METHOD TO STABILISE SPHERICAL DOUBLE-BASE POWDER

FIELD: explosives. ^ SUBSTANCE: proposed method comprises preparing 1.5 to 3.5%-aqueous stabilising emulsion, powder suspension in reactor incorporating mixer, introducing produced stabilising emulsion in obtained powder suspension and treating powder suspension on mixing by stabilising emulsion. St...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: STAROVEROV ALEKSANDR ALEKSANDROVICH, ENEJKINA TAT'JANA ALEKSANDROVNA, SOPIN VLADIMIR FEDOROVICH, KHATSRINOV ALEKSEJ IL'ICH, LJAPIN NIKOLAJ MIKHAJLOVICH, GARIFULLIN IL'DUS SHUGAEBOVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator STAROVEROV ALEKSANDR ALEKSANDROVICH
ENEJKINA TAT'JANA ALEKSANDROVNA
SOPIN VLADIMIR FEDOROVICH
KHATSRINOV ALEKSEJ IL'ICH
LJAPIN NIKOLAJ MIKHAJLOVICH
GARIFULLIN IL'DUS SHUGAEBOVICH
description FIELD: explosives. ^ SUBSTANCE: proposed method comprises preparing 1.5 to 3.5%-aqueous stabilising emulsion, powder suspension in reactor incorporating mixer, introducing produced stabilising emulsion in obtained powder suspension and treating powder suspension on mixing by stabilising emulsion. Stabilising emulsion is prepared by mixing, with water and in preset ratio, of pure skin glue and dimethyl-diphenyl urea 1, or mix of dimethyl-diphenyl urea and dinitrotoluene. Prior to introducing produced stabilising emulsion into powder suspension, the former is heated to 76 to 80C. Powder suspension is treated by stabilising suspension for 60 to 65 minutes at 76 to 80C. ^ EFFECT: increased powder gas pressure, reduced small arms cartridge charges. ^ 1 tbl, 6 ex Изобретение относится к области производства сферических двухосновных порохов для снаряжения патронов стрелкового оружия. Способ флегматизации сферического двухосновного пороха включает приготовление 1,5-3,5%-ной водной флегматизирующей эмульсии, приготовление суспензии пороха в реакторе с перемешивающим устройством, введение полученной флегматизирующей эмульсии в полученную суспензию пороха, обработку суспензии пороха при перемешивании флегматизирующей эмульсией. Флегматизирующую эмульсию готовят перемешиванием с водой в определенном соотношении мездрового клея и централита I или смеси централита и динитротолуола. Полученную флегматизирующую эмульсию перед введением ее в суспензию пороха нагревают до температуры 76-80°С. Обработку суспензии пороха флегматизирующей эмульсией ведут в течение 60-65 минут при температуре 76-80°С. Изобретение обеспечивает повышение давления пороховых газов и снижение массы зарядов для снаряжения патронов стрелкового оружия. 1 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2367639C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2367639C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2367639C23</originalsourceid><addsrcrecordid>eNrjZDDwdQ3x8HdRCPFXCA5xdPL08Qx2VQgO8HAN8nR29FFw8Q918nHVdXIEigb4h7u4BvEwsKYl5hSn8kJpbgYFN9cQZw_d1IL8-NTigsTk1LzUkvigUCNjM3MzY0tnI2MilAAA368mBA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD TO STABILISE SPHERICAL DOUBLE-BASE POWDER</title><source>esp@cenet</source><creator>STAROVEROV ALEKSANDR ALEKSANDROVICH ; ENEJKINA TAT'JANA ALEKSANDROVNA ; SOPIN VLADIMIR FEDOROVICH ; KHATSRINOV ALEKSEJ IL'ICH ; LJAPIN NIKOLAJ MIKHAJLOVICH ; GARIFULLIN IL'DUS SHUGAEBOVICH</creator><creatorcontrib>STAROVEROV ALEKSANDR ALEKSANDROVICH ; ENEJKINA TAT'JANA ALEKSANDROVNA ; SOPIN VLADIMIR FEDOROVICH ; KHATSRINOV ALEKSEJ IL'ICH ; LJAPIN NIKOLAJ MIKHAJLOVICH ; GARIFULLIN IL'DUS SHUGAEBOVICH</creatorcontrib><description>FIELD: explosives. ^ SUBSTANCE: proposed method comprises preparing 1.5 to 3.5%-aqueous stabilising emulsion, powder suspension in reactor incorporating mixer, introducing produced stabilising emulsion in obtained powder suspension and treating powder suspension on mixing by stabilising emulsion. Stabilising emulsion is prepared by mixing, with water and in preset ratio, of pure skin glue and dimethyl-diphenyl urea 1, or mix of dimethyl-diphenyl urea and dinitrotoluene. Prior to introducing produced stabilising emulsion into powder suspension, the former is heated to 76 to 80C. Powder suspension is treated by stabilising suspension for 60 to 65 minutes at 76 to 80C. ^ EFFECT: increased powder gas pressure, reduced small arms cartridge charges. ^ 1 tbl, 6 ex Изобретение относится к области производства сферических двухосновных порохов для снаряжения патронов стрелкового оружия. Способ флегматизации сферического двухосновного пороха включает приготовление 1,5-3,5%-ной водной флегматизирующей эмульсии, приготовление суспензии пороха в реакторе с перемешивающим устройством, введение полученной флегматизирующей эмульсии в полученную суспензию пороха, обработку суспензии пороха при перемешивании флегматизирующей эмульсией. Флегматизирующую эмульсию готовят перемешиванием с водой в определенном соотношении мездрового клея и централита I или смеси централита и динитротолуола. Полученную флегматизирующую эмульсию перед введением ее в суспензию пороха нагревают до температуры 76-80°С. Обработку суспензии пороха флегматизирующей эмульсией ведут в течение 60-65 минут при температуре 76-80°С. Изобретение обеспечивает повышение давления пороховых газов и снижение массы зарядов для снаряжения патронов стрелкового оружия. 1 табл.</description><language>eng ; rus</language><subject>CHEMISTRY ; EXPLOSIVES ; EXPLOSIVES OR THERMIC COMPOSITIONS ; MANUFACTURE THEREOF ; MATCHES ; METALLURGY ; USE OF SINGLE SUBSTANCES AS EXPLOSIVES</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090920&amp;DB=EPODOC&amp;CC=RU&amp;NR=2367639C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25566,76549</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090920&amp;DB=EPODOC&amp;CC=RU&amp;NR=2367639C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>STAROVEROV ALEKSANDR ALEKSANDROVICH</creatorcontrib><creatorcontrib>ENEJKINA TAT'JANA ALEKSANDROVNA</creatorcontrib><creatorcontrib>SOPIN VLADIMIR FEDOROVICH</creatorcontrib><creatorcontrib>KHATSRINOV ALEKSEJ IL'ICH</creatorcontrib><creatorcontrib>LJAPIN NIKOLAJ MIKHAJLOVICH</creatorcontrib><creatorcontrib>GARIFULLIN IL'DUS SHUGAEBOVICH</creatorcontrib><title>METHOD TO STABILISE SPHERICAL DOUBLE-BASE POWDER</title><description>FIELD: explosives. ^ SUBSTANCE: proposed method comprises preparing 1.5 to 3.5%-aqueous stabilising emulsion, powder suspension in reactor incorporating mixer, introducing produced stabilising emulsion in obtained powder suspension and treating powder suspension on mixing by stabilising emulsion. Stabilising emulsion is prepared by mixing, with water and in preset ratio, of pure skin glue and dimethyl-diphenyl urea 1, or mix of dimethyl-diphenyl urea and dinitrotoluene. Prior to introducing produced stabilising emulsion into powder suspension, the former is heated to 76 to 80C. Powder suspension is treated by stabilising suspension for 60 to 65 minutes at 76 to 80C. ^ EFFECT: increased powder gas pressure, reduced small arms cartridge charges. ^ 1 tbl, 6 ex Изобретение относится к области производства сферических двухосновных порохов для снаряжения патронов стрелкового оружия. Способ флегматизации сферического двухосновного пороха включает приготовление 1,5-3,5%-ной водной флегматизирующей эмульсии, приготовление суспензии пороха в реакторе с перемешивающим устройством, введение полученной флегматизирующей эмульсии в полученную суспензию пороха, обработку суспензии пороха при перемешивании флегматизирующей эмульсией. Флегматизирующую эмульсию готовят перемешиванием с водой в определенном соотношении мездрового клея и централита I или смеси централита и динитротолуола. Полученную флегматизирующую эмульсию перед введением ее в суспензию пороха нагревают до температуры 76-80°С. Обработку суспензии пороха флегматизирующей эмульсией ведут в течение 60-65 минут при температуре 76-80°С. Изобретение обеспечивает повышение давления пороховых газов и снижение массы зарядов для снаряжения патронов стрелкового оружия. 1 табл.</description><subject>CHEMISTRY</subject><subject>EXPLOSIVES</subject><subject>EXPLOSIVES OR THERMIC COMPOSITIONS</subject><subject>MANUFACTURE THEREOF</subject><subject>MATCHES</subject><subject>METALLURGY</subject><subject>USE OF SINGLE SUBSTANCES AS EXPLOSIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDwdQ3x8HdRCPFXCA5xdPL08Qx2VQgO8HAN8nR29FFw8Q918nHVdXIEigb4h7u4BvEwsKYl5hSn8kJpbgYFN9cQZw_d1IL8-NTigsTk1LzUkvigUCNjM3MzY0tnI2MilAAA368mBA</recordid><startdate>20090920</startdate><enddate>20090920</enddate><creator>STAROVEROV ALEKSANDR ALEKSANDROVICH</creator><creator>ENEJKINA TAT'JANA ALEKSANDROVNA</creator><creator>SOPIN VLADIMIR FEDOROVICH</creator><creator>KHATSRINOV ALEKSEJ IL'ICH</creator><creator>LJAPIN NIKOLAJ MIKHAJLOVICH</creator><creator>GARIFULLIN IL'DUS SHUGAEBOVICH</creator><scope>EVB</scope></search><sort><creationdate>20090920</creationdate><title>METHOD TO STABILISE SPHERICAL DOUBLE-BASE POWDER</title><author>STAROVEROV ALEKSANDR ALEKSANDROVICH ; ENEJKINA TAT'JANA ALEKSANDROVNA ; SOPIN VLADIMIR FEDOROVICH ; KHATSRINOV ALEKSEJ IL'ICH ; LJAPIN NIKOLAJ MIKHAJLOVICH ; GARIFULLIN IL'DUS SHUGAEBOVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2367639C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2009</creationdate><topic>CHEMISTRY</topic><topic>EXPLOSIVES</topic><topic>EXPLOSIVES OR THERMIC COMPOSITIONS</topic><topic>MANUFACTURE THEREOF</topic><topic>MATCHES</topic><topic>METALLURGY</topic><topic>USE OF SINGLE SUBSTANCES AS EXPLOSIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>STAROVEROV ALEKSANDR ALEKSANDROVICH</creatorcontrib><creatorcontrib>ENEJKINA TAT'JANA ALEKSANDROVNA</creatorcontrib><creatorcontrib>SOPIN VLADIMIR FEDOROVICH</creatorcontrib><creatorcontrib>KHATSRINOV ALEKSEJ IL'ICH</creatorcontrib><creatorcontrib>LJAPIN NIKOLAJ MIKHAJLOVICH</creatorcontrib><creatorcontrib>GARIFULLIN IL'DUS SHUGAEBOVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>STAROVEROV ALEKSANDR ALEKSANDROVICH</au><au>ENEJKINA TAT'JANA ALEKSANDROVNA</au><au>SOPIN VLADIMIR FEDOROVICH</au><au>KHATSRINOV ALEKSEJ IL'ICH</au><au>LJAPIN NIKOLAJ MIKHAJLOVICH</au><au>GARIFULLIN IL'DUS SHUGAEBOVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD TO STABILISE SPHERICAL DOUBLE-BASE POWDER</title><date>2009-09-20</date><risdate>2009</risdate><abstract>FIELD: explosives. ^ SUBSTANCE: proposed method comprises preparing 1.5 to 3.5%-aqueous stabilising emulsion, powder suspension in reactor incorporating mixer, introducing produced stabilising emulsion in obtained powder suspension and treating powder suspension on mixing by stabilising emulsion. Stabilising emulsion is prepared by mixing, with water and in preset ratio, of pure skin glue and dimethyl-diphenyl urea 1, or mix of dimethyl-diphenyl urea and dinitrotoluene. Prior to introducing produced stabilising emulsion into powder suspension, the former is heated to 76 to 80C. Powder suspension is treated by stabilising suspension for 60 to 65 minutes at 76 to 80C. ^ EFFECT: increased powder gas pressure, reduced small arms cartridge charges. ^ 1 tbl, 6 ex Изобретение относится к области производства сферических двухосновных порохов для снаряжения патронов стрелкового оружия. Способ флегматизации сферического двухосновного пороха включает приготовление 1,5-3,5%-ной водной флегматизирующей эмульсии, приготовление суспензии пороха в реакторе с перемешивающим устройством, введение полученной флегматизирующей эмульсии в полученную суспензию пороха, обработку суспензии пороха при перемешивании флегматизирующей эмульсией. Флегматизирующую эмульсию готовят перемешиванием с водой в определенном соотношении мездрового клея и централита I или смеси централита и динитротолуола. Полученную флегматизирующую эмульсию перед введением ее в суспензию пороха нагревают до температуры 76-80°С. Обработку суспензии пороха флегматизирующей эмульсией ведут в течение 60-65 минут при температуре 76-80°С. Изобретение обеспечивает повышение давления пороховых газов и снижение массы зарядов для снаряжения патронов стрелкового оружия. 1 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2367639C2
source esp@cenet
subjects CHEMISTRY
EXPLOSIVES
EXPLOSIVES OR THERMIC COMPOSITIONS
MANUFACTURE THEREOF
MATCHES
METALLURGY
USE OF SINGLE SUBSTANCES AS EXPLOSIVES
title METHOD TO STABILISE SPHERICAL DOUBLE-BASE POWDER
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-18T04%3A13%3A19IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=STAROVEROV%20ALEKSANDR%20ALEKSANDROVICH&rft.date=2009-09-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2367639C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true