ADSORBENT-DESICCANT AND PREPARATION METHOD THEREOF

FIELD: chemistry. ^ SUBSTANCE: invention relates to chemistry. The spherically shaped adsorbent-desiccant is prepared by balling moist powder of a nanostructured oxygen-containing aluminium compound. The granules undergo thermal-steam treatment in air at the first step at temperature 20-25C for 1-20...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NOSKOV ALEKSANDR STEPANOVICH, GLAZYRIN ALEKSEJ VLADIMIROVICH, BABENKO VLADIMIR SEMENOVICH, PARMON VALENTIN NIKOLAEVICH, DANILEVICH VLADIMIR VLADIMIROVICH, MOLCHANOV VIKTOR VIKTOROVICH, ISUPOVA LJUBOV' ALEKSANDROVNA, KRUGLJAKOV VASILIJ JUR'EVICH, KHARINA IRINA VALER'EVNA
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NOSKOV ALEKSANDR STEPANOVICH
GLAZYRIN ALEKSEJ VLADIMIROVICH
BABENKO VLADIMIR SEMENOVICH
PARMON VALENTIN NIKOLAEVICH
DANILEVICH VLADIMIR VLADIMIROVICH
MOLCHANOV VIKTOR VIKTOROVICH
ISUPOVA LJUBOV' ALEKSANDROVNA
KRUGLJAKOV VASILIJ JUR'EVICH
KHARINA IRINA VALER'EVNA
description FIELD: chemistry. ^ SUBSTANCE: invention relates to chemistry. The spherically shaped adsorbent-desiccant is prepared by balling moist powder of a nanostructured oxygen-containing aluminium compound. The granules undergo thermal-steam treatment in air at the first step at temperature 20-25C for 1-20 hours, at the second step at 100-120C for 1-20 hours and calcination at 450-550C in a current of dry air and rate of heating to calcination temperature of 20-50C/h for 2-6 hours. The nanostructured oxygen-containing aluminium compound of formula: Al2O3-x(OH)xnH2O, where x is in the range of 0-0.28 and n is in the range of 0.1-0.4, is mixed with a modifying additive such as: CaO and/or Na2O, and/or MgO, and/or zeolite. A spherically shaped adsorbent-desiccant is obtained, which contains aluminium oxide in form of a mixture ç-, -, - and is X-ray amorphous, and a modifying additive such as: zeolite and/or (in terms of) CaO and/or Na2O, and/or MgO is also obtained. ^ EFFECT: invention increases adsorbent capacity. ^ 11 cl, 1 tbl, 35 ex Изобретение относится к области химии. Адсорбент-осушитель сферической формы готовят путем скатывания увлажненного порошка наноструктурированного кислородсодержащего соединения алюминия. Гранулы подвергают термопаровой обработке, сушке на воздухе на первом этапе при температуре 20-25°C в течение 1-20 ч, на втором - при 100-120°C в течение 1-20 ч и прокаливанию при температуре 450-550°C в токе осушенного воздуха и скорости разогрева до температуры прокалки 20-50°С/ч в течение 2-6 ч. В наноструктурированное кислородсодержащее соединение алюминия состава: Al2O3-x(OH)x·nH2O, где x находится в диапазоне 0-0,28, а n в диапазоне 0,1-0,4, вводят модифицирующую добавку, такую как: CaO, и/или Na2O, и/или MgO, и/или цеолит. Получают адсорбент-осушитель сферической формы, содержащий оксидаалюминия в виде смеси χ-, η-, γ- и рентгеноаморфной фазы и модифицирующую добавку, такую как: цеолит, и/или (в пересчете) CaO, и/или Na2O, и/или MgO. Изобретение позволяет повысить емкость адсорбента. 2 н. и 9 з.п. ф-лы, 1 табл., 35 пр.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2455232C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2455232C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2455232C23</originalsourceid><addsrcrecordid>eNrjZDBydAn2D3Jy9QvRdXEN9nR2dvQLUXD0c1EICHINcAxyDPH091PwdQ3x8HdRCPFwDXL1d-NhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoUYmpqZGxkbORsZEKAEAOG8mnA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>ADSORBENT-DESICCANT AND PREPARATION METHOD THEREOF</title><source>esp@cenet</source><creator>NOSKOV ALEKSANDR STEPANOVICH ; GLAZYRIN ALEKSEJ VLADIMIROVICH ; BABENKO VLADIMIR SEMENOVICH ; PARMON VALENTIN NIKOLAEVICH ; DANILEVICH VLADIMIR VLADIMIROVICH ; MOLCHANOV VIKTOR VIKTOROVICH ; ISUPOVA LJUBOV' ALEKSANDROVNA ; KRUGLJAKOV VASILIJ JUR'EVICH ; KHARINA IRINA VALER'EVNA</creator><creatorcontrib>NOSKOV ALEKSANDR STEPANOVICH ; GLAZYRIN ALEKSEJ VLADIMIROVICH ; BABENKO VLADIMIR SEMENOVICH ; PARMON VALENTIN NIKOLAEVICH ; DANILEVICH VLADIMIR VLADIMIROVICH ; MOLCHANOV VIKTOR VIKTOROVICH ; ISUPOVA LJUBOV' ALEKSANDROVNA ; KRUGLJAKOV VASILIJ JUR'EVICH ; KHARINA IRINA VALER'EVNA</creatorcontrib><description>FIELD: chemistry. ^ SUBSTANCE: invention relates to chemistry. The spherically shaped adsorbent-desiccant is prepared by balling moist powder of a nanostructured oxygen-containing aluminium compound. The granules undergo thermal-steam treatment in air at the first step at temperature 20-25C for 1-20 hours, at the second step at 100-120C for 1-20 hours and calcination at 450-550C in a current of dry air and rate of heating to calcination temperature of 20-50C/h for 2-6 hours. The nanostructured oxygen-containing aluminium compound of formula: Al2O3-x(OH)xnH2O, where x is in the range of 0-0.28 and n is in the range of 0.1-0.4, is mixed with a modifying additive such as: CaO and/or Na2O, and/or MgO, and/or zeolite. A spherically shaped adsorbent-desiccant is obtained, which contains aluminium oxide in form of a mixture ç-, -, - and is X-ray amorphous, and a modifying additive such as: zeolite and/or (in terms of) CaO and/or Na2O, and/or MgO is also obtained. ^ EFFECT: invention increases adsorbent capacity. ^ 11 cl, 1 tbl, 35 ex Изобретение относится к области химии. Адсорбент-осушитель сферической формы готовят путем скатывания увлажненного порошка наноструктурированного кислородсодержащего соединения алюминия. Гранулы подвергают термопаровой обработке, сушке на воздухе на первом этапе при температуре 20-25°C в течение 1-20 ч, на втором - при 100-120°C в течение 1-20 ч и прокаливанию при температуре 450-550°C в токе осушенного воздуха и скорости разогрева до температуры прокалки 20-50°С/ч в течение 2-6 ч. В наноструктурированное кислородсодержащее соединение алюминия состава: Al2O3-x(OH)x·nH2O, где x находится в диапазоне 0-0,28, а n в диапазоне 0,1-0,4, вводят модифицирующую добавку, такую как: CaO, и/или Na2O, и/или MgO, и/или цеолит. Получают адсорбент-осушитель сферической формы, содержащий оксидаалюминия в виде смеси χ-, η-, γ- и рентгеноаморфной фазы и модифицирующую добавку, такую как: цеолит, и/или (в пересчете) CaO, и/или Na2O, и/или MgO. Изобретение позволяет повысить емкость адсорбента. 2 н. и 9 з.п. ф-лы, 1 табл., 35 пр.</description><language>eng ; rus</language><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; INORGANIC CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; SEPARATION ; THEIR RELEVANT APPARATUS ; TRANSPORTING</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120710&amp;DB=EPODOC&amp;CC=RU&amp;NR=2455232C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120710&amp;DB=EPODOC&amp;CC=RU&amp;NR=2455232C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NOSKOV ALEKSANDR STEPANOVICH</creatorcontrib><creatorcontrib>GLAZYRIN ALEKSEJ VLADIMIROVICH</creatorcontrib><creatorcontrib>BABENKO VLADIMIR SEMENOVICH</creatorcontrib><creatorcontrib>PARMON VALENTIN NIKOLAEVICH</creatorcontrib><creatorcontrib>DANILEVICH VLADIMIR VLADIMIROVICH</creatorcontrib><creatorcontrib>MOLCHANOV VIKTOR VIKTOROVICH</creatorcontrib><creatorcontrib>ISUPOVA LJUBOV' ALEKSANDROVNA</creatorcontrib><creatorcontrib>KRUGLJAKOV VASILIJ JUR'EVICH</creatorcontrib><creatorcontrib>KHARINA IRINA VALER'EVNA</creatorcontrib><title>ADSORBENT-DESICCANT AND PREPARATION METHOD THEREOF</title><description>FIELD: chemistry. ^ SUBSTANCE: invention relates to chemistry. The spherically shaped adsorbent-desiccant is prepared by balling moist powder of a nanostructured oxygen-containing aluminium compound. The granules undergo thermal-steam treatment in air at the first step at temperature 20-25C for 1-20 hours, at the second step at 100-120C for 1-20 hours and calcination at 450-550C in a current of dry air and rate of heating to calcination temperature of 20-50C/h for 2-6 hours. The nanostructured oxygen-containing aluminium compound of formula: Al2O3-x(OH)xnH2O, where x is in the range of 0-0.28 and n is in the range of 0.1-0.4, is mixed with a modifying additive such as: CaO and/or Na2O, and/or MgO, and/or zeolite. A spherically shaped adsorbent-desiccant is obtained, which contains aluminium oxide in form of a mixture ç-, -, - and is X-ray amorphous, and a modifying additive such as: zeolite and/or (in terms of) CaO and/or Na2O, and/or MgO is also obtained. ^ EFFECT: invention increases adsorbent capacity. ^ 11 cl, 1 tbl, 35 ex Изобретение относится к области химии. Адсорбент-осушитель сферической формы готовят путем скатывания увлажненного порошка наноструктурированного кислородсодержащего соединения алюминия. Гранулы подвергают термопаровой обработке, сушке на воздухе на первом этапе при температуре 20-25°C в течение 1-20 ч, на втором - при 100-120°C в течение 1-20 ч и прокаливанию при температуре 450-550°C в токе осушенного воздуха и скорости разогрева до температуры прокалки 20-50°С/ч в течение 2-6 ч. В наноструктурированное кислородсодержащее соединение алюминия состава: Al2O3-x(OH)x·nH2O, где x находится в диапазоне 0-0,28, а n в диапазоне 0,1-0,4, вводят модифицирующую добавку, такую как: CaO, и/или Na2O, и/или MgO, и/или цеолит. Получают адсорбент-осушитель сферической формы, содержащий оксидаалюминия в виде смеси χ-, η-, γ- и рентгеноаморфной фазы и модифицирующую добавку, такую как: цеолит, и/или (в пересчете) CaO, и/или Na2O, и/или MgO. Изобретение позволяет повысить емкость адсорбента. 2 н. и 9 з.п. ф-лы, 1 табл., 35 пр.</description><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>SEPARATION</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDBydAn2D3Jy9QvRdXEN9nR2dvQLUXD0c1EICHINcAxyDPH091PwdQ3x8HdRCPFwDXL1d-NhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoUYmpqZGxkbORsZEKAEAOG8mnA</recordid><startdate>20120710</startdate><enddate>20120710</enddate><creator>NOSKOV ALEKSANDR STEPANOVICH</creator><creator>GLAZYRIN ALEKSEJ VLADIMIROVICH</creator><creator>BABENKO VLADIMIR SEMENOVICH</creator><creator>PARMON VALENTIN NIKOLAEVICH</creator><creator>DANILEVICH VLADIMIR VLADIMIROVICH</creator><creator>MOLCHANOV VIKTOR VIKTOROVICH</creator><creator>ISUPOVA LJUBOV' ALEKSANDROVNA</creator><creator>KRUGLJAKOV VASILIJ JUR'EVICH</creator><creator>KHARINA IRINA VALER'EVNA</creator><scope>EVB</scope></search><sort><creationdate>20120710</creationdate><title>ADSORBENT-DESICCANT AND PREPARATION METHOD THEREOF</title><author>NOSKOV ALEKSANDR STEPANOVICH ; GLAZYRIN ALEKSEJ VLADIMIROVICH ; BABENKO VLADIMIR SEMENOVICH ; PARMON VALENTIN NIKOLAEVICH ; DANILEVICH VLADIMIR VLADIMIROVICH ; MOLCHANOV VIKTOR VIKTOROVICH ; ISUPOVA LJUBOV' ALEKSANDROVNA ; KRUGLJAKOV VASILIJ JUR'EVICH ; KHARINA IRINA VALER'EVNA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2455232C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2012</creationdate><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>SEPARATION</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>NOSKOV ALEKSANDR STEPANOVICH</creatorcontrib><creatorcontrib>GLAZYRIN ALEKSEJ VLADIMIROVICH</creatorcontrib><creatorcontrib>BABENKO VLADIMIR SEMENOVICH</creatorcontrib><creatorcontrib>PARMON VALENTIN NIKOLAEVICH</creatorcontrib><creatorcontrib>DANILEVICH VLADIMIR VLADIMIROVICH</creatorcontrib><creatorcontrib>MOLCHANOV VIKTOR VIKTOROVICH</creatorcontrib><creatorcontrib>ISUPOVA LJUBOV' ALEKSANDROVNA</creatorcontrib><creatorcontrib>KRUGLJAKOV VASILIJ JUR'EVICH</creatorcontrib><creatorcontrib>KHARINA IRINA VALER'EVNA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NOSKOV ALEKSANDR STEPANOVICH</au><au>GLAZYRIN ALEKSEJ VLADIMIROVICH</au><au>BABENKO VLADIMIR SEMENOVICH</au><au>PARMON VALENTIN NIKOLAEVICH</au><au>DANILEVICH VLADIMIR VLADIMIROVICH</au><au>MOLCHANOV VIKTOR VIKTOROVICH</au><au>ISUPOVA LJUBOV' ALEKSANDROVNA</au><au>KRUGLJAKOV VASILIJ JUR'EVICH</au><au>KHARINA IRINA VALER'EVNA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>ADSORBENT-DESICCANT AND PREPARATION METHOD THEREOF</title><date>2012-07-10</date><risdate>2012</risdate><abstract>FIELD: chemistry. ^ SUBSTANCE: invention relates to chemistry. The spherically shaped adsorbent-desiccant is prepared by balling moist powder of a nanostructured oxygen-containing aluminium compound. The granules undergo thermal-steam treatment in air at the first step at temperature 20-25C for 1-20 hours, at the second step at 100-120C for 1-20 hours and calcination at 450-550C in a current of dry air and rate of heating to calcination temperature of 20-50C/h for 2-6 hours. The nanostructured oxygen-containing aluminium compound of formula: Al2O3-x(OH)xnH2O, where x is in the range of 0-0.28 and n is in the range of 0.1-0.4, is mixed with a modifying additive such as: CaO and/or Na2O, and/or MgO, and/or zeolite. A spherically shaped adsorbent-desiccant is obtained, which contains aluminium oxide in form of a mixture ç-, -, - and is X-ray amorphous, and a modifying additive such as: zeolite and/or (in terms of) CaO and/or Na2O, and/or MgO is also obtained. ^ EFFECT: invention increases adsorbent capacity. ^ 11 cl, 1 tbl, 35 ex Изобретение относится к области химии. Адсорбент-осушитель сферической формы готовят путем скатывания увлажненного порошка наноструктурированного кислородсодержащего соединения алюминия. Гранулы подвергают термопаровой обработке, сушке на воздухе на первом этапе при температуре 20-25°C в течение 1-20 ч, на втором - при 100-120°C в течение 1-20 ч и прокаливанию при температуре 450-550°C в токе осушенного воздуха и скорости разогрева до температуры прокалки 20-50°С/ч в течение 2-6 ч. В наноструктурированное кислородсодержащее соединение алюминия состава: Al2O3-x(OH)x·nH2O, где x находится в диапазоне 0-0,28, а n в диапазоне 0,1-0,4, вводят модифицирующую добавку, такую как: CaO, и/или Na2O, и/или MgO, и/или цеолит. Получают адсорбент-осушитель сферической формы, содержащий оксидаалюминия в виде смеси χ-, η-, γ- и рентгеноаморфной фазы и модифицирующую добавку, такую как: цеолит, и/или (в пересчете) CaO, и/или Na2O, и/или MgO. Изобретение позволяет повысить емкость адсорбента. 2 н. и 9 з.п. ф-лы, 1 табл., 35 пр.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2455232C2
source esp@cenet
subjects CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY
CHEMISTRY
COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS
INORGANIC CHEMISTRY
METALLURGY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
SEPARATION
THEIR RELEVANT APPARATUS
TRANSPORTING
title ADSORBENT-DESICCANT AND PREPARATION METHOD THEREOF
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-26T06%3A51%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NOSKOV%20ALEKSANDR%20STEPANOVICH&rft.date=2012-07-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2455232C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true