FIBER SHEETING MAINLY FOR CORRUGATING AND PACKAGING MADE OF IT

FIELD: textile, paper. ^ SUBSTANCE: invention relates to pulp and paper industry, precisely to paper for corrugating as well as packaging made by using it. Fiber sheeting contains waste paper in quantity 35-75 wt % and softwood pulp - 25-65 wt % with 60-65 % yield of cellulose fiber at the degree of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZVJAGIN GENNADIJ VASIL'EVICH, KONOVALOVA ELENA EVGEN'EVNA, TORJANSKIJ MIKHAIL IVANOVICH, SMIRNOV GENNADIJ ALEKSANDROVICH, FITSNER ALEKSANDR LEONIDOVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZVJAGIN GENNADIJ VASIL'EVICH
KONOVALOVA ELENA EVGEN'EVNA
TORJANSKIJ MIKHAIL IVANOVICH
SMIRNOV GENNADIJ ALEKSANDROVICH
FITSNER ALEKSANDR LEONIDOVICH
description FIELD: textile, paper. ^ SUBSTANCE: invention relates to pulp and paper industry, precisely to paper for corrugating as well as packaging made by using it. Fiber sheeting contains waste paper in quantity 35-75 wt % and softwood pulp - 25-65 wt % with 60-65 % yield of cellulose fiber at the degree of pulp cooking 75-95 units of Kappa. Cellulose is prepared by modified Mg-bisulfite pulp cooking of the mixture containing pine and fir chips, the ratio of fir is not less than 30 wt %. Corrugated board is prepared by gluing corrugated and plane layers of paper with said composition. Packaging, for example corrugated boxes, are made of corrugated board usually having three or five layers. High content of resinous matters ensures required blotting capacity without applying sizing compounds. ^ EFFECT: fiber sheeting and packaging produced by using it have high strength and stiffening properties. ^ 3 cl, 1 tbl, 5 ex Изобретение относится к целлюлозно-бумажной промышленности, в частности к бумаге для гофрирования, а также таре, выполненной с ее использованием. Листовой волокнистый материал содержит макулатуру в количестве 35-75 мас.% и хвойную целлюлозу 25-65 мас.% с выходом целлюлозного волокна 60-65% со степенью делигнификации 75-95 единиц Каппа. Целлюлоза получена путем модифицированной Mg-бисульфитной варки смеси щепы сосны и ели с содержанием ели не менее 30 мас.%. Гофрированный картон получен путем склеивания гофрированных и плоских слоев из бумаги указанного состава. Из готового картона, обычно трехслойного или пятислойного, изготавливают тару, например гофроящики. Высокое содержание смолистых веществ обеспечивает требуемую впитываемость бумаги без введения проклеивающих веществ. Листовой волокнистый материал и тара, полученная с его использованием, обладают высокими прочностными и жесткостными характеристиками. 2 з.п. ф-лы, 1 табл.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2355840C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2355840C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2355840C13</originalsourceid><addsrcrecordid>eNrjZLBz83RyDVII9nB1DfH0c1fwdfT084lUcPMPUnD2DwoKdXcECzv6uSgEODp7O7pDFLm4Kvi7KXiG8DCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQI2NTUwsTA2dDYyKUAADaWClh</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>FIBER SHEETING MAINLY FOR CORRUGATING AND PACKAGING MADE OF IT</title><source>esp@cenet</source><creator>ZVJAGIN GENNADIJ VASIL'EVICH ; KONOVALOVA ELENA EVGEN'EVNA ; TORJANSKIJ MIKHAIL IVANOVICH ; SMIRNOV GENNADIJ ALEKSANDROVICH ; FITSNER ALEKSANDR LEONIDOVICH</creator><creatorcontrib>ZVJAGIN GENNADIJ VASIL'EVICH ; KONOVALOVA ELENA EVGEN'EVNA ; TORJANSKIJ MIKHAIL IVANOVICH ; SMIRNOV GENNADIJ ALEKSANDROVICH ; FITSNER ALEKSANDR LEONIDOVICH</creatorcontrib><description>FIELD: textile, paper. ^ SUBSTANCE: invention relates to pulp and paper industry, precisely to paper for corrugating as well as packaging made by using it. Fiber sheeting contains waste paper in quantity 35-75 wt % and softwood pulp - 25-65 wt % with 60-65 % yield of cellulose fiber at the degree of pulp cooking 75-95 units of Kappa. Cellulose is prepared by modified Mg-bisulfite pulp cooking of the mixture containing pine and fir chips, the ratio of fir is not less than 30 wt %. Corrugated board is prepared by gluing corrugated and plane layers of paper with said composition. Packaging, for example corrugated boxes, are made of corrugated board usually having three or five layers. High content of resinous matters ensures required blotting capacity without applying sizing compounds. ^ EFFECT: fiber sheeting and packaging produced by using it have high strength and stiffening properties. ^ 3 cl, 1 tbl, 5 ex Изобретение относится к целлюлозно-бумажной промышленности, в частности к бумаге для гофрирования, а также таре, выполненной с ее использованием. Листовой волокнистый материал содержит макулатуру в количестве 35-75 мас.% и хвойную целлюлозу 25-65 мас.% с выходом целлюлозного волокна 60-65% со степенью делигнификации 75-95 единиц Каппа. Целлюлоза получена путем модифицированной Mg-бисульфитной варки смеси щепы сосны и ели с содержанием ели не менее 30 мас.%. Гофрированный картон получен путем склеивания гофрированных и плоских слоев из бумаги указанного состава. Из готового картона, обычно трехслойного или пятислойного, изготавливают тару, например гофроящики. Высокое содержание смолистых веществ обеспечивает требуемую впитываемость бумаги без введения проклеивающих веществ. Листовой волокнистый материал и тара, полученная с его использованием, обладают высокими прочностными и жесткостными характеристиками. 2 з.п. ф-лы, 1 табл.</description><language>eng ; rus</language><subject>METHODS OF PRODUCING PAPER THEREON ; PAPER-MAKING ; PAPER-MAKING MACHINES ; PRODUCTION OF CELLULOSE ; TEXTILES</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090520&amp;DB=EPODOC&amp;CC=RU&amp;NR=2355840C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090520&amp;DB=EPODOC&amp;CC=RU&amp;NR=2355840C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZVJAGIN GENNADIJ VASIL'EVICH</creatorcontrib><creatorcontrib>KONOVALOVA ELENA EVGEN'EVNA</creatorcontrib><creatorcontrib>TORJANSKIJ MIKHAIL IVANOVICH</creatorcontrib><creatorcontrib>SMIRNOV GENNADIJ ALEKSANDROVICH</creatorcontrib><creatorcontrib>FITSNER ALEKSANDR LEONIDOVICH</creatorcontrib><title>FIBER SHEETING MAINLY FOR CORRUGATING AND PACKAGING MADE OF IT</title><description>FIELD: textile, paper. ^ SUBSTANCE: invention relates to pulp and paper industry, precisely to paper for corrugating as well as packaging made by using it. Fiber sheeting contains waste paper in quantity 35-75 wt % and softwood pulp - 25-65 wt % with 60-65 % yield of cellulose fiber at the degree of pulp cooking 75-95 units of Kappa. Cellulose is prepared by modified Mg-bisulfite pulp cooking of the mixture containing pine and fir chips, the ratio of fir is not less than 30 wt %. Corrugated board is prepared by gluing corrugated and plane layers of paper with said composition. Packaging, for example corrugated boxes, are made of corrugated board usually having three or five layers. High content of resinous matters ensures required blotting capacity without applying sizing compounds. ^ EFFECT: fiber sheeting and packaging produced by using it have high strength and stiffening properties. ^ 3 cl, 1 tbl, 5 ex Изобретение относится к целлюлозно-бумажной промышленности, в частности к бумаге для гофрирования, а также таре, выполненной с ее использованием. Листовой волокнистый материал содержит макулатуру в количестве 35-75 мас.% и хвойную целлюлозу 25-65 мас.% с выходом целлюлозного волокна 60-65% со степенью делигнификации 75-95 единиц Каппа. Целлюлоза получена путем модифицированной Mg-бисульфитной варки смеси щепы сосны и ели с содержанием ели не менее 30 мас.%. Гофрированный картон получен путем склеивания гофрированных и плоских слоев из бумаги указанного состава. Из готового картона, обычно трехслойного или пятислойного, изготавливают тару, например гофроящики. Высокое содержание смолистых веществ обеспечивает требуемую впитываемость бумаги без введения проклеивающих веществ. Листовой волокнистый материал и тара, полученная с его использованием, обладают высокими прочностными и жесткостными характеристиками. 2 з.п. ф-лы, 1 табл.</description><subject>METHODS OF PRODUCING PAPER THEREON</subject><subject>PAPER-MAKING</subject><subject>PAPER-MAKING MACHINES</subject><subject>PRODUCTION OF CELLULOSE</subject><subject>TEXTILES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLBz83RyDVII9nB1DfH0c1fwdfT084lUcPMPUnD2DwoKdXcECzv6uSgEODp7O7pDFLm4Kvi7KXiG8DCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQI2NTUwsTA2dDYyKUAADaWClh</recordid><startdate>20090520</startdate><enddate>20090520</enddate><creator>ZVJAGIN GENNADIJ VASIL'EVICH</creator><creator>KONOVALOVA ELENA EVGEN'EVNA</creator><creator>TORJANSKIJ MIKHAIL IVANOVICH</creator><creator>SMIRNOV GENNADIJ ALEKSANDROVICH</creator><creator>FITSNER ALEKSANDR LEONIDOVICH</creator><scope>EVB</scope></search><sort><creationdate>20090520</creationdate><title>FIBER SHEETING MAINLY FOR CORRUGATING AND PACKAGING MADE OF IT</title><author>ZVJAGIN GENNADIJ VASIL'EVICH ; KONOVALOVA ELENA EVGEN'EVNA ; TORJANSKIJ MIKHAIL IVANOVICH ; SMIRNOV GENNADIJ ALEKSANDROVICH ; FITSNER ALEKSANDR LEONIDOVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2355840C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2009</creationdate><topic>METHODS OF PRODUCING PAPER THEREON</topic><topic>PAPER-MAKING</topic><topic>PAPER-MAKING MACHINES</topic><topic>PRODUCTION OF CELLULOSE</topic><topic>TEXTILES</topic><toplevel>online_resources</toplevel><creatorcontrib>ZVJAGIN GENNADIJ VASIL'EVICH</creatorcontrib><creatorcontrib>KONOVALOVA ELENA EVGEN'EVNA</creatorcontrib><creatorcontrib>TORJANSKIJ MIKHAIL IVANOVICH</creatorcontrib><creatorcontrib>SMIRNOV GENNADIJ ALEKSANDROVICH</creatorcontrib><creatorcontrib>FITSNER ALEKSANDR LEONIDOVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZVJAGIN GENNADIJ VASIL'EVICH</au><au>KONOVALOVA ELENA EVGEN'EVNA</au><au>TORJANSKIJ MIKHAIL IVANOVICH</au><au>SMIRNOV GENNADIJ ALEKSANDROVICH</au><au>FITSNER ALEKSANDR LEONIDOVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>FIBER SHEETING MAINLY FOR CORRUGATING AND PACKAGING MADE OF IT</title><date>2009-05-20</date><risdate>2009</risdate><abstract>FIELD: textile, paper. ^ SUBSTANCE: invention relates to pulp and paper industry, precisely to paper for corrugating as well as packaging made by using it. Fiber sheeting contains waste paper in quantity 35-75 wt % and softwood pulp - 25-65 wt % with 60-65 % yield of cellulose fiber at the degree of pulp cooking 75-95 units of Kappa. Cellulose is prepared by modified Mg-bisulfite pulp cooking of the mixture containing pine and fir chips, the ratio of fir is not less than 30 wt %. Corrugated board is prepared by gluing corrugated and plane layers of paper with said composition. Packaging, for example corrugated boxes, are made of corrugated board usually having three or five layers. High content of resinous matters ensures required blotting capacity without applying sizing compounds. ^ EFFECT: fiber sheeting and packaging produced by using it have high strength and stiffening properties. ^ 3 cl, 1 tbl, 5 ex Изобретение относится к целлюлозно-бумажной промышленности, в частности к бумаге для гофрирования, а также таре, выполненной с ее использованием. Листовой волокнистый материал содержит макулатуру в количестве 35-75 мас.% и хвойную целлюлозу 25-65 мас.% с выходом целлюлозного волокна 60-65% со степенью делигнификации 75-95 единиц Каппа. Целлюлоза получена путем модифицированной Mg-бисульфитной варки смеси щепы сосны и ели с содержанием ели не менее 30 мас.%. Гофрированный картон получен путем склеивания гофрированных и плоских слоев из бумаги указанного состава. Из готового картона, обычно трехслойного или пятислойного, изготавливают тару, например гофроящики. Высокое содержание смолистых веществ обеспечивает требуемую впитываемость бумаги без введения проклеивающих веществ. Листовой волокнистый материал и тара, полученная с его использованием, обладают высокими прочностными и жесткостными характеристиками. 2 з.п. ф-лы, 1 табл.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2355840C1
source esp@cenet
subjects METHODS OF PRODUCING PAPER THEREON
PAPER-MAKING
PAPER-MAKING MACHINES
PRODUCTION OF CELLULOSE
TEXTILES
title FIBER SHEETING MAINLY FOR CORRUGATING AND PACKAGING MADE OF IT
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T14%3A05%3A37IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZVJAGIN%20GENNADIJ%20VASIL'EVICH&rft.date=2009-05-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2355840C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true