCJdPX0c1fwd1MI8PeJdA0OcQ1SCPEIcnV0CeZhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoZYmBsaGJiYmjsZEKAEAfB8jQA</recordid><startdate>19960820</startdate><enddate>19960820</enddate><creator>ANDRONOVA A.P</creator><creator>ISAKOV V.F</creator><scope>EVB</scope></search><sort><creationdate>19960820</creationdate><title>METHOD FOR DYEING OF POLYESTER THREADS</title><author>ANDRONOVA A.P ; ISAKOV V.F</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU94031444A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>1996</creationdate><topic>DYEING LEATHER, FURS, OR SOLID MACROMOLECULAR SUBSTANCES INANY FORM</topic><topic>DYEING OR PRINTING TEXTILES</topic><topic>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</topic><topic>LAUNDERING</topic><topic>TEXTILES</topic><topic>TREATMENT OF TEXTILES OR THE LIKE</topic><toplevel>online_resources</toplevel><creatorcontrib>ANDRONOVA A.P</creatorcontrib><creatorcontrib>ISAKOV V.F</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ANDRONOVA A.P</au><au>ISAKOV V.F</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR DYEING OF POLYESTER THREADS</title><date>1996-08-20</date><risdate>1996</risdate><abstract>FIELD: dyeing-finishing production; applicable in dyeing of polyester threads and ropes in course of their production. SUBSTANCE: method for dyeing of polyester threads is effected at thread tensioning of less than 0.3 gf/tex in one dyeing bath in two stages at temperature of 100.5-105.0 C. At the first stage, freshly spun fiber is dyed at constant speed of its transportation in the bath and at the second stage, it is dyed at increasing speed of transportation by 1.5-10 times. In this case, ratio of fiber path at the first stage to that at the second stage equals (1:1)-(2:1). EFFECT: higher efficiency. 1 cl, 3 dwg Использование: в красильно-отделочном производстве для крашения полиэфирных нитей и жгутов в процессе их получения. Сущность изобретения: способ крашения полиэфирных нитей осуществляют при натяжении нити менее 0,3 гс/текс в одной красильной ванне в две стадии при температуре 100,5-105,0°С, при этом на первой стадии крашение свежесформованной нити проводят при постоянной скорости транспортирования нитей в ванне, а на второй стадии - при возрастании скорости транспортирования нитей в 1,5-10 раз, причем отношение длины пути нити на первой стадии к длине пути нити на второй стадии равно 1:1 - 2: 1.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU94031444A
source esp@cenet
subjects DYEING LEATHER, FURS, OR SOLID MACROMOLECULAR SUBSTANCES INANY FORM
DYEING OR PRINTING TEXTILES
FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR
LAUNDERING
TEXTILES
TREATMENT OF TEXTILES OR THE LIKE
title METHOD FOR DYEING OF POLYESTER THREADS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T13%3A45%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ANDRONOVA%20A.P&rft.date=1996-08-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU94031444A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true