METHOD OF MAGNETOCONDUCTIVE CASING REPAIR

FIELD: machine building.SUBSTANCE: method of magnetoconductive casing repair implies forming of compaction on damaged area made from ferromagnetic adhesive composition applying this composition on a patch piece, placement of the patch piece with this composition on casing damaged area, action on the...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: STAROVOJTOV VIKTOR SEMENOVICH, DEMJANENKO NIKOLAJ ALEKSANDROVICH, GALAJ MIKHAIL IVANOVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator STAROVOJTOV VIKTOR SEMENOVICH
DEMJANENKO NIKOLAJ ALEKSANDROVICH
GALAJ MIKHAIL IVANOVICH
description FIELD: machine building.SUBSTANCE: method of magnetoconductive casing repair implies forming of compaction on damaged area made from ferromagnetic adhesive composition applying this composition on a patch piece, placement of the patch piece with this composition on casing damaged area, action on the composition through the patch piece by continuous magnetic field generated by external source of magnetic field, and removal of external source of magnetic field after composition curing. As a patch piece non-magnetoconductive layered elastic flexible plate is used, one of outer layers of which is made from elastic mechanically strong material, non-permeable for adhesive composition, and the other outer layer is made from flexible material. Adhesive composition is applied on non-permeable for it outer layer of plate.EFFECT: enlarging area of application, reducing labour intensity and time consumption for repair, improving reliability and quality of repaired casing sealing, improving efficiency of magnets use.3 dwg Изобретение относится к строительству и может быть использовано для ликвидации негерметичностей в виде течей, свищей, отверстий, трещин, пробоин магнитопроводных оболочек трубопроводов, емкостей, резервуаров, сосудов, корпусов судов и других аналогичных объектов и коммуникаций, находящихся под действием избыточного давления жидкости или газа. Способ ремонта магнитопроводной оболочки включает создание на поврежденном участке уплотнения из ферромагнитной клеевой композиции путем нанесения этой композиции на заплату, установки заплаты с указанной композицией на участок повреждения оболочки, воздействия на композицию через заплату постоянным магнитным полем, создаваемым внешним источником магнитного поля, и удаления внешнего источника магнитного поля после отверждения композиции. В качестве заплаты используют немагнитопроводную слоистую упругоэластичную пластину, один из внешних слоев которой выполнен из эластичного механически прочного материала, непроницаемого для клеевой композиции, а другой внешний слой - из упругого материала. Клеевую композицию наносят на непроницаемый для нее внешний слой пластины. Технический результат: расширение области применения, снижение трудоемкости и затрат времени на проведение ремонта, повышение надежности и качества герметизации ремонтируемых оболочек, повышение эффективности использования магнитов. 3 ил.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2499945C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2499945C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2499945C23</originalsourceid><addsrcrecordid>eNrjZND0dQ3x8HdR8HdT8HV093MN8Xf293MJdQ7xDHNVcHYM9vRzVwhyDXD0DOJhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoUYmlpaWJqbORsZEKAEA7x0kQw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF MAGNETOCONDUCTIVE CASING REPAIR</title><source>esp@cenet</source><creator>STAROVOJTOV VIKTOR SEMENOVICH ; DEMJANENKO NIKOLAJ ALEKSANDROVICH ; GALAJ MIKHAIL IVANOVICH</creator><creatorcontrib>STAROVOJTOV VIKTOR SEMENOVICH ; DEMJANENKO NIKOLAJ ALEKSANDROVICH ; GALAJ MIKHAIL IVANOVICH</creatorcontrib><description>FIELD: machine building.SUBSTANCE: method of magnetoconductive casing repair implies forming of compaction on damaged area made from ferromagnetic adhesive composition applying this composition on a patch piece, placement of the patch piece with this composition on casing damaged area, action on the composition through the patch piece by continuous magnetic field generated by external source of magnetic field, and removal of external source of magnetic field after composition curing. As a patch piece non-magnetoconductive layered elastic flexible plate is used, one of outer layers of which is made from elastic mechanically strong material, non-permeable for adhesive composition, and the other outer layer is made from flexible material. Adhesive composition is applied on non-permeable for it outer layer of plate.EFFECT: enlarging area of application, reducing labour intensity and time consumption for repair, improving reliability and quality of repaired casing sealing, improving efficiency of magnets use.3 dwg Изобретение относится к строительству и может быть использовано для ликвидации негерметичностей в виде течей, свищей, отверстий, трещин, пробоин магнитопроводных оболочек трубопроводов, емкостей, резервуаров, сосудов, корпусов судов и других аналогичных объектов и коммуникаций, находящихся под действием избыточного давления жидкости или газа. Способ ремонта магнитопроводной оболочки включает создание на поврежденном участке уплотнения из ферромагнитной клеевой композиции путем нанесения этой композиции на заплату, установки заплаты с указанной композицией на участок повреждения оболочки, воздействия на композицию через заплату постоянным магнитным полем, создаваемым внешним источником магнитного поля, и удаления внешнего источника магнитного поля после отверждения композиции. В качестве заплаты используют немагнитопроводную слоистую упругоэластичную пластину, один из внешних слоев которой выполнен из эластичного механически прочного материала, непроницаемого для клеевой композиции, а другой внешний слой - из упругого материала. Клеевую композицию наносят на непроницаемый для нее внешний слой пластины. Технический результат: расширение области применения, снижение трудоемкости и затрат времени на проведение ремонта, повышение надежности и качества герметизации ремонтируемых оболочек, повышение эффективности использования магнитов. 3 ил.</description><language>eng ; rus</language><subject>BLASTING ; ENGINEERING ELEMENTS AND UNITS ; GENERAL MEASURES FOR PRODUCING AND MAINTAINING EFFECTIVEFUNCTIONING OF MACHINES OR INSTALLATIONS ; HEATING ; JOINTS OR FITTINGS FOR PIPES ; LIGHTING ; MEANS FOR THERMAL INSULATION IN GENERAL ; MECHANICAL ENGINEERING ; PIPES ; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING ; THERMAL INSULATION IN GENERAL ; WEAPONS</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20131127&amp;DB=EPODOC&amp;CC=RU&amp;NR=2499945C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20131127&amp;DB=EPODOC&amp;CC=RU&amp;NR=2499945C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>STAROVOJTOV VIKTOR SEMENOVICH</creatorcontrib><creatorcontrib>DEMJANENKO NIKOLAJ ALEKSANDROVICH</creatorcontrib><creatorcontrib>GALAJ MIKHAIL IVANOVICH</creatorcontrib><title>METHOD OF MAGNETOCONDUCTIVE CASING REPAIR</title><description>FIELD: machine building.SUBSTANCE: method of magnetoconductive casing repair implies forming of compaction on damaged area made from ferromagnetic adhesive composition applying this composition on a patch piece, placement of the patch piece with this composition on casing damaged area, action on the composition through the patch piece by continuous magnetic field generated by external source of magnetic field, and removal of external source of magnetic field after composition curing. As a patch piece non-magnetoconductive layered elastic flexible plate is used, one of outer layers of which is made from elastic mechanically strong material, non-permeable for adhesive composition, and the other outer layer is made from flexible material. Adhesive composition is applied on non-permeable for it outer layer of plate.EFFECT: enlarging area of application, reducing labour intensity and time consumption for repair, improving reliability and quality of repaired casing sealing, improving efficiency of magnets use.3 dwg Изобретение относится к строительству и может быть использовано для ликвидации негерметичностей в виде течей, свищей, отверстий, трещин, пробоин магнитопроводных оболочек трубопроводов, емкостей, резервуаров, сосудов, корпусов судов и других аналогичных объектов и коммуникаций, находящихся под действием избыточного давления жидкости или газа. Способ ремонта магнитопроводной оболочки включает создание на поврежденном участке уплотнения из ферромагнитной клеевой композиции путем нанесения этой композиции на заплату, установки заплаты с указанной композицией на участок повреждения оболочки, воздействия на композицию через заплату постоянным магнитным полем, создаваемым внешним источником магнитного поля, и удаления внешнего источника магнитного поля после отверждения композиции. В качестве заплаты используют немагнитопроводную слоистую упругоэластичную пластину, один из внешних слоев которой выполнен из эластичного механически прочного материала, непроницаемого для клеевой композиции, а другой внешний слой - из упругого материала. Клеевую композицию наносят на непроницаемый для нее внешний слой пластины. Технический результат: расширение области применения, снижение трудоемкости и затрат времени на проведение ремонта, повышение надежности и качества герметизации ремонтируемых оболочек, повышение эффективности использования магнитов. 3 ил.</description><subject>BLASTING</subject><subject>ENGINEERING ELEMENTS AND UNITS</subject><subject>GENERAL MEASURES FOR PRODUCING AND MAINTAINING EFFECTIVEFUNCTIONING OF MACHINES OR INSTALLATIONS</subject><subject>HEATING</subject><subject>JOINTS OR FITTINGS FOR PIPES</subject><subject>LIGHTING</subject><subject>MEANS FOR THERMAL INSULATION IN GENERAL</subject><subject>MECHANICAL ENGINEERING</subject><subject>PIPES</subject><subject>SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING</subject><subject>THERMAL INSULATION IN GENERAL</subject><subject>WEAPONS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND0dQ3x8HdR8HdT8HV093MN8Xf293MJdQ7xDHNVcHYM9vRzVwhyDXD0DOJhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoUYmlpaWJqbORsZEKAEA7x0kQw</recordid><startdate>20131127</startdate><enddate>20131127</enddate><creator>STAROVOJTOV VIKTOR SEMENOVICH</creator><creator>DEMJANENKO NIKOLAJ ALEKSANDROVICH</creator><creator>GALAJ MIKHAIL IVANOVICH</creator><scope>EVB</scope></search><sort><creationdate>20131127</creationdate><title>METHOD OF MAGNETOCONDUCTIVE CASING REPAIR</title><author>STAROVOJTOV VIKTOR SEMENOVICH ; DEMJANENKO NIKOLAJ ALEKSANDROVICH ; GALAJ MIKHAIL IVANOVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2499945C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2013</creationdate><topic>BLASTING</topic><topic>ENGINEERING ELEMENTS AND UNITS</topic><topic>GENERAL MEASURES FOR PRODUCING AND MAINTAINING EFFECTIVEFUNCTIONING OF MACHINES OR INSTALLATIONS</topic><topic>HEATING</topic><topic>JOINTS OR FITTINGS FOR PIPES</topic><topic>LIGHTING</topic><topic>MEANS FOR THERMAL INSULATION IN GENERAL</topic><topic>MECHANICAL ENGINEERING</topic><topic>PIPES</topic><topic>SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING</topic><topic>THERMAL INSULATION IN GENERAL</topic><topic>WEAPONS</topic><toplevel>online_resources</toplevel><creatorcontrib>STAROVOJTOV VIKTOR SEMENOVICH</creatorcontrib><creatorcontrib>DEMJANENKO NIKOLAJ ALEKSANDROVICH</creatorcontrib><creatorcontrib>GALAJ MIKHAIL IVANOVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>STAROVOJTOV VIKTOR SEMENOVICH</au><au>DEMJANENKO NIKOLAJ ALEKSANDROVICH</au><au>GALAJ MIKHAIL IVANOVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF MAGNETOCONDUCTIVE CASING REPAIR</title><date>2013-11-27</date><risdate>2013</risdate><abstract>FIELD: machine building.SUBSTANCE: method of magnetoconductive casing repair implies forming of compaction on damaged area made from ferromagnetic adhesive composition applying this composition on a patch piece, placement of the patch piece with this composition on casing damaged area, action on the composition through the patch piece by continuous magnetic field generated by external source of magnetic field, and removal of external source of magnetic field after composition curing. As a patch piece non-magnetoconductive layered elastic flexible plate is used, one of outer layers of which is made from elastic mechanically strong material, non-permeable for adhesive composition, and the other outer layer is made from flexible material. Adhesive composition is applied on non-permeable for it outer layer of plate.EFFECT: enlarging area of application, reducing labour intensity and time consumption for repair, improving reliability and quality of repaired casing sealing, improving efficiency of magnets use.3 dwg Изобретение относится к строительству и может быть использовано для ликвидации негерметичностей в виде течей, свищей, отверстий, трещин, пробоин магнитопроводных оболочек трубопроводов, емкостей, резервуаров, сосудов, корпусов судов и других аналогичных объектов и коммуникаций, находящихся под действием избыточного давления жидкости или газа. Способ ремонта магнитопроводной оболочки включает создание на поврежденном участке уплотнения из ферромагнитной клеевой композиции путем нанесения этой композиции на заплату, установки заплаты с указанной композицией на участок повреждения оболочки, воздействия на композицию через заплату постоянным магнитным полем, создаваемым внешним источником магнитного поля, и удаления внешнего источника магнитного поля после отверждения композиции. В качестве заплаты используют немагнитопроводную слоистую упругоэластичную пластину, один из внешних слоев которой выполнен из эластичного механически прочного материала, непроницаемого для клеевой композиции, а другой внешний слой - из упругого материала. Клеевую композицию наносят на непроницаемый для нее внешний слой пластины. Технический результат: расширение области применения, снижение трудоемкости и затрат времени на проведение ремонта, повышение надежности и качества герметизации ремонтируемых оболочек, повышение эффективности использования магнитов. 3 ил.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2499945C2
source esp@cenet
subjects BLASTING
ENGINEERING ELEMENTS AND UNITS
GENERAL MEASURES FOR PRODUCING AND MAINTAINING EFFECTIVEFUNCTIONING OF MACHINES OR INSTALLATIONS
HEATING
JOINTS OR FITTINGS FOR PIPES
LIGHTING
MEANS FOR THERMAL INSULATION IN GENERAL
MECHANICAL ENGINEERING
PIPES
SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING
THERMAL INSULATION IN GENERAL
WEAPONS
title METHOD OF MAGNETOCONDUCTIVE CASING REPAIR
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-25T03%3A20%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=STAROVOJTOV%20VIKTOR%20SEMENOVICH&rft.date=2013-11-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2499945C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true