METHOD OF OBTAINING BARIUM ALUMINATES

FIELD: chemistry. ^ SUBSTANCE: barium aluminates are obtained from aluminium oxide or hydroxide and barium oxide or hydroxide, which are sintered at 700-900C for 4-8 hours. ^ EFFECT: barium aluminates, obtained by claimed method, meet all requirements, made for initial products for manufacturing the...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ISKHAKOVA LJUDMILA DMITRIEVNA, KUDRJAVTSEVA ELENA PAVLOVNA, SANDU ROMAN ALEKSANDROVICH, KISELEVA LARISA VITAL'EVNA, EMEL'JANOVA OL'GA NIKOLAEVNA
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: chemistry. ^ SUBSTANCE: barium aluminates are obtained from aluminium oxide or hydroxide and barium oxide or hydroxide, which are sintered at 700-900C for 4-8 hours. ^ EFFECT: barium aluminates, obtained by claimed method, meet all requirements, made for initial products for manufacturing thermoregulating coatings, applied in manufacturing space vehicles. ^ 2 dwg, 5 ex Изобретение относится к области химии. Алюминаты бария получают из оксида или гидроксида алюминия и оксида бария или гидроксида бария, которые спекают при 700-900°С в течение 4-8 часов. Алюминаты бария, полученные данным способом, соответствуют всем требованиям, предъявляемым к исходным продуктам для изготовления терморегулирующих покрытий, применяемых при изготовлении космических аппаратов. 2 ил., 5 пр.