METHOD FOR OBTAINING GRAIN-ORIENTED COPPER CONTAINING SILICON STEEL

FIELD: metallurgy. ^ SUBSTANCE: method involves the following stages: hot rolling of slab workpiece, primary cold rolling, degreasing of strip, moderate decarburising annealing so that the strip is heated up to 800C or more in shielding environment with PH2O/PH2, which is equal to 0.50-0.88 during 3...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TSZI JAMIN, LI GOBAO, JAN GOKHUA, SJUJ JUN'PEHN, KHUAN CHANGO, SUN' KHUAN'DEH, JAN JUNTSZILEH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TSZI JAMIN
LI GOBAO
JAN GOKHUA
SJUJ JUN'PEHN
KHUAN CHANGO
SUN' KHUAN'DEH
JAN JUNTSZILEH
description FIELD: metallurgy. ^ SUBSTANCE: method involves the following stages: hot rolling of slab workpiece, primary cold rolling, degreasing of strip, moderate decarburising annealing so that the strip is heated up to 800C or more in shielding environment with PH2O/PH2, which is equal to 0.50-0.88 during 3-8 minutes in order to reduce the carbon content of steel plate to the level of less than 30 ppm; after that, shot blasting and acid etching in order to remove Fe oxide from the surface and to control the oxygen content to the value which is lower than 500 ppm, secondary cold rolling to final thickness and coating of the strip with separating device in the form of water suspension, drying-out to reduce water content to value which is lower than 1.5%, high-temperature annealing in shielding atmosphere containing hydrogen having oxidability (PH2O/PH2); in the range of 0.0001-0.2, application of tension coating and annealing for tension correction. ^ EFFECT: obtaining grain-oriented strip steel with high electromagnetic characteristics and superior quality of the surface. ^ 2 cl, 4 ex, 5 tbl Изобретение относится к производству тектурированной Si стали, содержащей Сu. Для получения текстурованной полосовой стали с высокими электромагнитными характеристиками и превосходным качеством поверхности проводят горячую прокатку слябовой заготовки, первичную холодную прокатку, обезжиривание полосы, умеренный обезуглероживающий отжиг с нагревом полосы до 800°С или более высокой температуры в защитной атмосфере с РH2O/РH2, равным 0,50-0,88, в течение 3-8 минут для снижения содержания углерода стального листа до уровня менее чем 30 ч. на млн, затем обдувку дробью и кислотное травление для удаления оксида Fe с поверхности и для регулирования содержания кислорода до значения ниже, чем 500 ч. на млн, вторичную холодную прокатку до конечной толщины и покрытие полосы сепарирующим средством в виде водной суспензии, высушивание для снижения содержания воды до значения ниже, чем 1,5%, высокотемпературный отжиг в защитной атмосфере, содержащей водород, имеющей способность к окислению (РH2O/РH2); в диапазоне 0,0001-0,2, нанесение покрытия натяжения и отжиг для растяжной правки. 2 з.п. ф-лы, 4 пр., 5 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2457260C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2457260C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2457260C13</originalsourceid><addsrcrecordid>eNrjZHD2dQ3x8HdRcPMPUvB3CnH09PP0c1dwDwIydP2DPF39QlxdFJz9AwJcg4CUH0xBsKePJ5CrEBzi6urDw8CalphTnMoLpbkZFNxcQ5w9dFML8uNTiwsSk1PzUkvig0KNTEzNjcwMnA2NiVACAOEzK0o</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR OBTAINING GRAIN-ORIENTED COPPER CONTAINING SILICON STEEL</title><source>esp@cenet</source><creator>TSZI JAMIN ; LI GOBAO ; JAN GOKHUA ; SJUJ JUN'PEHN ; KHUAN CHANGO ; SUN' KHUAN'DEH ; JAN JUNTSZILEH</creator><creatorcontrib>TSZI JAMIN ; LI GOBAO ; JAN GOKHUA ; SJUJ JUN'PEHN ; KHUAN CHANGO ; SUN' KHUAN'DEH ; JAN JUNTSZILEH</creatorcontrib><description>FIELD: metallurgy. ^ SUBSTANCE: method involves the following stages: hot rolling of slab workpiece, primary cold rolling, degreasing of strip, moderate decarburising annealing so that the strip is heated up to 800C or more in shielding environment with PH2O/PH2, which is equal to 0.50-0.88 during 3-8 minutes in order to reduce the carbon content of steel plate to the level of less than 30 ppm; after that, shot blasting and acid etching in order to remove Fe oxide from the surface and to control the oxygen content to the value which is lower than 500 ppm, secondary cold rolling to final thickness and coating of the strip with separating device in the form of water suspension, drying-out to reduce water content to value which is lower than 1.5%, high-temperature annealing in shielding atmosphere containing hydrogen having oxidability (PH2O/PH2); in the range of 0.0001-0.2, application of tension coating and annealing for tension correction. ^ EFFECT: obtaining grain-oriented strip steel with high electromagnetic characteristics and superior quality of the surface. ^ 2 cl, 4 ex, 5 tbl Изобретение относится к производству тектурированной Si стали, содержащей Сu. Для получения текстурованной полосовой стали с высокими электромагнитными характеристиками и превосходным качеством поверхности проводят горячую прокатку слябовой заготовки, первичную холодную прокатку, обезжиривание полосы, умеренный обезуглероживающий отжиг с нагревом полосы до 800°С или более высокой температуры в защитной атмосфере с РH2O/РH2, равным 0,50-0,88, в течение 3-8 минут для снижения содержания углерода стального листа до уровня менее чем 30 ч. на млн, затем обдувку дробью и кислотное травление для удаления оксида Fe с поверхности и для регулирования содержания кислорода до значения ниже, чем 500 ч. на млн, вторичную холодную прокатку до конечной толщины и покрытие полосы сепарирующим средством в виде водной суспензии, высушивание для снижения содержания воды до значения ниже, чем 1,5%, высокотемпературный отжиг в защитной атмосфере, содержащей водород, имеющей способность к окислению (РH2O/РH2); в диапазоне 0,0001-0,2, нанесение покрытия натяжения и отжиг для растяжной правки. 2 з.п. ф-лы, 4 пр., 5 табл.</description><language>eng ; rus</language><subject>ALLOYS ; BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; ELECTRICITY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; INDUCTANCES ; MAGNETS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES ; TRANSFORMERS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120727&amp;DB=EPODOC&amp;CC=RU&amp;NR=2457260C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120727&amp;DB=EPODOC&amp;CC=RU&amp;NR=2457260C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TSZI JAMIN</creatorcontrib><creatorcontrib>LI GOBAO</creatorcontrib><creatorcontrib>JAN GOKHUA</creatorcontrib><creatorcontrib>SJUJ JUN'PEHN</creatorcontrib><creatorcontrib>KHUAN CHANGO</creatorcontrib><creatorcontrib>SUN' KHUAN'DEH</creatorcontrib><creatorcontrib>JAN JUNTSZILEH</creatorcontrib><title>METHOD FOR OBTAINING GRAIN-ORIENTED COPPER CONTAINING SILICON STEEL</title><description>FIELD: metallurgy. ^ SUBSTANCE: method involves the following stages: hot rolling of slab workpiece, primary cold rolling, degreasing of strip, moderate decarburising annealing so that the strip is heated up to 800C or more in shielding environment with PH2O/PH2, which is equal to 0.50-0.88 during 3-8 minutes in order to reduce the carbon content of steel plate to the level of less than 30 ppm; after that, shot blasting and acid etching in order to remove Fe oxide from the surface and to control the oxygen content to the value which is lower than 500 ppm, secondary cold rolling to final thickness and coating of the strip with separating device in the form of water suspension, drying-out to reduce water content to value which is lower than 1.5%, high-temperature annealing in shielding atmosphere containing hydrogen having oxidability (PH2O/PH2); in the range of 0.0001-0.2, application of tension coating and annealing for tension correction. ^ EFFECT: obtaining grain-oriented strip steel with high electromagnetic characteristics and superior quality of the surface. ^ 2 cl, 4 ex, 5 tbl Изобретение относится к производству тектурированной Si стали, содержащей Сu. Для получения текстурованной полосовой стали с высокими электромагнитными характеристиками и превосходным качеством поверхности проводят горячую прокатку слябовой заготовки, первичную холодную прокатку, обезжиривание полосы, умеренный обезуглероживающий отжиг с нагревом полосы до 800°С или более высокой температуры в защитной атмосфере с РH2O/РH2, равным 0,50-0,88, в течение 3-8 минут для снижения содержания углерода стального листа до уровня менее чем 30 ч. на млн, затем обдувку дробью и кислотное травление для удаления оксида Fe с поверхности и для регулирования содержания кислорода до значения ниже, чем 500 ч. на млн, вторичную холодную прокатку до конечной толщины и покрытие полосы сепарирующим средством в виде водной суспензии, высушивание для снижения содержания воды до значения ниже, чем 1,5%, высокотемпературный отжиг в защитной атмосфере, содержащей водород, имеющей способность к окислению (РH2O/РH2); в диапазоне 0,0001-0,2, нанесение покрытия натяжения и отжиг для растяжной правки. 2 з.п. ф-лы, 4 пр., 5 табл.</description><subject>ALLOYS</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>ELECTRICITY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>INDUCTANCES</subject><subject>MAGNETS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</subject><subject>TRANSFORMERS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD2dQ3x8HdRcPMPUvB3CnH09PP0c1dwDwIydP2DPF39QlxdFJz9AwJcg4CUH0xBsKePJ5CrEBzi6urDw8CalphTnMoLpbkZFNxcQ5w9dFML8uNTiwsSk1PzUkvig0KNTEzNjcwMnA2NiVACAOEzK0o</recordid><startdate>20120727</startdate><enddate>20120727</enddate><creator>TSZI JAMIN</creator><creator>LI GOBAO</creator><creator>JAN GOKHUA</creator><creator>SJUJ JUN'PEHN</creator><creator>KHUAN CHANGO</creator><creator>SUN' KHUAN'DEH</creator><creator>JAN JUNTSZILEH</creator><scope>EVB</scope></search><sort><creationdate>20120727</creationdate><title>METHOD FOR OBTAINING GRAIN-ORIENTED COPPER CONTAINING SILICON STEEL</title><author>TSZI JAMIN ; LI GOBAO ; JAN GOKHUA ; SJUJ JUN'PEHN ; KHUAN CHANGO ; SUN' KHUAN'DEH ; JAN JUNTSZILEH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2457260C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2012</creationdate><topic>ALLOYS</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>ELECTRICITY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>INDUCTANCES</topic><topic>MAGNETS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</topic><topic>TRANSFORMERS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>TSZI JAMIN</creatorcontrib><creatorcontrib>LI GOBAO</creatorcontrib><creatorcontrib>JAN GOKHUA</creatorcontrib><creatorcontrib>SJUJ JUN'PEHN</creatorcontrib><creatorcontrib>KHUAN CHANGO</creatorcontrib><creatorcontrib>SUN' KHUAN'DEH</creatorcontrib><creatorcontrib>JAN JUNTSZILEH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TSZI JAMIN</au><au>LI GOBAO</au><au>JAN GOKHUA</au><au>SJUJ JUN'PEHN</au><au>KHUAN CHANGO</au><au>SUN' KHUAN'DEH</au><au>JAN JUNTSZILEH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR OBTAINING GRAIN-ORIENTED COPPER CONTAINING SILICON STEEL</title><date>2012-07-27</date><risdate>2012</risdate><abstract>FIELD: metallurgy. ^ SUBSTANCE: method involves the following stages: hot rolling of slab workpiece, primary cold rolling, degreasing of strip, moderate decarburising annealing so that the strip is heated up to 800C or more in shielding environment with PH2O/PH2, which is equal to 0.50-0.88 during 3-8 minutes in order to reduce the carbon content of steel plate to the level of less than 30 ppm; after that, shot blasting and acid etching in order to remove Fe oxide from the surface and to control the oxygen content to the value which is lower than 500 ppm, secondary cold rolling to final thickness and coating of the strip with separating device in the form of water suspension, drying-out to reduce water content to value which is lower than 1.5%, high-temperature annealing in shielding atmosphere containing hydrogen having oxidability (PH2O/PH2); in the range of 0.0001-0.2, application of tension coating and annealing for tension correction. ^ EFFECT: obtaining grain-oriented strip steel with high electromagnetic characteristics and superior quality of the surface. ^ 2 cl, 4 ex, 5 tbl Изобретение относится к производству тектурированной Si стали, содержащей Сu. Для получения текстурованной полосовой стали с высокими электромагнитными характеристиками и превосходным качеством поверхности проводят горячую прокатку слябовой заготовки, первичную холодную прокатку, обезжиривание полосы, умеренный обезуглероживающий отжиг с нагревом полосы до 800°С или более высокой температуры в защитной атмосфере с РH2O/РH2, равным 0,50-0,88, в течение 3-8 минут для снижения содержания углерода стального листа до уровня менее чем 30 ч. на млн, затем обдувку дробью и кислотное травление для удаления оксида Fe с поверхности и для регулирования содержания кислорода до значения ниже, чем 500 ч. на млн, вторичную холодную прокатку до конечной толщины и покрытие полосы сепарирующим средством в виде водной суспензии, высушивание для снижения содержания воды до значения ниже, чем 1,5%, высокотемпературный отжиг в защитной атмосфере, содержащей водород, имеющей способность к окислению (РH2O/РH2); в диапазоне 0,0001-0,2, нанесение покрытия натяжения и отжиг для растяжной правки. 2 з.п. ф-лы, 4 пр., 5 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2457260C1
source esp@cenet
subjects ALLOYS
BASIC ELECTRIC ELEMENTS
CHEMISTRY
ELECTRICITY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
INDUCTANCES
MAGNETS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
TRANSFORMERS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title METHOD FOR OBTAINING GRAIN-ORIENTED COPPER CONTAINING SILICON STEEL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T22%3A38%3A42IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TSZI%20JAMIN&rft.date=2012-07-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2457260C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true