METHOD FOR PRODUCING CARBOBORIDES OF RARE-EARTH METALS
FIELD: metallurgy.SUBSTANCE: initial blank is shaped as a stoichiometric powder charge of low hydride phase of metal, carbon and boron, after that the initial blank is annealed in vacuum at 1100°C for 10 minutes, the blank is cooled, ground and pressed into a rod, which is annealed at 1100°C for 10...