METHOD FOR PRODUCING HEAT-INSULATING PRODUCT BASED ON VERMICULITE
FIELD: construction.SUBSTANCE: method for producing a heat-insulating product based on vermiculite involves production of a binding mixture by mixing potassium hydroxide, microsilica and water, which is preheated up to the temperature of 70 - 85°C, mixing of the binding mixture with foamed vermiculi...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | RAKHMANOVA IRINA ANATOL'EVNA RJABOV SERGEJ IVANOVICH SARKISOV JURIJ SERGEEVICH |
description | FIELD: construction.SUBSTANCE: method for producing a heat-insulating product based on vermiculite involves production of a binding mixture by mixing potassium hydroxide, microsilica and water, which is preheated up to the temperature of 70 - 85°C, mixing of the binding mixture with foamed vermiculite, arrangement of the obtained raw mass in a mould and compaction, fixation of the mould by a tight cover, placement into a furnace pre-heated up to the temperature of 350 - 400°C and exposure at this temperature for 45 - 60 minutes, further cooling of the mould containing the product and removal from the mould at the following component ratio, wt %: potassium hydroxide 9 - 12, microsilica 20 - 28, hot water 60 - 71. Foamed vermiculite is taken in the amount of 65 - 80% of the binding mixture weight. The method provides for mixing of the binding mixture with foamed vermiculite during 2-3 minutes.EFFECT: reduction of energy consumption at simultaneous improvement of operating characteristics of a heat-insulating product: compressive strength, density, freeze resistance and water resistance.2 cl, 2 tbl
Изобретение относится к области промышленности строительных материалов и может быть использовано при изготовлении теплоизоляционных изделий различной геометрической формы, преимущественно плит. Способ получения теплоизоляционного изделия на основе вермикулита включает получение связующей смеси путем перемешивания гидроксида калия, микрокремнезема и воды, предварительно нагретой до температуры 70 - 85°C, перемешивание связующей смеси со вспученным вермикулитом, размещение полученной сырьевой массы в форму и уплотнение, фиксирование формы плотной крышкой, помещение в печь, предварительно нагретую до температуры 350 - 400°C и выдерживание при этой температуре 45 - 60 мин, последующее охлаждение формы с изделием и распалубку при следующем соотношении компонентов, мас.%: гидроксид калия 9 - 12, микрокремнезем 20 - 28, горячая вода 60 - 71, причем вспученный вермикулит берут в количестве 65 - 80% от массы связующей смеси. Способ предусматривает перемешивание связующей смеси со вспученным вермикулитом в течение 2-3 мин. Технический результат - снижение энергоемкости при одновременном повышении эксплуатационных характеристик теплоизоляционного изделия: прочности на сжатие, плотности, морозостойкости и водостойкости. 1 з.п. ф-лы, 2 табл. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2563263C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2563263C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2563263C13</originalsourceid><addsrcrecordid>eNrjZHD0dQ3x8HdRcPMPUggI8ncJdfb0c1fwcHUM0fX0Cw71cQwB8SEyIQpOjsGuLgr-fgphrkG-ns6hPp4hrjwMrGmJOcWpvFCam0HBzTXE2UM3tSA_PrW4IDE5NS-1JD4o1MjUzNjIzNjZ0JgIJQCXAyrU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING HEAT-INSULATING PRODUCT BASED ON VERMICULITE</title><source>esp@cenet</source><creator>RAKHMANOVA IRINA ANATOL'EVNA ; RJABOV SERGEJ IVANOVICH ; SARKISOV JURIJ SERGEEVICH</creator><creatorcontrib>RAKHMANOVA IRINA ANATOL'EVNA ; RJABOV SERGEJ IVANOVICH ; SARKISOV JURIJ SERGEEVICH</creatorcontrib><description>FIELD: construction.SUBSTANCE: method for producing a heat-insulating product based on vermiculite involves production of a binding mixture by mixing potassium hydroxide, microsilica and water, which is preheated up to the temperature of 70 - 85°C, mixing of the binding mixture with foamed vermiculite, arrangement of the obtained raw mass in a mould and compaction, fixation of the mould by a tight cover, placement into a furnace pre-heated up to the temperature of 350 - 400°C and exposure at this temperature for 45 - 60 minutes, further cooling of the mould containing the product and removal from the mould at the following component ratio, wt %: potassium hydroxide 9 - 12, microsilica 20 - 28, hot water 60 - 71. Foamed vermiculite is taken in the amount of 65 - 80% of the binding mixture weight. The method provides for mixing of the binding mixture with foamed vermiculite during 2-3 minutes.EFFECT: reduction of energy consumption at simultaneous improvement of operating characteristics of a heat-insulating product: compressive strength, density, freeze resistance and water resistance.2 cl, 2 tbl
Изобретение относится к области промышленности строительных материалов и может быть использовано при изготовлении теплоизоляционных изделий различной геометрической формы, преимущественно плит. Способ получения теплоизоляционного изделия на основе вермикулита включает получение связующей смеси путем перемешивания гидроксида калия, микрокремнезема и воды, предварительно нагретой до температуры 70 - 85°C, перемешивание связующей смеси со вспученным вермикулитом, размещение полученной сырьевой массы в форму и уплотнение, фиксирование формы плотной крышкой, помещение в печь, предварительно нагретую до температуры 350 - 400°C и выдерживание при этой температуре 45 - 60 мин, последующее охлаждение формы с изделием и распалубку при следующем соотношении компонентов, мас.%: гидроксид калия 9 - 12, микрокремнезем 20 - 28, горячая вода 60 - 71, причем вспученный вермикулит берут в количестве 65 - 80% от массы связующей смеси. Способ предусматривает перемешивание связующей смеси со вспученным вермикулитом в течение 2-3 мин. Технический результат - снижение энергоемкости при одновременном повышении эксплуатационных характеристик теплоизоляционного изделия: прочности на сжатие, плотности, морозостойкости и водостойкости. 1 з.п. ф-лы, 2 табл.</description><language>eng ; rus</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150920&DB=EPODOC&CC=RU&NR=2563263C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150920&DB=EPODOC&CC=RU&NR=2563263C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>RAKHMANOVA IRINA ANATOL'EVNA</creatorcontrib><creatorcontrib>RJABOV SERGEJ IVANOVICH</creatorcontrib><creatorcontrib>SARKISOV JURIJ SERGEEVICH</creatorcontrib><title>METHOD FOR PRODUCING HEAT-INSULATING PRODUCT BASED ON VERMICULITE</title><description>FIELD: construction.SUBSTANCE: method for producing a heat-insulating product based on vermiculite involves production of a binding mixture by mixing potassium hydroxide, microsilica and water, which is preheated up to the temperature of 70 - 85°C, mixing of the binding mixture with foamed vermiculite, arrangement of the obtained raw mass in a mould and compaction, fixation of the mould by a tight cover, placement into a furnace pre-heated up to the temperature of 350 - 400°C and exposure at this temperature for 45 - 60 minutes, further cooling of the mould containing the product and removal from the mould at the following component ratio, wt %: potassium hydroxide 9 - 12, microsilica 20 - 28, hot water 60 - 71. Foamed vermiculite is taken in the amount of 65 - 80% of the binding mixture weight. The method provides for mixing of the binding mixture with foamed vermiculite during 2-3 minutes.EFFECT: reduction of energy consumption at simultaneous improvement of operating characteristics of a heat-insulating product: compressive strength, density, freeze resistance and water resistance.2 cl, 2 tbl
Изобретение относится к области промышленности строительных материалов и может быть использовано при изготовлении теплоизоляционных изделий различной геометрической формы, преимущественно плит. Способ получения теплоизоляционного изделия на основе вермикулита включает получение связующей смеси путем перемешивания гидроксида калия, микрокремнезема и воды, предварительно нагретой до температуры 70 - 85°C, перемешивание связующей смеси со вспученным вермикулитом, размещение полученной сырьевой массы в форму и уплотнение, фиксирование формы плотной крышкой, помещение в печь, предварительно нагретую до температуры 350 - 400°C и выдерживание при этой температуре 45 - 60 мин, последующее охлаждение формы с изделием и распалубку при следующем соотношении компонентов, мас.%: гидроксид калия 9 - 12, микрокремнезем 20 - 28, горячая вода 60 - 71, причем вспученный вермикулит берут в количестве 65 - 80% от массы связующей смеси. Способ предусматривает перемешивание связующей смеси со вспученным вермикулитом в течение 2-3 мин. Технический результат - снижение энергоемкости при одновременном повышении эксплуатационных характеристик теплоизоляционного изделия: прочности на сжатие, плотности, морозостойкости и водостойкости. 1 з.п. ф-лы, 2 табл.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD0dQ3x8HdRcPMPUggI8ncJdfb0c1fwcHUM0fX0Cw71cQwB8SEyIQpOjsGuLgr-fgphrkG-ns6hPp4hrjwMrGmJOcWpvFCam0HBzTXE2UM3tSA_PrW4IDE5NS-1JD4o1MjUzNjIzNjZ0JgIJQCXAyrU</recordid><startdate>20150920</startdate><enddate>20150920</enddate><creator>RAKHMANOVA IRINA ANATOL'EVNA</creator><creator>RJABOV SERGEJ IVANOVICH</creator><creator>SARKISOV JURIJ SERGEEVICH</creator><scope>EVB</scope></search><sort><creationdate>20150920</creationdate><title>METHOD FOR PRODUCING HEAT-INSULATING PRODUCT BASED ON VERMICULITE</title><author>RAKHMANOVA IRINA ANATOL'EVNA ; RJABOV SERGEJ IVANOVICH ; SARKISOV JURIJ SERGEEVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2563263C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2015</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>RAKHMANOVA IRINA ANATOL'EVNA</creatorcontrib><creatorcontrib>RJABOV SERGEJ IVANOVICH</creatorcontrib><creatorcontrib>SARKISOV JURIJ SERGEEVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>RAKHMANOVA IRINA ANATOL'EVNA</au><au>RJABOV SERGEJ IVANOVICH</au><au>SARKISOV JURIJ SERGEEVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING HEAT-INSULATING PRODUCT BASED ON VERMICULITE</title><date>2015-09-20</date><risdate>2015</risdate><abstract>FIELD: construction.SUBSTANCE: method for producing a heat-insulating product based on vermiculite involves production of a binding mixture by mixing potassium hydroxide, microsilica and water, which is preheated up to the temperature of 70 - 85°C, mixing of the binding mixture with foamed vermiculite, arrangement of the obtained raw mass in a mould and compaction, fixation of the mould by a tight cover, placement into a furnace pre-heated up to the temperature of 350 - 400°C and exposure at this temperature for 45 - 60 minutes, further cooling of the mould containing the product and removal from the mould at the following component ratio, wt %: potassium hydroxide 9 - 12, microsilica 20 - 28, hot water 60 - 71. Foamed vermiculite is taken in the amount of 65 - 80% of the binding mixture weight. The method provides for mixing of the binding mixture with foamed vermiculite during 2-3 minutes.EFFECT: reduction of energy consumption at simultaneous improvement of operating characteristics of a heat-insulating product: compressive strength, density, freeze resistance and water resistance.2 cl, 2 tbl
Изобретение относится к области промышленности строительных материалов и может быть использовано при изготовлении теплоизоляционных изделий различной геометрической формы, преимущественно плит. Способ получения теплоизоляционного изделия на основе вермикулита включает получение связующей смеси путем перемешивания гидроксида калия, микрокремнезема и воды, предварительно нагретой до температуры 70 - 85°C, перемешивание связующей смеси со вспученным вермикулитом, размещение полученной сырьевой массы в форму и уплотнение, фиксирование формы плотной крышкой, помещение в печь, предварительно нагретую до температуры 350 - 400°C и выдерживание при этой температуре 45 - 60 мин, последующее охлаждение формы с изделием и распалубку при следующем соотношении компонентов, мас.%: гидроксид калия 9 - 12, микрокремнезем 20 - 28, горячая вода 60 - 71, причем вспученный вермикулит берут в количестве 65 - 80% от массы связующей смеси. Способ предусматривает перемешивание связующей смеси со вспученным вермикулитом в течение 2-3 мин. Технический результат - снижение энергоемкости при одновременном повышении эксплуатационных характеристик теплоизоляционного изделия: прочности на сжатие, плотности, морозостойкости и водостойкости. 1 з.п. ф-лы, 2 табл.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; rus |
recordid | cdi_epo_espacenet_RU2563263C1 |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
title | METHOD FOR PRODUCING HEAT-INSULATING PRODUCT BASED ON VERMICULITE |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-03T16%3A28%3A12IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=RAKHMANOVA%20IRINA%20ANATOL'EVNA&rft.date=2015-09-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2563263C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |