METHOD FOR PRODUCING VALVE-METAL SINTERED ITEMS HAVING LARGE SPECIFIC SURFACE AREA AND LOW OXYGEN CONTENT

FIELD: metallurgy.SUBSTANCE: group of inventions relates to the manufacture of sintered items from the powder of valve metals. Said valve metal powder contains more than 4,100 ppm g/mof oxygen, nitrogen in the amount of less than 300 ppm, boron less than 10 ppm, sulfur in quantities of less than 20 ...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KHAAS, Khelmut, KHAGIMASI, Marsel, RAVOL, Kristin
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KHAAS, Khelmut
KHAGIMASI, Marsel
RAVOL, Kristin
description FIELD: metallurgy.SUBSTANCE: group of inventions relates to the manufacture of sintered items from the powder of valve metals. Said valve metal powder contains more than 4,100 ppm g/mof oxygen, nitrogen in the amount of less than 300 ppm, boron less than 10 ppm, sulfur in quantities of less than 20 ppm, silicon in an amount of less than 20 ppm, arsenic less than 10 ppm and phosphorus in an amount of less than 20 ppm. This method of manufacturing a sintered item includes pressing a powder, providing the resulting pressed product with a solid or liquid reducing agent, wherein the pressed product is not in direct contact or does not come into direct contact with the reducing agent, heating to ensure sintering of the powder to obtain a sintered item, which has an oxygen content of from 2,400 to 3,600 ppm g/m.EFFECT: low oxygen content and high resistance to tearing the wire embedded in an anode item are provided.33 cl, 2 dwg, 8 tbl Группа изобретений относится к изготовлению спеченных изделий из порошка вентильных металлов. Порошок вентильного металла содержит кислород в количестве более 4100 ч.н.м.⋅г/м, азот в количестве менее 300 ч.н.м., бор в количестве менее 10 ч.н.м., серу в количестве менее 20 ч.н.м., кремний в количестве менее 20 ч.н.м., мышьяк в количестве менее 10 ч.н.м. и фосфор в количестве менее 20 ч.н.м. Способ изготовления спеченного изделия включает прессование порошка, предоставление полученного прессованного изделия с твердым или жидким восстановителем, причем прессованное изделие не находится в непосредственном контакте или не вступает в непосредственный контакт с восстановителем, нагревание с обеспечением спекания порошка с получением спеченного изделия, которое имеет содержание кислорода от 2400 до 3600 ч.н.м.⋅г/м. Обеспечивается низкое содержание кислорода и высокая прочность на вырывание заделанного в анодное изделие провода. 4 н. и 29 з.п. ф-лы, 2 ил., 8 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2678220C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2678220C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2678220C23</originalsourceid><addsrcrecordid>eNqNjEEKwjAQAHvxIOof9gMFiaBel82mDaRJSdKop1IkgiBaqP_HCj7A0xxmmGVxbzjWToJyHlrvZEfaVpDQJC5nhQaCtpE9S9CRmwA1pm9h0FcMoWXSShOEziskBvSMgFaCcSdw50vFFsjNAxvXxeI2PKa8-XFVgOJIdZnHV5-ncbjmZ373vhP7w1GILYndH8kH2341cw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING VALVE-METAL SINTERED ITEMS HAVING LARGE SPECIFIC SURFACE AREA AND LOW OXYGEN CONTENT</title><source>esp@cenet</source><creator>KHAAS, Khelmut ; KHAGIMASI, Marsel ; RAVOL, Kristin</creator><creatorcontrib>KHAAS, Khelmut ; KHAGIMASI, Marsel ; RAVOL, Kristin</creatorcontrib><description>FIELD: metallurgy.SUBSTANCE: group of inventions relates to the manufacture of sintered items from the powder of valve metals. Said valve metal powder contains more than 4,100 ppm g/mof oxygen, nitrogen in the amount of less than 300 ppm, boron less than 10 ppm, sulfur in quantities of less than 20 ppm, silicon in an amount of less than 20 ppm, arsenic less than 10 ppm and phosphorus in an amount of less than 20 ppm. This method of manufacturing a sintered item includes pressing a powder, providing the resulting pressed product with a solid or liquid reducing agent, wherein the pressed product is not in direct contact or does not come into direct contact with the reducing agent, heating to ensure sintering of the powder to obtain a sintered item, which has an oxygen content of from 2,400 to 3,600 ppm g/m.EFFECT: low oxygen content and high resistance to tearing the wire embedded in an anode item are provided.33 cl, 2 dwg, 8 tbl Группа изобретений относится к изготовлению спеченных изделий из порошка вентильных металлов. Порошок вентильного металла содержит кислород в количестве более 4100 ч.н.м.⋅г/м, азот в количестве менее 300 ч.н.м., бор в количестве менее 10 ч.н.м., серу в количестве менее 20 ч.н.м., кремний в количестве менее 20 ч.н.м., мышьяк в количестве менее 10 ч.н.м. и фосфор в количестве менее 20 ч.н.м. Способ изготовления спеченного изделия включает прессование порошка, предоставление полученного прессованного изделия с твердым или жидким восстановителем, причем прессованное изделие не находится в непосредственном контакте или не вступает в непосредственный контакт с восстановителем, нагревание с обеспечением спекания порошка с получением спеченного изделия, которое имеет содержание кислорода от 2400 до 3600 ч.н.м.⋅г/м. Обеспечивается низкое содержание кислорода и высокая прочность на вырывание заделанного в анодное изделие провода. 4 н. и 29 з.п. ф-лы, 2 ил., 8 табл.</description><language>eng ; rus</language><subject>ALLOYS ; CASTING ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; MAKING METALLIC POWDER ; MANUFACTURE OF ARTICLES FROM METALLIC POWDER ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS ; WORKING METALLIC POWDER</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190124&amp;DB=EPODOC&amp;CC=RU&amp;NR=2678220C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190124&amp;DB=EPODOC&amp;CC=RU&amp;NR=2678220C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KHAAS, Khelmut</creatorcontrib><creatorcontrib>KHAGIMASI, Marsel</creatorcontrib><creatorcontrib>RAVOL, Kristin</creatorcontrib><title>METHOD FOR PRODUCING VALVE-METAL SINTERED ITEMS HAVING LARGE SPECIFIC SURFACE AREA AND LOW OXYGEN CONTENT</title><description>FIELD: metallurgy.SUBSTANCE: group of inventions relates to the manufacture of sintered items from the powder of valve metals. Said valve metal powder contains more than 4,100 ppm g/mof oxygen, nitrogen in the amount of less than 300 ppm, boron less than 10 ppm, sulfur in quantities of less than 20 ppm, silicon in an amount of less than 20 ppm, arsenic less than 10 ppm and phosphorus in an amount of less than 20 ppm. This method of manufacturing a sintered item includes pressing a powder, providing the resulting pressed product with a solid or liquid reducing agent, wherein the pressed product is not in direct contact or does not come into direct contact with the reducing agent, heating to ensure sintering of the powder to obtain a sintered item, which has an oxygen content of from 2,400 to 3,600 ppm g/m.EFFECT: low oxygen content and high resistance to tearing the wire embedded in an anode item are provided.33 cl, 2 dwg, 8 tbl Группа изобретений относится к изготовлению спеченных изделий из порошка вентильных металлов. Порошок вентильного металла содержит кислород в количестве более 4100 ч.н.м.⋅г/м, азот в количестве менее 300 ч.н.м., бор в количестве менее 10 ч.н.м., серу в количестве менее 20 ч.н.м., кремний в количестве менее 20 ч.н.м., мышьяк в количестве менее 10 ч.н.м. и фосфор в количестве менее 20 ч.н.м. Способ изготовления спеченного изделия включает прессование порошка, предоставление полученного прессованного изделия с твердым или жидким восстановителем, причем прессованное изделие не находится в непосредственном контакте или не вступает в непосредственный контакт с восстановителем, нагревание с обеспечением спекания порошка с получением спеченного изделия, которое имеет содержание кислорода от 2400 до 3600 ч.н.м.⋅г/м. Обеспечивается низкое содержание кислорода и высокая прочность на вырывание заделанного в анодное изделие провода. 4 н. и 29 з.п. ф-лы, 2 ил., 8 табл.</description><subject>ALLOYS</subject><subject>CASTING</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>MAKING METALLIC POWDER</subject><subject>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><subject>WORKING METALLIC POWDER</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEEKwjAQAHvxIOof9gMFiaBel82mDaRJSdKop1IkgiBaqP_HCj7A0xxmmGVxbzjWToJyHlrvZEfaVpDQJC5nhQaCtpE9S9CRmwA1pm9h0FcMoWXSShOEziskBvSMgFaCcSdw50vFFsjNAxvXxeI2PKa8-XFVgOJIdZnHV5-ncbjmZ373vhP7w1GILYndH8kH2341cw</recordid><startdate>20190124</startdate><enddate>20190124</enddate><creator>KHAAS, Khelmut</creator><creator>KHAGIMASI, Marsel</creator><creator>RAVOL, Kristin</creator><scope>EVB</scope></search><sort><creationdate>20190124</creationdate><title>METHOD FOR PRODUCING VALVE-METAL SINTERED ITEMS HAVING LARGE SPECIFIC SURFACE AREA AND LOW OXYGEN CONTENT</title><author>KHAAS, Khelmut ; KHAGIMASI, Marsel ; RAVOL, Kristin</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2678220C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2019</creationdate><topic>ALLOYS</topic><topic>CASTING</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>MAKING METALLIC POWDER</topic><topic>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><topic>WORKING METALLIC POWDER</topic><toplevel>online_resources</toplevel><creatorcontrib>KHAAS, Khelmut</creatorcontrib><creatorcontrib>KHAGIMASI, Marsel</creatorcontrib><creatorcontrib>RAVOL, Kristin</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KHAAS, Khelmut</au><au>KHAGIMASI, Marsel</au><au>RAVOL, Kristin</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING VALVE-METAL SINTERED ITEMS HAVING LARGE SPECIFIC SURFACE AREA AND LOW OXYGEN CONTENT</title><date>2019-01-24</date><risdate>2019</risdate><abstract>FIELD: metallurgy.SUBSTANCE: group of inventions relates to the manufacture of sintered items from the powder of valve metals. Said valve metal powder contains more than 4,100 ppm g/mof oxygen, nitrogen in the amount of less than 300 ppm, boron less than 10 ppm, sulfur in quantities of less than 20 ppm, silicon in an amount of less than 20 ppm, arsenic less than 10 ppm and phosphorus in an amount of less than 20 ppm. This method of manufacturing a sintered item includes pressing a powder, providing the resulting pressed product with a solid or liquid reducing agent, wherein the pressed product is not in direct contact or does not come into direct contact with the reducing agent, heating to ensure sintering of the powder to obtain a sintered item, which has an oxygen content of from 2,400 to 3,600 ppm g/m.EFFECT: low oxygen content and high resistance to tearing the wire embedded in an anode item are provided.33 cl, 2 dwg, 8 tbl Группа изобретений относится к изготовлению спеченных изделий из порошка вентильных металлов. Порошок вентильного металла содержит кислород в количестве более 4100 ч.н.м.⋅г/м, азот в количестве менее 300 ч.н.м., бор в количестве менее 10 ч.н.м., серу в количестве менее 20 ч.н.м., кремний в количестве менее 20 ч.н.м., мышьяк в количестве менее 10 ч.н.м. и фосфор в количестве менее 20 ч.н.м. Способ изготовления спеченного изделия включает прессование порошка, предоставление полученного прессованного изделия с твердым или жидким восстановителем, причем прессованное изделие не находится в непосредственном контакте или не вступает в непосредственный контакт с восстановителем, нагревание с обеспечением спекания порошка с получением спеченного изделия, которое имеет содержание кислорода от 2400 до 3600 ч.н.м.⋅г/м. Обеспечивается низкое содержание кислорода и высокая прочность на вырывание заделанного в анодное изделие провода. 4 н. и 29 з.п. ф-лы, 2 ил., 8 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2678220C2
source esp@cenet
subjects ALLOYS
CASTING
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
MAKING METALLIC POWDER
MANUFACTURE OF ARTICLES FROM METALLIC POWDER
METALLURGY
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
WORKING METALLIC POWDER
title METHOD FOR PRODUCING VALVE-METAL SINTERED ITEMS HAVING LARGE SPECIFIC SURFACE AREA AND LOW OXYGEN CONTENT
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-26T06%3A20%3A02IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KHAAS,%20Khelmut&rft.date=2019-01-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2678220C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true