BIMETALLIC CONTACT CORROSION SENSOR
FIELD: chemistry. ^ SUBSTANCE: bimetallic contact corrosion sensor consists of a piece of steel pipe 1 with a calibrated wall thickness. Copper covers/plugs 2 are attached to the ends of the piece of steel pipe 1 by a copper pin 3 through airtight dielectric spacers 4, and moisture-absorbing materia...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | SHESTERIKOV GENNADIJ PETROVICH SHESTERIKOV ANDREJ GENNAD'EVICH LUBENTSOV NIKOLAJ VALER'EVICH ASTANIN ALEKSANDR JUR'EVICH |
description | FIELD: chemistry. ^ SUBSTANCE: bimetallic contact corrosion sensor consists of a piece of steel pipe 1 with a calibrated wall thickness. Copper covers/plugs 2 are attached to the ends of the piece of steel pipe 1 by a copper pin 3 through airtight dielectric spacers 4, and moisture-absorbing material 5, saturated with a salt solution and dried, is laid on the inner surface of the piece of steel pipe 1. A contact electrode 6 made from metal foil is then laid onto the moisture-absorbing material 5, and the cavity 10 of the bimetallic contact corrosion sensor is filled with any dielectric material, e.g., sand. Measuring conductors 8 and 9 are led from the inner surface of the piece of steel pipe 1, measuring conductors 10 and 11 are led from the inner surface of the copper covers/plugs 2, and a measuring conductor 12 is led from the contact electrode 6 made from metal foil. The piece of steel pipe 1 is the housing, detecting element and contact electrode at the same time, and the copper covers/plugs 2, together with the piece of steel pipe 1, form a steel-copper corrosion galvanic couple. ^ EFFECT: determining contact corrosion current and accurate rapid evaluation of cathode protection. ^ 2 cl, 7 dwg
Изобретение относится к технике коррозионного мониторинга подземных трубопроводов, в частности к биметаллическим датчикам контактной коррозии, и может быть использовано в газовой, нефтяной и смежных отраслях промышленности. Биметаллический датчик контактной коррозии состоит из отрезка стальной трубы 1 с калиброванной толщиной стенки. При этом на торцы отрезка стальной трубы 1 закреплены медные крышки - заглушки 2 с помощью медной шпильки 3 через герметичные диэлектрические прокладки 4, а на внутреннюю поверхность отрезка стальной трубы 1 накладывают влагопоглощающий материал 5, пропитанный солевым раствором и высушенный. Затем на влагопоглощающий материал 5 накладывают контактный электрод 6 из металлической фольги, а полость 10 биметаллического датчика контактной коррозии заполняют любым диэлектрическим материалом, например песком. При этом от внутренней поверхности отрезка стальной трубы 1 выводят измерительные проводники 8 и 9, от внутренней поверхности медных крышек-заглушек 2 выводят измерительные проводники 10 и 11, а от контактного электрода 6 из металлической фольги выводят измерительный проводник 12. При этом отрезок стальной трубы 1 является одновременно корпусом, чувствительным элементом и контактным электродом, а медные крышки-заглушки 2 с отрезком ст |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2463576C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2463576C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2463576C13</originalsourceid><addsrcrecordid>eNrjZFB28vR1DXH08fF0VnD29wtxdA4B0kFB_sGe_n4Kwa5-wf5BPAysaYk5xam8UJqbQcHNNcTZQze1ID8-tbggMTk1L7UkPijUyMTM2NTczNnQmAglAC6sIrY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>BIMETALLIC CONTACT CORROSION SENSOR</title><source>esp@cenet</source><creator>SHESTERIKOV GENNADIJ PETROVICH ; SHESTERIKOV ANDREJ GENNAD'EVICH ; LUBENTSOV NIKOLAJ VALER'EVICH ; ASTANIN ALEKSANDR JUR'EVICH</creator><creatorcontrib>SHESTERIKOV GENNADIJ PETROVICH ; SHESTERIKOV ANDREJ GENNAD'EVICH ; LUBENTSOV NIKOLAJ VALER'EVICH ; ASTANIN ALEKSANDR JUR'EVICH</creatorcontrib><description>FIELD: chemistry. ^ SUBSTANCE: bimetallic contact corrosion sensor consists of a piece of steel pipe 1 with a calibrated wall thickness. Copper covers/plugs 2 are attached to the ends of the piece of steel pipe 1 by a copper pin 3 through airtight dielectric spacers 4, and moisture-absorbing material 5, saturated with a salt solution and dried, is laid on the inner surface of the piece of steel pipe 1. A contact electrode 6 made from metal foil is then laid onto the moisture-absorbing material 5, and the cavity 10 of the bimetallic contact corrosion sensor is filled with any dielectric material, e.g., sand. Measuring conductors 8 and 9 are led from the inner surface of the piece of steel pipe 1, measuring conductors 10 and 11 are led from the inner surface of the copper covers/plugs 2, and a measuring conductor 12 is led from the contact electrode 6 made from metal foil. The piece of steel pipe 1 is the housing, detecting element and contact electrode at the same time, and the copper covers/plugs 2, together with the piece of steel pipe 1, form a steel-copper corrosion galvanic couple. ^ EFFECT: determining contact corrosion current and accurate rapid evaluation of cathode protection. ^ 2 cl, 7 dwg
Изобретение относится к технике коррозионного мониторинга подземных трубопроводов, в частности к биметаллическим датчикам контактной коррозии, и может быть использовано в газовой, нефтяной и смежных отраслях промышленности. Биметаллический датчик контактной коррозии состоит из отрезка стальной трубы 1 с калиброванной толщиной стенки. При этом на торцы отрезка стальной трубы 1 закреплены медные крышки - заглушки 2 с помощью медной шпильки 3 через герметичные диэлектрические прокладки 4, а на внутреннюю поверхность отрезка стальной трубы 1 накладывают влагопоглощающий материал 5, пропитанный солевым раствором и высушенный. Затем на влагопоглощающий материал 5 накладывают контактный электрод 6 из металлической фольги, а полость 10 биметаллического датчика контактной коррозии заполняют любым диэлектрическим материалом, например песком. При этом от внутренней поверхности отрезка стальной трубы 1 выводят измерительные проводники 8 и 9, от внутренней поверхности медных крышек-заглушек 2 выводят измерительные проводники 10 и 11, а от контактного электрода 6 из металлической фольги выводят измерительный проводник 12. При этом отрезок стальной трубы 1 является одновременно корпусом, чувствительным элементом и контактным электродом, а медные крышки-заглушки 2 с отрезком стальной трубы 1 образуют коррозионную гальванопару сталь - медь. Техническим результатом изобретения является определение коррозионного тока контактной коррозии и точной экспресс-оценки полноты катодной защиты. 1 з.п. ф-лы, 7 ил.</description><language>eng ; rus</language><subject>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES ; MEASURING ; PHYSICS ; TESTING</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20121010&DB=EPODOC&CC=RU&NR=2463576C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20121010&DB=EPODOC&CC=RU&NR=2463576C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SHESTERIKOV GENNADIJ PETROVICH</creatorcontrib><creatorcontrib>SHESTERIKOV ANDREJ GENNAD'EVICH</creatorcontrib><creatorcontrib>LUBENTSOV NIKOLAJ VALER'EVICH</creatorcontrib><creatorcontrib>ASTANIN ALEKSANDR JUR'EVICH</creatorcontrib><title>BIMETALLIC CONTACT CORROSION SENSOR</title><description>FIELD: chemistry. ^ SUBSTANCE: bimetallic contact corrosion sensor consists of a piece of steel pipe 1 with a calibrated wall thickness. Copper covers/plugs 2 are attached to the ends of the piece of steel pipe 1 by a copper pin 3 through airtight dielectric spacers 4, and moisture-absorbing material 5, saturated with a salt solution and dried, is laid on the inner surface of the piece of steel pipe 1. A contact electrode 6 made from metal foil is then laid onto the moisture-absorbing material 5, and the cavity 10 of the bimetallic contact corrosion sensor is filled with any dielectric material, e.g., sand. Measuring conductors 8 and 9 are led from the inner surface of the piece of steel pipe 1, measuring conductors 10 and 11 are led from the inner surface of the copper covers/plugs 2, and a measuring conductor 12 is led from the contact electrode 6 made from metal foil. The piece of steel pipe 1 is the housing, detecting element and contact electrode at the same time, and the copper covers/plugs 2, together with the piece of steel pipe 1, form a steel-copper corrosion galvanic couple. ^ EFFECT: determining contact corrosion current and accurate rapid evaluation of cathode protection. ^ 2 cl, 7 dwg
Изобретение относится к технике коррозионного мониторинга подземных трубопроводов, в частности к биметаллическим датчикам контактной коррозии, и может быть использовано в газовой, нефтяной и смежных отраслях промышленности. Биметаллический датчик контактной коррозии состоит из отрезка стальной трубы 1 с калиброванной толщиной стенки. При этом на торцы отрезка стальной трубы 1 закреплены медные крышки - заглушки 2 с помощью медной шпильки 3 через герметичные диэлектрические прокладки 4, а на внутреннюю поверхность отрезка стальной трубы 1 накладывают влагопоглощающий материал 5, пропитанный солевым раствором и высушенный. Затем на влагопоглощающий материал 5 накладывают контактный электрод 6 из металлической фольги, а полость 10 биметаллического датчика контактной коррозии заполняют любым диэлектрическим материалом, например песком. При этом от внутренней поверхности отрезка стальной трубы 1 выводят измерительные проводники 8 и 9, от внутренней поверхности медных крышек-заглушек 2 выводят измерительные проводники 10 и 11, а от контактного электрода 6 из металлической фольги выводят измерительный проводник 12. При этом отрезок стальной трубы 1 является одновременно корпусом, чувствительным элементом и контактным электродом, а медные крышки-заглушки 2 с отрезком стальной трубы 1 образуют коррозионную гальванопару сталь - медь. Техническим результатом изобретения является определение коррозионного тока контактной коррозии и точной экспресс-оценки полноты катодной защиты. 1 з.п. ф-лы, 7 ил.</description><subject>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES</subject><subject>MEASURING</subject><subject>PHYSICS</subject><subject>TESTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFB28vR1DXH08fF0VnD29wtxdA4B0kFB_sGe_n4Kwa5-wf5BPAysaYk5xam8UJqbQcHNNcTZQze1ID8-tbggMTk1L7UkPijUyMTM2NTczNnQmAglAC6sIrY</recordid><startdate>20121010</startdate><enddate>20121010</enddate><creator>SHESTERIKOV GENNADIJ PETROVICH</creator><creator>SHESTERIKOV ANDREJ GENNAD'EVICH</creator><creator>LUBENTSOV NIKOLAJ VALER'EVICH</creator><creator>ASTANIN ALEKSANDR JUR'EVICH</creator><scope>EVB</scope></search><sort><creationdate>20121010</creationdate><title>BIMETALLIC CONTACT CORROSION SENSOR</title><author>SHESTERIKOV GENNADIJ PETROVICH ; SHESTERIKOV ANDREJ GENNAD'EVICH ; LUBENTSOV NIKOLAJ VALER'EVICH ; ASTANIN ALEKSANDR JUR'EVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2463576C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2012</creationdate><topic>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES</topic><topic>MEASURING</topic><topic>PHYSICS</topic><topic>TESTING</topic><toplevel>online_resources</toplevel><creatorcontrib>SHESTERIKOV GENNADIJ PETROVICH</creatorcontrib><creatorcontrib>SHESTERIKOV ANDREJ GENNAD'EVICH</creatorcontrib><creatorcontrib>LUBENTSOV NIKOLAJ VALER'EVICH</creatorcontrib><creatorcontrib>ASTANIN ALEKSANDR JUR'EVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SHESTERIKOV GENNADIJ PETROVICH</au><au>SHESTERIKOV ANDREJ GENNAD'EVICH</au><au>LUBENTSOV NIKOLAJ VALER'EVICH</au><au>ASTANIN ALEKSANDR JUR'EVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>BIMETALLIC CONTACT CORROSION SENSOR</title><date>2012-10-10</date><risdate>2012</risdate><abstract>FIELD: chemistry. ^ SUBSTANCE: bimetallic contact corrosion sensor consists of a piece of steel pipe 1 with a calibrated wall thickness. Copper covers/plugs 2 are attached to the ends of the piece of steel pipe 1 by a copper pin 3 through airtight dielectric spacers 4, and moisture-absorbing material 5, saturated with a salt solution and dried, is laid on the inner surface of the piece of steel pipe 1. A contact electrode 6 made from metal foil is then laid onto the moisture-absorbing material 5, and the cavity 10 of the bimetallic contact corrosion sensor is filled with any dielectric material, e.g., sand. Measuring conductors 8 and 9 are led from the inner surface of the piece of steel pipe 1, measuring conductors 10 and 11 are led from the inner surface of the copper covers/plugs 2, and a measuring conductor 12 is led from the contact electrode 6 made from metal foil. The piece of steel pipe 1 is the housing, detecting element and contact electrode at the same time, and the copper covers/plugs 2, together with the piece of steel pipe 1, form a steel-copper corrosion galvanic couple. ^ EFFECT: determining contact corrosion current and accurate rapid evaluation of cathode protection. ^ 2 cl, 7 dwg
Изобретение относится к технике коррозионного мониторинга подземных трубопроводов, в частности к биметаллическим датчикам контактной коррозии, и может быть использовано в газовой, нефтяной и смежных отраслях промышленности. Биметаллический датчик контактной коррозии состоит из отрезка стальной трубы 1 с калиброванной толщиной стенки. При этом на торцы отрезка стальной трубы 1 закреплены медные крышки - заглушки 2 с помощью медной шпильки 3 через герметичные диэлектрические прокладки 4, а на внутреннюю поверхность отрезка стальной трубы 1 накладывают влагопоглощающий материал 5, пропитанный солевым раствором и высушенный. Затем на влагопоглощающий материал 5 накладывают контактный электрод 6 из металлической фольги, а полость 10 биметаллического датчика контактной коррозии заполняют любым диэлектрическим материалом, например песком. При этом от внутренней поверхности отрезка стальной трубы 1 выводят измерительные проводники 8 и 9, от внутренней поверхности медных крышек-заглушек 2 выводят измерительные проводники 10 и 11, а от контактного электрода 6 из металлической фольги выводят измерительный проводник 12. При этом отрезок стальной трубы 1 является одновременно корпусом, чувствительным элементом и контактным электродом, а медные крышки-заглушки 2 с отрезком стальной трубы 1 образуют коррозионную гальванопару сталь - медь. Техническим результатом изобретения является определение коррозионного тока контактной коррозии и точной экспресс-оценки полноты катодной защиты. 1 з.п. ф-лы, 7 ил.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; rus |
recordid | cdi_epo_espacenet_RU2463576C1 |
source | esp@cenet |
subjects | INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES MEASURING PHYSICS TESTING |
title | BIMETALLIC CONTACT CORROSION SENSOR |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T12%3A25%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SHESTERIKOV%20GENNADIJ%20PETROVICH&rft.date=2012-10-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2463576C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |