METHOD TO PREPARE CONCRETE MIX

FIELD: construction.SUBSTANCE: method to prepare concrete mix includes double-stage mixing of a binder, fillers, a superplasticiser and tempering water, at the first stage they first mix the binder, fine filler, 70-80% of coarse filler and 75-85% of tempering water to produce a homogeneous mix, then...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHLJAKHOVA ELENA AL'BERTOVNA, KHOLOSTOVA ALENA IVANOVNA, PITERSKIJ AL'BERT MIKHAJLOVICH, LEZHNEV VADIM NIKOLAEVICH, SHLJAKHOV MIKHAIL ALEKSANDROVICH, KHARITONOV ALEKSANDR ALEKSANDROVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SHLJAKHOVA ELENA AL'BERTOVNA
KHOLOSTOVA ALENA IVANOVNA
PITERSKIJ AL'BERT MIKHAJLOVICH
LEZHNEV VADIM NIKOLAEVICH
SHLJAKHOV MIKHAIL ALEKSANDROVICH
KHARITONOV ALEKSANDR ALEKSANDROVICH
description FIELD: construction.SUBSTANCE: method to prepare concrete mix includes double-stage mixing of a binder, fillers, a superplasticiser and tempering water, at the first stage they first mix the binder, fine filler, 70-80% of coarse filler and 75-85% of tempering water to produce a homogeneous mix, then at the second stage to the previously mixed mixtyre they add the remaining part of the coarse filler, superplasticiser with remaining part of the tempering water, and finally all components are mixed to produce a homogeneous concrete mix of required workability. The superplasticiser is additive of Cemaktiv SU-1.EFFECT: reduced consumption of superplasticiser and provision of the possibility to reduce duration of heat and moisture treatment of concrete.2 cl, 1 tbl Изобретение относится к технологии приготовления строительных смесей, в том числе бетонных смесей с суперпластификаторами для производства сборных бетонных и железобетонных изделий и конструкций. Технический результат заключается в снижении расхода суперпластификатора и обеспечении возможности сокращения длительности тепловлажностной обработки бетона. Способ приготовления бетонной смеси включает двухстадийное перемешивание вяжущего, заполнителей, суперпластификатора и воды затворения, на первой стадии предварительно перемешивают вяжущее, мелкий заполнитель, 70-80% крупного заполнителя и 75-85% воды затворения до получения однородной смеси, затем на второй стадии к предварительно перемешанной смеси добавляют оставшуюся часть крупного заполнителя, суперпластификатор с остальной частью воды затворения и окончательно перемешивают все компоненты до получения однородной бетонной смеси требуемой удобоукладываемости. В качестве суперпластификатора применяется добавка Цемактив СУ-1. 1 з.п. ф-лы, 1 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2548263C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2548263C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2548263C13</originalsourceid><addsrcrecordid>eNrjZJDzdQ3x8HdRCPFXCAhyDXAMclVw9vdzDnINcVXw9YzgYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxQaFGpiYWRmbGzobGRCgBAG19IQU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD TO PREPARE CONCRETE MIX</title><source>esp@cenet</source><creator>SHLJAKHOVA ELENA AL'BERTOVNA ; KHOLOSTOVA ALENA IVANOVNA ; PITERSKIJ AL'BERT MIKHAJLOVICH ; LEZHNEV VADIM NIKOLAEVICH ; SHLJAKHOV MIKHAIL ALEKSANDROVICH ; KHARITONOV ALEKSANDR ALEKSANDROVICH</creator><creatorcontrib>SHLJAKHOVA ELENA AL'BERTOVNA ; KHOLOSTOVA ALENA IVANOVNA ; PITERSKIJ AL'BERT MIKHAJLOVICH ; LEZHNEV VADIM NIKOLAEVICH ; SHLJAKHOV MIKHAIL ALEKSANDROVICH ; KHARITONOV ALEKSANDR ALEKSANDROVICH</creatorcontrib><description>FIELD: construction.SUBSTANCE: method to prepare concrete mix includes double-stage mixing of a binder, fillers, a superplasticiser and tempering water, at the first stage they first mix the binder, fine filler, 70-80% of coarse filler and 75-85% of tempering water to produce a homogeneous mix, then at the second stage to the previously mixed mixtyre they add the remaining part of the coarse filler, superplasticiser with remaining part of the tempering water, and finally all components are mixed to produce a homogeneous concrete mix of required workability. The superplasticiser is additive of Cemaktiv SU-1.EFFECT: reduced consumption of superplasticiser and provision of the possibility to reduce duration of heat and moisture treatment of concrete.2 cl, 1 tbl Изобретение относится к технологии приготовления строительных смесей, в том числе бетонных смесей с суперпластификаторами для производства сборных бетонных и железобетонных изделий и конструкций. Технический результат заключается в снижении расхода суперпластификатора и обеспечении возможности сокращения длительности тепловлажностной обработки бетона. Способ приготовления бетонной смеси включает двухстадийное перемешивание вяжущего, заполнителей, суперпластификатора и воды затворения, на первой стадии предварительно перемешивают вяжущее, мелкий заполнитель, 70-80% крупного заполнителя и 75-85% воды затворения до получения однородной смеси, затем на второй стадии к предварительно перемешанной смеси добавляют оставшуюся часть крупного заполнителя, суперпластификатор с остальной частью воды затворения и окончательно перемешивают все компоненты до получения однородной бетонной смеси требуемой удобоукладываемости. В качестве суперпластификатора применяется добавка Цемактив СУ-1. 1 з.п. ф-лы, 1 табл.</description><language>eng ; rus</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150420&amp;DB=EPODOC&amp;CC=RU&amp;NR=2548263C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150420&amp;DB=EPODOC&amp;CC=RU&amp;NR=2548263C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SHLJAKHOVA ELENA AL'BERTOVNA</creatorcontrib><creatorcontrib>KHOLOSTOVA ALENA IVANOVNA</creatorcontrib><creatorcontrib>PITERSKIJ AL'BERT MIKHAJLOVICH</creatorcontrib><creatorcontrib>LEZHNEV VADIM NIKOLAEVICH</creatorcontrib><creatorcontrib>SHLJAKHOV MIKHAIL ALEKSANDROVICH</creatorcontrib><creatorcontrib>KHARITONOV ALEKSANDR ALEKSANDROVICH</creatorcontrib><title>METHOD TO PREPARE CONCRETE MIX</title><description>FIELD: construction.SUBSTANCE: method to prepare concrete mix includes double-stage mixing of a binder, fillers, a superplasticiser and tempering water, at the first stage they first mix the binder, fine filler, 70-80% of coarse filler and 75-85% of tempering water to produce a homogeneous mix, then at the second stage to the previously mixed mixtyre they add the remaining part of the coarse filler, superplasticiser with remaining part of the tempering water, and finally all components are mixed to produce a homogeneous concrete mix of required workability. The superplasticiser is additive of Cemaktiv SU-1.EFFECT: reduced consumption of superplasticiser and provision of the possibility to reduce duration of heat and moisture treatment of concrete.2 cl, 1 tbl Изобретение относится к технологии приготовления строительных смесей, в том числе бетонных смесей с суперпластификаторами для производства сборных бетонных и железобетонных изделий и конструкций. Технический результат заключается в снижении расхода суперпластификатора и обеспечении возможности сокращения длительности тепловлажностной обработки бетона. Способ приготовления бетонной смеси включает двухстадийное перемешивание вяжущего, заполнителей, суперпластификатора и воды затворения, на первой стадии предварительно перемешивают вяжущее, мелкий заполнитель, 70-80% крупного заполнителя и 75-85% воды затворения до получения однородной смеси, затем на второй стадии к предварительно перемешанной смеси добавляют оставшуюся часть крупного заполнителя, суперпластификатор с остальной частью воды затворения и окончательно перемешивают все компоненты до получения однородной бетонной смеси требуемой удобоукладываемости. В качестве суперпластификатора применяется добавка Цемактив СУ-1. 1 з.п. ф-лы, 1 табл.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJDzdQ3x8HdRCPFXCAhyDXAMclVw9vdzDnINcVXw9YzgYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxQaFGpiYWRmbGzobGRCgBAG19IQU</recordid><startdate>20150420</startdate><enddate>20150420</enddate><creator>SHLJAKHOVA ELENA AL'BERTOVNA</creator><creator>KHOLOSTOVA ALENA IVANOVNA</creator><creator>PITERSKIJ AL'BERT MIKHAJLOVICH</creator><creator>LEZHNEV VADIM NIKOLAEVICH</creator><creator>SHLJAKHOV MIKHAIL ALEKSANDROVICH</creator><creator>KHARITONOV ALEKSANDR ALEKSANDROVICH</creator><scope>EVB</scope></search><sort><creationdate>20150420</creationdate><title>METHOD TO PREPARE CONCRETE MIX</title><author>SHLJAKHOVA ELENA AL'BERTOVNA ; KHOLOSTOVA ALENA IVANOVNA ; PITERSKIJ AL'BERT MIKHAJLOVICH ; LEZHNEV VADIM NIKOLAEVICH ; SHLJAKHOV MIKHAIL ALEKSANDROVICH ; KHARITONOV ALEKSANDR ALEKSANDROVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2548263C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2015</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>SHLJAKHOVA ELENA AL'BERTOVNA</creatorcontrib><creatorcontrib>KHOLOSTOVA ALENA IVANOVNA</creatorcontrib><creatorcontrib>PITERSKIJ AL'BERT MIKHAJLOVICH</creatorcontrib><creatorcontrib>LEZHNEV VADIM NIKOLAEVICH</creatorcontrib><creatorcontrib>SHLJAKHOV MIKHAIL ALEKSANDROVICH</creatorcontrib><creatorcontrib>KHARITONOV ALEKSANDR ALEKSANDROVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SHLJAKHOVA ELENA AL'BERTOVNA</au><au>KHOLOSTOVA ALENA IVANOVNA</au><au>PITERSKIJ AL'BERT MIKHAJLOVICH</au><au>LEZHNEV VADIM NIKOLAEVICH</au><au>SHLJAKHOV MIKHAIL ALEKSANDROVICH</au><au>KHARITONOV ALEKSANDR ALEKSANDROVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD TO PREPARE CONCRETE MIX</title><date>2015-04-20</date><risdate>2015</risdate><abstract>FIELD: construction.SUBSTANCE: method to prepare concrete mix includes double-stage mixing of a binder, fillers, a superplasticiser and tempering water, at the first stage they first mix the binder, fine filler, 70-80% of coarse filler and 75-85% of tempering water to produce a homogeneous mix, then at the second stage to the previously mixed mixtyre they add the remaining part of the coarse filler, superplasticiser with remaining part of the tempering water, and finally all components are mixed to produce a homogeneous concrete mix of required workability. The superplasticiser is additive of Cemaktiv SU-1.EFFECT: reduced consumption of superplasticiser and provision of the possibility to reduce duration of heat and moisture treatment of concrete.2 cl, 1 tbl Изобретение относится к технологии приготовления строительных смесей, в том числе бетонных смесей с суперпластификаторами для производства сборных бетонных и железобетонных изделий и конструкций. Технический результат заключается в снижении расхода суперпластификатора и обеспечении возможности сокращения длительности тепловлажностной обработки бетона. Способ приготовления бетонной смеси включает двухстадийное перемешивание вяжущего, заполнителей, суперпластификатора и воды затворения, на первой стадии предварительно перемешивают вяжущее, мелкий заполнитель, 70-80% крупного заполнителя и 75-85% воды затворения до получения однородной смеси, затем на второй стадии к предварительно перемешанной смеси добавляют оставшуюся часть крупного заполнителя, суперпластификатор с остальной частью воды затворения и окончательно перемешивают все компоненты до получения однородной бетонной смеси требуемой удобоукладываемости. В качестве суперпластификатора применяется добавка Цемактив СУ-1. 1 з.п. ф-лы, 1 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2548263C1
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title METHOD TO PREPARE CONCRETE MIX
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T10%3A23%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SHLJAKHOVA%20ELENA%20AL'BERTOVNA&rft.date=2015-04-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2548263C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true