MANUFACTURING METHOD OF BLACK SHEET IRON

FIELD: metallurgy. ^ SUBSTANCE: for manufacturing of electrotinning sheet metal with high plastic properties and qualitative surface it is implemented continuous slab casting from aluminium-killed steel, got rolling and winding of strip into roll at 670-690C, strips etching, cold rolling with total...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DUBROVSKIJ BORIS ALEKSANDROVICH, ZAVALISHCHIN ALEKSANDR NIKOLAEVICH, MOLEVA OL'GA NIKOLAEVNA, ZHELTOUKHOV JURIJ BORISOVICH, FAJZULINA RIMMA VAFIROVNA, D'JAKONOV ALEKSANDR ANATOL'EVICH, DENISOV SERGEJ VLADIMIROVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DUBROVSKIJ BORIS ALEKSANDROVICH
ZAVALISHCHIN ALEKSANDR NIKOLAEVICH
MOLEVA OL'GA NIKOLAEVNA
ZHELTOUKHOV JURIJ BORISOVICH
FAJZULINA RIMMA VAFIROVNA
D'JAKONOV ALEKSANDR ANATOL'EVICH
DENISOV SERGEJ VLADIMIROVICH
description FIELD: metallurgy. ^ SUBSTANCE: for manufacturing of electrotinning sheet metal with high plastic properties and qualitative surface it is implemented continuous slab casting from aluminium-killed steel, got rolling and winding of strip into roll at 670-690C, strips etching, cold rolling with total drafting 90-93%, degreasing, recrystallisation annealing in bell-type furnace and temper rolling, herewith recrystallisation annealing in bell-type furnace is implemented with regulation of temperature conditions of annealing by temperature of winding of strips into roll: at first stand thermocouple is installed to the temperature of the beginning of steel recrystallisation: 550C - for steel 08 ps, at which it is kept 5-8 hours, it is implemented heating up to temperature higher than temperature of the beginning of recrystallisation 100-120C, it is kept 3-6 hours, then temperature is reduced for 40-50C lower than Ar1 for steel 08 ps - 680C is isolated 5-10 hours and cooled with switched on burners under heating hood up to temperature Ar1(100-80) C, at which heating hood is removed and cooled under muffle up to 120-150C. Training is implemented at 20-40C with drafting 0.5-1.0%. ^ EFFECT: development of effective method of black sheet iron manufacturing from low-carbon steel. ^ 2 tbl, 1 ex Изобретение относится к области металлургии, в частности к производству черной жести из малоуглеродистой стали. Для производства жести электролитического лужения с высокими пластическими свойствами и качественной поверхностью проводят непрерывную разливку слябов из раскисленной алюминием стали, горячую прокатку и смотку полосы в рулон при 670-690°С, травление полос, холодную прокатку с суммарными обжатиями 90-93%, обезжиривание, рекристаллизационный отжиг в колпаковой печи и дрессировку, при этом рекристаллизационный отжиг в колпаковой печи производят с регулированием температурного режима отжига по температуре смотки полос в рулон: сначала стендовую термопару устанавливают на температуру начала рекристаллизации стали: 550°С - для стали 08 пс, при которой выдерживают 5-8 ч, производят нагрев до температуры выше температуры начала рекристаллизации на 100-120°С, выдерживают 3-6 ч, затем температуру снижают на 40-50°С ниже Ar1 для стали 08пс - 680°С выдерживают 5-10 ч и охлаждают с выключенными горелками под нагревательным колпаком до температуры Ar1-(100-80)°C, при которой нагревательный колпак снимают и охлаждают под муфелем до 120-150°С. Дрессировку производят при 20-40°С с обжа
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2371486C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2371486C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2371486C13</originalsourceid><addsrcrecordid>eNrjZNDwdfQLdXN0DgkN8vRzV_B1DfHwd1Hwd1Nw8nF09lYI9nB1DVHwDPL342FgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8UGhRsbmhiYWZs6GxkQoAQC6FCO1</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MANUFACTURING METHOD OF BLACK SHEET IRON</title><source>esp@cenet</source><creator>DUBROVSKIJ BORIS ALEKSANDROVICH ; ZAVALISHCHIN ALEKSANDR NIKOLAEVICH ; MOLEVA OL'GA NIKOLAEVNA ; ZHELTOUKHOV JURIJ BORISOVICH ; FAJZULINA RIMMA VAFIROVNA ; D'JAKONOV ALEKSANDR ANATOL'EVICH ; DENISOV SERGEJ VLADIMIROVICH</creator><creatorcontrib>DUBROVSKIJ BORIS ALEKSANDROVICH ; ZAVALISHCHIN ALEKSANDR NIKOLAEVICH ; MOLEVA OL'GA NIKOLAEVNA ; ZHELTOUKHOV JURIJ BORISOVICH ; FAJZULINA RIMMA VAFIROVNA ; D'JAKONOV ALEKSANDR ANATOL'EVICH ; DENISOV SERGEJ VLADIMIROVICH</creatorcontrib><description>FIELD: metallurgy. ^ SUBSTANCE: for manufacturing of electrotinning sheet metal with high plastic properties and qualitative surface it is implemented continuous slab casting from aluminium-killed steel, got rolling and winding of strip into roll at 670-690C, strips etching, cold rolling with total drafting 90-93%, degreasing, recrystallisation annealing in bell-type furnace and temper rolling, herewith recrystallisation annealing in bell-type furnace is implemented with regulation of temperature conditions of annealing by temperature of winding of strips into roll: at first stand thermocouple is installed to the temperature of the beginning of steel recrystallisation: 550C - for steel 08 ps, at which it is kept 5-8 hours, it is implemented heating up to temperature higher than temperature of the beginning of recrystallisation 100-120C, it is kept 3-6 hours, then temperature is reduced for 40-50C lower than Ar1 for steel 08 ps - 680C is isolated 5-10 hours and cooled with switched on burners under heating hood up to temperature Ar1(100-80) C, at which heating hood is removed and cooled under muffle up to 120-150C. Training is implemented at 20-40C with drafting 0.5-1.0%. ^ EFFECT: development of effective method of black sheet iron manufacturing from low-carbon steel. ^ 2 tbl, 1 ex Изобретение относится к области металлургии, в частности к производству черной жести из малоуглеродистой стали. Для производства жести электролитического лужения с высокими пластическими свойствами и качественной поверхностью проводят непрерывную разливку слябов из раскисленной алюминием стали, горячую прокатку и смотку полосы в рулон при 670-690°С, травление полос, холодную прокатку с суммарными обжатиями 90-93%, обезжиривание, рекристаллизационный отжиг в колпаковой печи и дрессировку, при этом рекристаллизационный отжиг в колпаковой печи производят с регулированием температурного режима отжига по температуре смотки полос в рулон: сначала стендовую термопару устанавливают на температуру начала рекристаллизации стали: 550°С - для стали 08 пс, при которой выдерживают 5-8 ч, производят нагрев до температуры выше температуры начала рекристаллизации на 100-120°С, выдерживают 3-6 ч, затем температуру снижают на 40-50°С ниже Ar1 для стали 08пс - 680°С выдерживают 5-10 ч и охлаждают с выключенными горелками под нагревательным колпаком до температуры Ar1-(100-80)°C, при которой нагревательный колпак снимают и охлаждают под муфелем до 120-150°С. Дрессировку производят при 20-40°С с обжатием 0,5-1,0%. 2 табл.</description><language>eng ; rus</language><subject>CHEMISTRY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091027&amp;DB=EPODOC&amp;CC=RU&amp;NR=2371486C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091027&amp;DB=EPODOC&amp;CC=RU&amp;NR=2371486C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DUBROVSKIJ BORIS ALEKSANDROVICH</creatorcontrib><creatorcontrib>ZAVALISHCHIN ALEKSANDR NIKOLAEVICH</creatorcontrib><creatorcontrib>MOLEVA OL'GA NIKOLAEVNA</creatorcontrib><creatorcontrib>ZHELTOUKHOV JURIJ BORISOVICH</creatorcontrib><creatorcontrib>FAJZULINA RIMMA VAFIROVNA</creatorcontrib><creatorcontrib>D'JAKONOV ALEKSANDR ANATOL'EVICH</creatorcontrib><creatorcontrib>DENISOV SERGEJ VLADIMIROVICH</creatorcontrib><title>MANUFACTURING METHOD OF BLACK SHEET IRON</title><description>FIELD: metallurgy. ^ SUBSTANCE: for manufacturing of electrotinning sheet metal with high plastic properties and qualitative surface it is implemented continuous slab casting from aluminium-killed steel, got rolling and winding of strip into roll at 670-690C, strips etching, cold rolling with total drafting 90-93%, degreasing, recrystallisation annealing in bell-type furnace and temper rolling, herewith recrystallisation annealing in bell-type furnace is implemented with regulation of temperature conditions of annealing by temperature of winding of strips into roll: at first stand thermocouple is installed to the temperature of the beginning of steel recrystallisation: 550C - for steel 08 ps, at which it is kept 5-8 hours, it is implemented heating up to temperature higher than temperature of the beginning of recrystallisation 100-120C, it is kept 3-6 hours, then temperature is reduced for 40-50C lower than Ar1 for steel 08 ps - 680C is isolated 5-10 hours and cooled with switched on burners under heating hood up to temperature Ar1(100-80) C, at which heating hood is removed and cooled under muffle up to 120-150C. Training is implemented at 20-40C with drafting 0.5-1.0%. ^ EFFECT: development of effective method of black sheet iron manufacturing from low-carbon steel. ^ 2 tbl, 1 ex Изобретение относится к области металлургии, в частности к производству черной жести из малоуглеродистой стали. Для производства жести электролитического лужения с высокими пластическими свойствами и качественной поверхностью проводят непрерывную разливку слябов из раскисленной алюминием стали, горячую прокатку и смотку полосы в рулон при 670-690°С, травление полос, холодную прокатку с суммарными обжатиями 90-93%, обезжиривание, рекристаллизационный отжиг в колпаковой печи и дрессировку, при этом рекристаллизационный отжиг в колпаковой печи производят с регулированием температурного режима отжига по температуре смотки полос в рулон: сначала стендовую термопару устанавливают на температуру начала рекристаллизации стали: 550°С - для стали 08 пс, при которой выдерживают 5-8 ч, производят нагрев до температуры выше температуры начала рекристаллизации на 100-120°С, выдерживают 3-6 ч, затем температуру снижают на 40-50°С ниже Ar1 для стали 08пс - 680°С выдерживают 5-10 ч и охлаждают с выключенными горелками под нагревательным колпаком до температуры Ar1-(100-80)°C, при которой нагревательный колпак снимают и охлаждают под муфелем до 120-150°С. Дрессировку производят при 20-40°С с обжатием 0,5-1,0%. 2 табл.</description><subject>CHEMISTRY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNDwdfQLdXN0DgkN8vRzV_B1DfHwd1Hwd1Nw8nF09lYI9nB1DVHwDPL342FgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8UGhRsbmhiYWZs6GxkQoAQC6FCO1</recordid><startdate>20091027</startdate><enddate>20091027</enddate><creator>DUBROVSKIJ BORIS ALEKSANDROVICH</creator><creator>ZAVALISHCHIN ALEKSANDR NIKOLAEVICH</creator><creator>MOLEVA OL'GA NIKOLAEVNA</creator><creator>ZHELTOUKHOV JURIJ BORISOVICH</creator><creator>FAJZULINA RIMMA VAFIROVNA</creator><creator>D'JAKONOV ALEKSANDR ANATOL'EVICH</creator><creator>DENISOV SERGEJ VLADIMIROVICH</creator><scope>EVB</scope></search><sort><creationdate>20091027</creationdate><title>MANUFACTURING METHOD OF BLACK SHEET IRON</title><author>DUBROVSKIJ BORIS ALEKSANDROVICH ; ZAVALISHCHIN ALEKSANDR NIKOLAEVICH ; MOLEVA OL'GA NIKOLAEVNA ; ZHELTOUKHOV JURIJ BORISOVICH ; FAJZULINA RIMMA VAFIROVNA ; D'JAKONOV ALEKSANDR ANATOL'EVICH ; DENISOV SERGEJ VLADIMIROVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2371486C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2009</creationdate><topic>CHEMISTRY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>DUBROVSKIJ BORIS ALEKSANDROVICH</creatorcontrib><creatorcontrib>ZAVALISHCHIN ALEKSANDR NIKOLAEVICH</creatorcontrib><creatorcontrib>MOLEVA OL'GA NIKOLAEVNA</creatorcontrib><creatorcontrib>ZHELTOUKHOV JURIJ BORISOVICH</creatorcontrib><creatorcontrib>FAJZULINA RIMMA VAFIROVNA</creatorcontrib><creatorcontrib>D'JAKONOV ALEKSANDR ANATOL'EVICH</creatorcontrib><creatorcontrib>DENISOV SERGEJ VLADIMIROVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DUBROVSKIJ BORIS ALEKSANDROVICH</au><au>ZAVALISHCHIN ALEKSANDR NIKOLAEVICH</au><au>MOLEVA OL'GA NIKOLAEVNA</au><au>ZHELTOUKHOV JURIJ BORISOVICH</au><au>FAJZULINA RIMMA VAFIROVNA</au><au>D'JAKONOV ALEKSANDR ANATOL'EVICH</au><au>DENISOV SERGEJ VLADIMIROVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MANUFACTURING METHOD OF BLACK SHEET IRON</title><date>2009-10-27</date><risdate>2009</risdate><abstract>FIELD: metallurgy. ^ SUBSTANCE: for manufacturing of electrotinning sheet metal with high plastic properties and qualitative surface it is implemented continuous slab casting from aluminium-killed steel, got rolling and winding of strip into roll at 670-690C, strips etching, cold rolling with total drafting 90-93%, degreasing, recrystallisation annealing in bell-type furnace and temper rolling, herewith recrystallisation annealing in bell-type furnace is implemented with regulation of temperature conditions of annealing by temperature of winding of strips into roll: at first stand thermocouple is installed to the temperature of the beginning of steel recrystallisation: 550C - for steel 08 ps, at which it is kept 5-8 hours, it is implemented heating up to temperature higher than temperature of the beginning of recrystallisation 100-120C, it is kept 3-6 hours, then temperature is reduced for 40-50C lower than Ar1 for steel 08 ps - 680C is isolated 5-10 hours and cooled with switched on burners under heating hood up to temperature Ar1(100-80) C, at which heating hood is removed and cooled under muffle up to 120-150C. Training is implemented at 20-40C with drafting 0.5-1.0%. ^ EFFECT: development of effective method of black sheet iron manufacturing from low-carbon steel. ^ 2 tbl, 1 ex Изобретение относится к области металлургии, в частности к производству черной жести из малоуглеродистой стали. Для производства жести электролитического лужения с высокими пластическими свойствами и качественной поверхностью проводят непрерывную разливку слябов из раскисленной алюминием стали, горячую прокатку и смотку полосы в рулон при 670-690°С, травление полос, холодную прокатку с суммарными обжатиями 90-93%, обезжиривание, рекристаллизационный отжиг в колпаковой печи и дрессировку, при этом рекристаллизационный отжиг в колпаковой печи производят с регулированием температурного режима отжига по температуре смотки полос в рулон: сначала стендовую термопару устанавливают на температуру начала рекристаллизации стали: 550°С - для стали 08 пс, при которой выдерживают 5-8 ч, производят нагрев до температуры выше температуры начала рекристаллизации на 100-120°С, выдерживают 3-6 ч, затем температуру снижают на 40-50°С ниже Ar1 для стали 08пс - 680°С выдерживают 5-10 ч и охлаждают с выключенными горелками под нагревательным колпаком до температуры Ar1-(100-80)°C, при которой нагревательный колпак снимают и охлаждают под муфелем до 120-150°С. Дрессировку производят при 20-40°С с обжатием 0,5-1,0%. 2 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2371486C1
source esp@cenet
subjects CHEMISTRY
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
title MANUFACTURING METHOD OF BLACK SHEET IRON
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-01T15%3A27%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DUBROVSKIJ%20BORIS%20ALEKSANDROVICH&rft.date=2009-10-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2371486C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true