METHOD OF OBTAINING BITUMEN EMULSION AND THE BITUMEN EMULSION

FIELD: construction.SUBSTANCE: technical solution relates to the field of building materials, more particularly to bitumen emulsions, and can be used for the production of heat and waterproofing materials intended for the construction and repair of various roofs, as well as in road construction as a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Ivanov Aleksandr Fedorovich, Andronov Sergej Yurevich, Kochetkov Andrej Viktorovich, Korotkovskij Sergej Alekseevich, Artemev Sergej Vyacheslavovich, Yankovskij Leonid Vatslavovich, Talalaj Viktor Vyacheslavovich
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Ivanov Aleksandr Fedorovich
Andronov Sergej Yurevich
Kochetkov Andrej Viktorovich
Korotkovskij Sergej Alekseevich
Artemev Sergej Vyacheslavovich
Yankovskij Leonid Vatslavovich
Talalaj Viktor Vyacheslavovich
description FIELD: construction.SUBSTANCE: technical solution relates to the field of building materials, more particularly to bitumen emulsions, and can be used for the production of heat and waterproofing materials intended for the construction and repair of various roofs, as well as in road construction as a binder for asphalt concrete mixtures. Method for producing a bitumen emulsion comprises the preparation of an aqueous solution of an emulsifier by mixing under a constant mixing in a certain proportion in water a solid emulsifier, that is used as phosphogypsum, and subsequent introduction into the finished aqueous solution of the emulsifier of the heated bitumen. Before mixing the solid emulsifier with water, it is crushed and milled in air into a powdered activated dispersed medium with a particle size of 0.063-0.1 mm, then connect it with water at temperature of 15-30 °C, and the bitumen is heated up-to temperature of 130-160 °C. Bitumen emulsion obtained after mixing the components has a composition, by mass %: bitumen - 20-25 %, phosphogypsum - 50-60 %, service water - 20-25 %.EFFECT: increase the processability of the method of preparation of bitumen emulsion and its application at the place of production, increase the shelf life of the bitumen emulsion and the strength characteristics of the final product (structure).8 cl, 1 dwg Техническое решение относится к области строительных материалов, более конкретно к битумным эмульсиям, и может быть использовано для производства тепло- и гидроизоляционных материалов, предназначенных для устройства и ремонта разнообразных кровель, а также в дорожном строительстве в качестве вяжущего для асфальтобетонных смесей. Способ получения битумной эмульсии включает приготовление водного раствора эмульгатора путем смешения при постоянном перемешивании в определенной пропорции в воде твердого эмульгатора, в качестве которого используют фосфогипс, и последующего введения в готовый водный раствор эмульгатора разогретого битума. Перед смешением твердого эмульгатора с водой осуществляют его дробление и перемалывание в воздушной среде в порошковую активированную дисперсную среду с размером частиц 0,063-0,1 мм, затем соединяют его с водой при температуре 15°С-30°C, а битум разогревают до температуры 130°С-160°C. Битумная эмульсия, полученная после смешения компонентов, имеет состав, мас. %: битум - 20-25%, фосфогипс - 50-60%, вода техническая - 20-25%. Техническим результатом изобретения является повышение технологичности способа п
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2662493C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2662493C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2662493C13</originalsourceid><addsrcrecordid>eNrjZLD1dQ3x8HdR8HdT8HcKcfT08_RzV3DyDAn1dfVTcPUN9Qn29PdTcPRzUQjxcMWQ4GFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8UGhRmZmRiaWxs6GxkQoAQDboSmZ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF OBTAINING BITUMEN EMULSION AND THE BITUMEN EMULSION</title><source>esp@cenet</source><creator>Ivanov Aleksandr Fedorovich ; Andronov Sergej Yurevich ; Kochetkov Andrej Viktorovich ; Korotkovskij Sergej Alekseevich ; Artemev Sergej Vyacheslavovich ; Yankovskij Leonid Vatslavovich ; Talalaj Viktor Vyacheslavovich</creator><creatorcontrib>Ivanov Aleksandr Fedorovich ; Andronov Sergej Yurevich ; Kochetkov Andrej Viktorovich ; Korotkovskij Sergej Alekseevich ; Artemev Sergej Vyacheslavovich ; Yankovskij Leonid Vatslavovich ; Talalaj Viktor Vyacheslavovich</creatorcontrib><description>FIELD: construction.SUBSTANCE: technical solution relates to the field of building materials, more particularly to bitumen emulsions, and can be used for the production of heat and waterproofing materials intended for the construction and repair of various roofs, as well as in road construction as a binder for asphalt concrete mixtures. Method for producing a bitumen emulsion comprises the preparation of an aqueous solution of an emulsifier by mixing under a constant mixing in a certain proportion in water a solid emulsifier, that is used as phosphogypsum, and subsequent introduction into the finished aqueous solution of the emulsifier of the heated bitumen. Before mixing the solid emulsifier with water, it is crushed and milled in air into a powdered activated dispersed medium with a particle size of 0.063-0.1 mm, then connect it with water at temperature of 15-30 °C, and the bitumen is heated up-to temperature of 130-160 °C. Bitumen emulsion obtained after mixing the components has a composition, by mass %: bitumen - 20-25 %, phosphogypsum - 50-60 %, service water - 20-25 %.EFFECT: increase the processability of the method of preparation of bitumen emulsion and its application at the place of production, increase the shelf life of the bitumen emulsion and the strength characteristics of the final product (structure).8 cl, 1 dwg Техническое решение относится к области строительных материалов, более конкретно к битумным эмульсиям, и может быть использовано для производства тепло- и гидроизоляционных материалов, предназначенных для устройства и ремонта разнообразных кровель, а также в дорожном строительстве в качестве вяжущего для асфальтобетонных смесей. Способ получения битумной эмульсии включает приготовление водного раствора эмульгатора путем смешения при постоянном перемешивании в определенной пропорции в воде твердого эмульгатора, в качестве которого используют фосфогипс, и последующего введения в готовый водный раствор эмульгатора разогретого битума. Перед смешением твердого эмульгатора с водой осуществляют его дробление и перемалывание в воздушной среде в порошковую активированную дисперсную среду с размером частиц 0,063-0,1 мм, затем соединяют его с водой при температуре 15°С-30°C, а битум разогревают до температуры 130°С-160°C. Битумная эмульсия, полученная после смешения компонентов, имеет состав, мас. %: битум - 20-25%, фосфогипс - 50-60%, вода техническая - 20-25%. Техническим результатом изобретения является повышение технологичности способа приготовления битумной эмульсии и применения ее на месте производства работ, увеличение срока хранения битумной эмульсии и прочностных характеристик конечного изделия (конструкции). 2 н. и 6 з.п. ф-лы, 1 ил.</description><language>eng ; rus</language><subject>ADHESIVES ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; DYES ; MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; POLISHES ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180726&amp;DB=EPODOC&amp;CC=RU&amp;NR=2662493C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180726&amp;DB=EPODOC&amp;CC=RU&amp;NR=2662493C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Ivanov Aleksandr Fedorovich</creatorcontrib><creatorcontrib>Andronov Sergej Yurevich</creatorcontrib><creatorcontrib>Kochetkov Andrej Viktorovich</creatorcontrib><creatorcontrib>Korotkovskij Sergej Alekseevich</creatorcontrib><creatorcontrib>Artemev Sergej Vyacheslavovich</creatorcontrib><creatorcontrib>Yankovskij Leonid Vatslavovich</creatorcontrib><creatorcontrib>Talalaj Viktor Vyacheslavovich</creatorcontrib><title>METHOD OF OBTAINING BITUMEN EMULSION AND THE BITUMEN EMULSION</title><description>FIELD: construction.SUBSTANCE: technical solution relates to the field of building materials, more particularly to bitumen emulsions, and can be used for the production of heat and waterproofing materials intended for the construction and repair of various roofs, as well as in road construction as a binder for asphalt concrete mixtures. Method for producing a bitumen emulsion comprises the preparation of an aqueous solution of an emulsifier by mixing under a constant mixing in a certain proportion in water a solid emulsifier, that is used as phosphogypsum, and subsequent introduction into the finished aqueous solution of the emulsifier of the heated bitumen. Before mixing the solid emulsifier with water, it is crushed and milled in air into a powdered activated dispersed medium with a particle size of 0.063-0.1 mm, then connect it with water at temperature of 15-30 °C, and the bitumen is heated up-to temperature of 130-160 °C. Bitumen emulsion obtained after mixing the components has a composition, by mass %: bitumen - 20-25 %, phosphogypsum - 50-60 %, service water - 20-25 %.EFFECT: increase the processability of the method of preparation of bitumen emulsion and its application at the place of production, increase the shelf life of the bitumen emulsion and the strength characteristics of the final product (structure).8 cl, 1 dwg Техническое решение относится к области строительных материалов, более конкретно к битумным эмульсиям, и может быть использовано для производства тепло- и гидроизоляционных материалов, предназначенных для устройства и ремонта разнообразных кровель, а также в дорожном строительстве в качестве вяжущего для асфальтобетонных смесей. Способ получения битумной эмульсии включает приготовление водного раствора эмульгатора путем смешения при постоянном перемешивании в определенной пропорции в воде твердого эмульгатора, в качестве которого используют фосфогипс, и последующего введения в готовый водный раствор эмульгатора разогретого битума. Перед смешением твердого эмульгатора с водой осуществляют его дробление и перемалывание в воздушной среде в порошковую активированную дисперсную среду с размером частиц 0,063-0,1 мм, затем соединяют его с водой при температуре 15°С-30°C, а битум разогревают до температуры 130°С-160°C. Битумная эмульсия, полученная после смешения компонентов, имеет состав, мас. %: битум - 20-25%, фосфогипс - 50-60%, вода техническая - 20-25%. Техническим результатом изобретения является повышение технологичности способа приготовления битумной эмульсии и применения ее на месте производства работ, увеличение срока хранения битумной эмульсии и прочностных характеристик конечного изделия (конструкции). 2 н. и 6 з.п. ф-лы, 1 ил.</description><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>DYES</subject><subject>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLD1dQ3x8HdR8HdT8HcKcfT08_RzV3DyDAn1dfVTcPUN9Qn29PdTcPRzUQjxcMWQ4GFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8UGhRmZmRiaWxs6GxkQoAQDboSmZ</recordid><startdate>20180726</startdate><enddate>20180726</enddate><creator>Ivanov Aleksandr Fedorovich</creator><creator>Andronov Sergej Yurevich</creator><creator>Kochetkov Andrej Viktorovich</creator><creator>Korotkovskij Sergej Alekseevich</creator><creator>Artemev Sergej Vyacheslavovich</creator><creator>Yankovskij Leonid Vatslavovich</creator><creator>Talalaj Viktor Vyacheslavovich</creator><scope>EVB</scope></search><sort><creationdate>20180726</creationdate><title>METHOD OF OBTAINING BITUMEN EMULSION AND THE BITUMEN EMULSION</title><author>Ivanov Aleksandr Fedorovich ; Andronov Sergej Yurevich ; Kochetkov Andrej Viktorovich ; Korotkovskij Sergej Alekseevich ; Artemev Sergej Vyacheslavovich ; Yankovskij Leonid Vatslavovich ; Talalaj Viktor Vyacheslavovich</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2662493C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2018</creationdate><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>DYES</topic><topic>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>Ivanov Aleksandr Fedorovich</creatorcontrib><creatorcontrib>Andronov Sergej Yurevich</creatorcontrib><creatorcontrib>Kochetkov Andrej Viktorovich</creatorcontrib><creatorcontrib>Korotkovskij Sergej Alekseevich</creatorcontrib><creatorcontrib>Artemev Sergej Vyacheslavovich</creatorcontrib><creatorcontrib>Yankovskij Leonid Vatslavovich</creatorcontrib><creatorcontrib>Talalaj Viktor Vyacheslavovich</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Ivanov Aleksandr Fedorovich</au><au>Andronov Sergej Yurevich</au><au>Kochetkov Andrej Viktorovich</au><au>Korotkovskij Sergej Alekseevich</au><au>Artemev Sergej Vyacheslavovich</au><au>Yankovskij Leonid Vatslavovich</au><au>Talalaj Viktor Vyacheslavovich</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF OBTAINING BITUMEN EMULSION AND THE BITUMEN EMULSION</title><date>2018-07-26</date><risdate>2018</risdate><abstract>FIELD: construction.SUBSTANCE: technical solution relates to the field of building materials, more particularly to bitumen emulsions, and can be used for the production of heat and waterproofing materials intended for the construction and repair of various roofs, as well as in road construction as a binder for asphalt concrete mixtures. Method for producing a bitumen emulsion comprises the preparation of an aqueous solution of an emulsifier by mixing under a constant mixing in a certain proportion in water a solid emulsifier, that is used as phosphogypsum, and subsequent introduction into the finished aqueous solution of the emulsifier of the heated bitumen. Before mixing the solid emulsifier with water, it is crushed and milled in air into a powdered activated dispersed medium with a particle size of 0.063-0.1 mm, then connect it with water at temperature of 15-30 °C, and the bitumen is heated up-to temperature of 130-160 °C. Bitumen emulsion obtained after mixing the components has a composition, by mass %: bitumen - 20-25 %, phosphogypsum - 50-60 %, service water - 20-25 %.EFFECT: increase the processability of the method of preparation of bitumen emulsion and its application at the place of production, increase the shelf life of the bitumen emulsion and the strength characteristics of the final product (structure).8 cl, 1 dwg Техническое решение относится к области строительных материалов, более конкретно к битумным эмульсиям, и может быть использовано для производства тепло- и гидроизоляционных материалов, предназначенных для устройства и ремонта разнообразных кровель, а также в дорожном строительстве в качестве вяжущего для асфальтобетонных смесей. Способ получения битумной эмульсии включает приготовление водного раствора эмульгатора путем смешения при постоянном перемешивании в определенной пропорции в воде твердого эмульгатора, в качестве которого используют фосфогипс, и последующего введения в готовый водный раствор эмульгатора разогретого битума. Перед смешением твердого эмульгатора с водой осуществляют его дробление и перемалывание в воздушной среде в порошковую активированную дисперсную среду с размером частиц 0,063-0,1 мм, затем соединяют его с водой при температуре 15°С-30°C, а битум разогревают до температуры 130°С-160°C. Битумная эмульсия, полученная после смешения компонентов, имеет состав, мас. %: битум - 20-25%, фосфогипс - 50-60%, вода техническая - 20-25%. Техническим результатом изобретения является повышение технологичности способа приготовления битумной эмульсии и применения ее на месте производства работ, увеличение срока хранения битумной эмульсии и прочностных характеристик конечного изделия (конструкции). 2 н. и 6 з.п. ф-лы, 1 ил.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2662493C1
source esp@cenet
subjects ADHESIVES
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
DYES
MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
ORGANIC MACROMOLECULAR COMPOUNDS
PAINTS
POLISHES
THEIR PREPARATION OR CHEMICAL WORKING-UP
title METHOD OF OBTAINING BITUMEN EMULSION AND THE BITUMEN EMULSION
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T03%3A30%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Ivanov%20Aleksandr%20Fedorovich&rft.date=2018-07-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2662493C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true