METHOD OF BONDERISING THREAD AND SEALING TAPER BORES OF COUPLINGS AND METALLIC SAFEGUARDS OF OIL COUNTRY TUBULAR GOODS
FIELD: metallurgy.SUBSTANCE: proposed method comprises degreasing, flushing in cold and hot water, bonderising and impregnation. Note here that degreasing is carried out in solution of BOK-6 detergent at 40-50°C, detergent content making 20-40 g/l.EFFECT: dense homogeneous fine crystalline coating,...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FIELD: metallurgy.SUBSTANCE: proposed method comprises degreasing, flushing in cold and hot water, bonderising and impregnation. Note here that degreasing is carried out in solution of BOK-6 detergent at 40-50°C, detergent content making 20-40 g/l.EFFECT: dense homogeneous fine crystalline coating, higher strength, longer life.
Изобретение относится к трубному производству и может быть использовано для фосфатирования резьбы и уплотнительных конических расточек муфт и металлических предохранительных деталей труб нефтяного сортамента, в частности насосно-компрессорных и обсадных труб. Способ включает операцию обезжиривания, промывки в горячей и холодной воде, фосфатирования и пропитки. При этом операцию обезжиривания проводят в растворе моющего средства БОК-6 при его содержании 20-40 г/л и температуре 40-50°С. Обеспечивается получение плотного, однородного, мелкокристаллического слоя фосфатного покрытия, исключающего искажение геометрических размеров резьбы и обеспечивающего увеличение количества операций свинчивания-развинчивания муфтового соединения без нарушения целостности слоя покрытия. |
---|