METHOD OF CONTACT BUTT PRESSURE WELDING

FIELD: technological processes.SUBSTANCE: invention relates to butt-contact pressure welding and can be used in butt welding of metal rods. In the ends of the welded bars there performed are blind cylindrical holes, the rods are pressed along the annular contacts by welding force, the metal of the r...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Tarkhova Lejlya Mukaddasovna, Masyagutov Rivaz Faizovich, Akhmetyanov Ilshat Rasimovich, Akhmarov Ramzit Gavisovich, Nafikov Marat Zakievich, Zagirov Ilnur Ildarovich, Yunusbaev Nail Murtazovich
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Tarkhova Lejlya Mukaddasovna
Masyagutov Rivaz Faizovich
Akhmetyanov Ilshat Rasimovich
Akhmarov Ramzit Gavisovich
Nafikov Marat Zakievich
Zagirov Ilnur Ildarovich
Yunusbaev Nail Murtazovich
description FIELD: technological processes.SUBSTANCE: invention relates to butt-contact pressure welding and can be used in butt welding of metal rods. In the ends of the welded bars there performed are blind cylindrical holes, the rods are pressed along the annular contacts by welding force, the metal of the rods is heated to the plastic state by welding current and is settled. Limiting half-clamps fixed on rods at joint point restrict plastic deformation in direction from bars axis. Butt welding mode is selected based on the condition of complete filling of the holes with heated metal. Recommended cross-section of holes is selected equal to 0.5...0.6 of bars cross-section, depth - 0.15...0.20 of bar diameters.EFFECT: application of the welding method makes it possible to form high-strength welded connection of rods without formation in the zone of joint of the external surfacing.1 cl, 2 dwg Изобретение относится к области стыковой контактной сварки давлением и может быть использовано при стыковой сварке металлических прутков. В торцах свариваемых прутков предварительно выполняют глухие цилиндрические отверстия, прижимают прутки по кольцевым контактам сварочным усилием, разогревают металл прутков до пластического состояния сварочным током и осаживают. Установленные на прутках в месте стыка полухомуты ограничивают пластическую деформацию в направлении от оси прутков. Режим стыковой сварки выбирают из условия полного заполнения полостей отверстий разогретым металлом. Рекомендуемые сечения отверстий выбирают равными 0,5...0,6 сечений прутков, глубину - 0,15...0,20 диаметров прутков. Применение способа сварки позволяет сформировать высокопрочное сварное соединение прутков без образования в зоне стыка наружного наплыва. 2 ил.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2716923C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2716923C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2716923C13</originalsourceid><addsrcrecordid>eNrjZFD3dQ3x8HdR8HdTcPb3C3F0DlFwCg0JUQgIcg0ODg1yVQh39XHx9HPnYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxQaFG5oZmlkbGzobGRCgBAKWGI54</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF CONTACT BUTT PRESSURE WELDING</title><source>esp@cenet</source><creator>Tarkhova Lejlya Mukaddasovna ; Masyagutov Rivaz Faizovich ; Akhmetyanov Ilshat Rasimovich ; Akhmarov Ramzit Gavisovich ; Nafikov Marat Zakievich ; Zagirov Ilnur Ildarovich ; Yunusbaev Nail Murtazovich</creator><creatorcontrib>Tarkhova Lejlya Mukaddasovna ; Masyagutov Rivaz Faizovich ; Akhmetyanov Ilshat Rasimovich ; Akhmarov Ramzit Gavisovich ; Nafikov Marat Zakievich ; Zagirov Ilnur Ildarovich ; Yunusbaev Nail Murtazovich</creatorcontrib><description>FIELD: technological processes.SUBSTANCE: invention relates to butt-contact pressure welding and can be used in butt welding of metal rods. In the ends of the welded bars there performed are blind cylindrical holes, the rods are pressed along the annular contacts by welding force, the metal of the rods is heated to the plastic state by welding current and is settled. Limiting half-clamps fixed on rods at joint point restrict plastic deformation in direction from bars axis. Butt welding mode is selected based on the condition of complete filling of the holes with heated metal. Recommended cross-section of holes is selected equal to 0.5...0.6 of bars cross-section, depth - 0.15...0.20 of bar diameters.EFFECT: application of the welding method makes it possible to form high-strength welded connection of rods without formation in the zone of joint of the external surfacing.1 cl, 2 dwg Изобретение относится к области стыковой контактной сварки давлением и может быть использовано при стыковой сварке металлических прутков. В торцах свариваемых прутков предварительно выполняют глухие цилиндрические отверстия, прижимают прутки по кольцевым контактам сварочным усилием, разогревают металл прутков до пластического состояния сварочным током и осаживают. Установленные на прутках в месте стыка полухомуты ограничивают пластическую деформацию в направлении от оси прутков. Режим стыковой сварки выбирают из условия полного заполнения полостей отверстий разогретым металлом. Рекомендуемые сечения отверстий выбирают равными 0,5...0,6 сечений прутков, глубину - 0,15...0,20 диаметров прутков. Применение способа сварки позволяет сформировать высокопрочное сварное соединение прутков без образования в зоне стыка наружного наплыва. 2 ил.</description><language>eng ; rus</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200317&amp;DB=EPODOC&amp;CC=RU&amp;NR=2716923C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200317&amp;DB=EPODOC&amp;CC=RU&amp;NR=2716923C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Tarkhova Lejlya Mukaddasovna</creatorcontrib><creatorcontrib>Masyagutov Rivaz Faizovich</creatorcontrib><creatorcontrib>Akhmetyanov Ilshat Rasimovich</creatorcontrib><creatorcontrib>Akhmarov Ramzit Gavisovich</creatorcontrib><creatorcontrib>Nafikov Marat Zakievich</creatorcontrib><creatorcontrib>Zagirov Ilnur Ildarovich</creatorcontrib><creatorcontrib>Yunusbaev Nail Murtazovich</creatorcontrib><title>METHOD OF CONTACT BUTT PRESSURE WELDING</title><description>FIELD: technological processes.SUBSTANCE: invention relates to butt-contact pressure welding and can be used in butt welding of metal rods. In the ends of the welded bars there performed are blind cylindrical holes, the rods are pressed along the annular contacts by welding force, the metal of the rods is heated to the plastic state by welding current and is settled. Limiting half-clamps fixed on rods at joint point restrict plastic deformation in direction from bars axis. Butt welding mode is selected based on the condition of complete filling of the holes with heated metal. Recommended cross-section of holes is selected equal to 0.5...0.6 of bars cross-section, depth - 0.15...0.20 of bar diameters.EFFECT: application of the welding method makes it possible to form high-strength welded connection of rods without formation in the zone of joint of the external surfacing.1 cl, 2 dwg Изобретение относится к области стыковой контактной сварки давлением и может быть использовано при стыковой сварке металлических прутков. В торцах свариваемых прутков предварительно выполняют глухие цилиндрические отверстия, прижимают прутки по кольцевым контактам сварочным усилием, разогревают металл прутков до пластического состояния сварочным током и осаживают. Установленные на прутках в месте стыка полухомуты ограничивают пластическую деформацию в направлении от оси прутков. Режим стыковой сварки выбирают из условия полного заполнения полостей отверстий разогретым металлом. Рекомендуемые сечения отверстий выбирают равными 0,5...0,6 сечений прутков, глубину - 0,15...0,20 диаметров прутков. Применение способа сварки позволяет сформировать высокопрочное сварное соединение прутков без образования в зоне стыка наружного наплыва. 2 ил.</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD3dQ3x8HdR8HdTcPb3C3F0DlFwCg0JUQgIcg0ODg1yVQh39XHx9HPnYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxQaFG5oZmlkbGzobGRCgBAKWGI54</recordid><startdate>20200317</startdate><enddate>20200317</enddate><creator>Tarkhova Lejlya Mukaddasovna</creator><creator>Masyagutov Rivaz Faizovich</creator><creator>Akhmetyanov Ilshat Rasimovich</creator><creator>Akhmarov Ramzit Gavisovich</creator><creator>Nafikov Marat Zakievich</creator><creator>Zagirov Ilnur Ildarovich</creator><creator>Yunusbaev Nail Murtazovich</creator><scope>EVB</scope></search><sort><creationdate>20200317</creationdate><title>METHOD OF CONTACT BUTT PRESSURE WELDING</title><author>Tarkhova Lejlya Mukaddasovna ; Masyagutov Rivaz Faizovich ; Akhmetyanov Ilshat Rasimovich ; Akhmarov Ramzit Gavisovich ; Nafikov Marat Zakievich ; Zagirov Ilnur Ildarovich ; Yunusbaev Nail Murtazovich</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2716923C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2020</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>Tarkhova Lejlya Mukaddasovna</creatorcontrib><creatorcontrib>Masyagutov Rivaz Faizovich</creatorcontrib><creatorcontrib>Akhmetyanov Ilshat Rasimovich</creatorcontrib><creatorcontrib>Akhmarov Ramzit Gavisovich</creatorcontrib><creatorcontrib>Nafikov Marat Zakievich</creatorcontrib><creatorcontrib>Zagirov Ilnur Ildarovich</creatorcontrib><creatorcontrib>Yunusbaev Nail Murtazovich</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Tarkhova Lejlya Mukaddasovna</au><au>Masyagutov Rivaz Faizovich</au><au>Akhmetyanov Ilshat Rasimovich</au><au>Akhmarov Ramzit Gavisovich</au><au>Nafikov Marat Zakievich</au><au>Zagirov Ilnur Ildarovich</au><au>Yunusbaev Nail Murtazovich</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF CONTACT BUTT PRESSURE WELDING</title><date>2020-03-17</date><risdate>2020</risdate><abstract>FIELD: technological processes.SUBSTANCE: invention relates to butt-contact pressure welding and can be used in butt welding of metal rods. In the ends of the welded bars there performed are blind cylindrical holes, the rods are pressed along the annular contacts by welding force, the metal of the rods is heated to the plastic state by welding current and is settled. Limiting half-clamps fixed on rods at joint point restrict plastic deformation in direction from bars axis. Butt welding mode is selected based on the condition of complete filling of the holes with heated metal. Recommended cross-section of holes is selected equal to 0.5...0.6 of bars cross-section, depth - 0.15...0.20 of bar diameters.EFFECT: application of the welding method makes it possible to form high-strength welded connection of rods without formation in the zone of joint of the external surfacing.1 cl, 2 dwg Изобретение относится к области стыковой контактной сварки давлением и может быть использовано при стыковой сварке металлических прутков. В торцах свариваемых прутков предварительно выполняют глухие цилиндрические отверстия, прижимают прутки по кольцевым контактам сварочным усилием, разогревают металл прутков до пластического состояния сварочным током и осаживают. Установленные на прутках в месте стыка полухомуты ограничивают пластическую деформацию в направлении от оси прутков. Режим стыковой сварки выбирают из условия полного заполнения полостей отверстий разогретым металлом. Рекомендуемые сечения отверстий выбирают равными 0,5...0,6 сечений прутков, глубину - 0,15...0,20 диаметров прутков. Применение способа сварки позволяет сформировать высокопрочное сварное соединение прутков без образования в зоне стыка наружного наплыва. 2 ил.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2716923C1
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title METHOD OF CONTACT BUTT PRESSURE WELDING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T03%3A43%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Tarkhova%20Lejlya%20Mukaddasovna&rft.date=2020-03-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2716923C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true