METHOD FOR REMOVAL OF SLAG CRUST IN HOT-METAL TRANSFER LADLE

FIELD: ferrous metallurgy; particular, methods for cleaning of metallurgical vessels, mainly, hot-metal transfer ladles and casting ladles from scull. SUBSTANCE: slag crust in hot-metal transfer ladles is removed by chipping-off. Prior to pouring cast iron into ladle, lining is heated up to 100-300...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LARIONOV E.D, LARIONOV A.E, POTAPOV N.M, POTAPOV V.N
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LARIONOV E.D
LARIONOV A.E
POTAPOV N.M
POTAPOV V.N
description FIELD: ferrous metallurgy; particular, methods for cleaning of metallurgical vessels, mainly, hot-metal transfer ladles and casting ladles from scull. SUBSTANCE: slag crust in hot-metal transfer ladles is removed by chipping-off. Prior to pouring cast iron into ladle, lining is heated up to 100-300 C and applied to lining is insulating layer in form of refracting mixture of carbon powder of 3-0-mm fraction and water glass with density of 1.18-1.22 g/cu.cm. in percentage ratio of 78:22 to 82:18 and 15-25 mm thick which is not baking with ladle lining and slag. This provides for easy removal of slag crust. EFFECT: high productivity, no failure of hot-metal transfer ladles, improved their rhythmic service and increased service life of lining. Изобретение относится к черной металлургии, а именно к способам очистки металлургических емкостей, преимущественно чугуновозных и стеларазливочных ковшей от настылей. Шлаковые настыли в чугуновозных ковшах удаляют путем скалывания, до приема чугуна в ковш, футеровку разогревают до 100-300°С, наносят на нее изоляционный слой в виде огнеупорной смеси из углеродистого порошка фракции 3-0 мм и жидкого стекла плотностью 1,18-1,22 г/см3 , в % отношении в пределах от 78:22 до 82:18, толщиной 15-25 мм, неспекающийся с футеровкой ковша и шлаком. Это обеспечивает легкое удаление шлаковых настылей, за счет чего повышается производительность труда, чугуновозные ковши не выходят из строя, улучшается ритмичность их службы, долговечность футеровки.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU94026807A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU94026807A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU94026807A3</originalsourceid><addsrcrecordid>eNrjZLDxdQ3x8HdRcPMPUghy9fUPc_RR8HdTCPZxdFdwDgoNDlHw9FPw8A_RBaoDSoUEOfoFu7kGKfg4uvi48jCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQSxMDIzMLA3NHYyKUAACUzCkJ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR REMOVAL OF SLAG CRUST IN HOT-METAL TRANSFER LADLE</title><source>esp@cenet</source><creator>LARIONOV E.D ; LARIONOV A.E ; POTAPOV N.M ; POTAPOV V.N</creator><creatorcontrib>LARIONOV E.D ; LARIONOV A.E ; POTAPOV N.M ; POTAPOV V.N</creatorcontrib><description>FIELD: ferrous metallurgy; particular, methods for cleaning of metallurgical vessels, mainly, hot-metal transfer ladles and casting ladles from scull. SUBSTANCE: slag crust in hot-metal transfer ladles is removed by chipping-off. Prior to pouring cast iron into ladle, lining is heated up to 100-300 C and applied to lining is insulating layer in form of refracting mixture of carbon powder of 3-0-mm fraction and water glass with density of 1.18-1.22 g/cu.cm. in percentage ratio of 78:22 to 82:18 and 15-25 mm thick which is not baking with ladle lining and slag. This provides for easy removal of slag crust. EFFECT: high productivity, no failure of hot-metal transfer ladles, improved their rhythmic service and increased service life of lining. Изобретение относится к черной металлургии, а именно к способам очистки металлургических емкостей, преимущественно чугуновозных и стеларазливочных ковшей от настылей. Шлаковые настыли в чугуновозных ковшах удаляют путем скалывания, до приема чугуна в ковш, футеровку разогревают до 100-300°С, наносят на нее изоляционный слой в виде огнеупорной смеси из углеродистого порошка фракции 3-0 мм и жидкого стекла плотностью 1,18-1,22 г/см&lt;M^&gt;3 , в % отношении в пределах от 78:22 до 82:18, толщиной 15-25 мм, неспекающийся с футеровкой ковша и шлаком. Это обеспечивает легкое удаление шлаковых настылей, за счет чего повышается производительность труда, чугуновозные ковши не выходят из строя, улучшается ритмичность их службы, долговечность футеровки.</description><language>eng ; rus</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>1996</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960520&amp;DB=EPODOC&amp;CC=RU&amp;NR=94026807A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960520&amp;DB=EPODOC&amp;CC=RU&amp;NR=94026807A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LARIONOV E.D</creatorcontrib><creatorcontrib>LARIONOV A.E</creatorcontrib><creatorcontrib>POTAPOV N.M</creatorcontrib><creatorcontrib>POTAPOV V.N</creatorcontrib><title>METHOD FOR REMOVAL OF SLAG CRUST IN HOT-METAL TRANSFER LADLE</title><description>FIELD: ferrous metallurgy; particular, methods for cleaning of metallurgical vessels, mainly, hot-metal transfer ladles and casting ladles from scull. SUBSTANCE: slag crust in hot-metal transfer ladles is removed by chipping-off. Prior to pouring cast iron into ladle, lining is heated up to 100-300 C and applied to lining is insulating layer in form of refracting mixture of carbon powder of 3-0-mm fraction and water glass with density of 1.18-1.22 g/cu.cm. in percentage ratio of 78:22 to 82:18 and 15-25 mm thick which is not baking with ladle lining and slag. This provides for easy removal of slag crust. EFFECT: high productivity, no failure of hot-metal transfer ladles, improved their rhythmic service and increased service life of lining. Изобретение относится к черной металлургии, а именно к способам очистки металлургических емкостей, преимущественно чугуновозных и стеларазливочных ковшей от настылей. Шлаковые настыли в чугуновозных ковшах удаляют путем скалывания, до приема чугуна в ковш, футеровку разогревают до 100-300°С, наносят на нее изоляционный слой в виде огнеупорной смеси из углеродистого порошка фракции 3-0 мм и жидкого стекла плотностью 1,18-1,22 г/см&lt;M^&gt;3 , в % отношении в пределах от 78:22 до 82:18, толщиной 15-25 мм, неспекающийся с футеровкой ковша и шлаком. Это обеспечивает легкое удаление шлаковых настылей, за счет чего повышается производительность труда, чугуновозные ковши не выходят из строя, улучшается ритмичность их службы, долговечность футеровки.</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1996</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDxdQ3x8HdRcPMPUghy9fUPc_RR8HdTCPZxdFdwDgoNDlHw9FPw8A_RBaoDSoUEOfoFu7kGKfg4uvi48jCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQSxMDIzMLA3NHYyKUAACUzCkJ</recordid><startdate>19960520</startdate><enddate>19960520</enddate><creator>LARIONOV E.D</creator><creator>LARIONOV A.E</creator><creator>POTAPOV N.M</creator><creator>POTAPOV V.N</creator><scope>EVB</scope></search><sort><creationdate>19960520</creationdate><title>METHOD FOR REMOVAL OF SLAG CRUST IN HOT-METAL TRANSFER LADLE</title><author>LARIONOV E.D ; LARIONOV A.E ; POTAPOV N.M ; POTAPOV V.N</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU94026807A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>1996</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>LARIONOV E.D</creatorcontrib><creatorcontrib>LARIONOV A.E</creatorcontrib><creatorcontrib>POTAPOV N.M</creatorcontrib><creatorcontrib>POTAPOV V.N</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LARIONOV E.D</au><au>LARIONOV A.E</au><au>POTAPOV N.M</au><au>POTAPOV V.N</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR REMOVAL OF SLAG CRUST IN HOT-METAL TRANSFER LADLE</title><date>1996-05-20</date><risdate>1996</risdate><abstract>FIELD: ferrous metallurgy; particular, methods for cleaning of metallurgical vessels, mainly, hot-metal transfer ladles and casting ladles from scull. SUBSTANCE: slag crust in hot-metal transfer ladles is removed by chipping-off. Prior to pouring cast iron into ladle, lining is heated up to 100-300 C and applied to lining is insulating layer in form of refracting mixture of carbon powder of 3-0-mm fraction and water glass with density of 1.18-1.22 g/cu.cm. in percentage ratio of 78:22 to 82:18 and 15-25 mm thick which is not baking with ladle lining and slag. This provides for easy removal of slag crust. EFFECT: high productivity, no failure of hot-metal transfer ladles, improved their rhythmic service and increased service life of lining. Изобретение относится к черной металлургии, а именно к способам очистки металлургических емкостей, преимущественно чугуновозных и стеларазливочных ковшей от настылей. Шлаковые настыли в чугуновозных ковшах удаляют путем скалывания, до приема чугуна в ковш, футеровку разогревают до 100-300°С, наносят на нее изоляционный слой в виде огнеупорной смеси из углеродистого порошка фракции 3-0 мм и жидкого стекла плотностью 1,18-1,22 г/см&lt;M^&gt;3 , в % отношении в пределах от 78:22 до 82:18, толщиной 15-25 мм, неспекающийся с футеровкой ковша и шлаком. Это обеспечивает легкое удаление шлаковых настылей, за счет чего повышается производительность труда, чугуновозные ковши не выходят из строя, улучшается ритмичность их службы, долговечность футеровки.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU94026807A
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title METHOD FOR REMOVAL OF SLAG CRUST IN HOT-METAL TRANSFER LADLE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T18%3A50%3A56IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LARIONOV%20E.D&rft.date=1996-05-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU94026807A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true