MANUFACTURE METHOD OF COMPRESSOR BLADES FROM TITANIUM ALLOY VT6
FIELD: metallurgy.SUBSTANCE: provide the hot gas moulding of the ingot with superplastic deformation at the temperatures from 870 up to 1000°C and the deformation rate 10c. Then using the ion-plasma condensation method, the optimally selected Ni-Ti-Cr-Y alloyage is deposited on the surface of the re...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: metallurgy.SUBSTANCE: provide the hot gas moulding of the ingot with superplastic deformation at the temperatures from 870 up to 1000°C and the deformation rate 10c. Then using the ion-plasma condensation method, the optimally selected Ni-Ti-Cr-Y alloyage is deposited on the surface of the resulted blades. After this, the compressor finished blades heat treatment is provided at the temperature of 870 to 950°C.EFFECT: method provides high mechanical properties of compressor blades made from titanium alloy VT6, in particular the fatigue strength, the heat resistance, the fracture toughness.1 cl
Изобретение может быть использовано для изготовления лопатки компрессора из высокопрочного титанового сплава ВТ6 на основе эвтектоидной системы легирования. Проводят горячую газовую формовку слитка со сверхпластической деформацией при температуре от 870 до 1000°С и скорости деформации 10c. Затем методом ионно-плазменного конденсирования на поверхность полученных лопаток осаждают оптимально подобранную лигатуру Ni-Ti-Cr-Y. После этого проводят термическую обработку готовых лопаток компрессора при температуре от 870 до 950°С. Способ обеспечивает высокие механические свойства лопаток компрессора из титанового сплава ВТ6, в частности усталостную прочность, жаропрочность, вязкость разрушения. |
---|