MELTING METHOD OF FERROTITANIUM
FIELD: metallurgy. ^ SUBSTANCE: invention relates to metallurgy field. Particularly it relates to production of ferroalloys by aluminothermy process. In the method in the capacity of titanium-bearing raw material it is used liquid titanic slag, it is mixed metallothermic part of charge, consisting o...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | KORZUN VIKTOR KAZIMIROVICH TREGUBENKO VIKTOR VASIL'EVICH BOBKOV LEONID NIKOLAEVICH KONOTOPCHIK KONSTANTIN UL'JANOVICH |
description | FIELD: metallurgy. ^ SUBSTANCE: invention relates to metallurgy field. Particularly it relates to production of ferroalloys by aluminothermy process. In the method in the capacity of titanium-bearing raw material it is used liquid titanic slag, it is mixed metallothermic part of charge, consisting of iron-ore concentrates, aluminium powder, lime and ferrosilicium in relation 1:(1.09-1.18):(0.27-0.33):(0.08-0.09) agreeably, in amount 126-146% of titanium slag mass, then it is mixed and penetrate main part of charge, consisting of iron-ore concentrate, lime and aluminium powder in relation 1:(0.1-0.29):(0.43-0.46) agreeably, in amount 15-25% of titanium slag mass. In the capacity of titanium-bearing raw material it is used liquid titanic slag with content 85-95% % TiO2 at temperature 1700-1850C. ^ EFFECT: reduction of aluminium consumption for melting ensured by usage of liquid titanic slag, and also receiving of titanium and aluminous semi-product for melting of synthetic slag. ^ 2 cl, 1 tbl
Изобретение относится к области металлургии, в частности к производству ферросплавов алюминотермическим процессом. В способе в качестве титаносодержащего сырья используют жидкий титановый шлак, смешивают металлотермическую часть шихты, состоящую из железорудного концентрата, алюминиевого порошка, извести и ферросилиция в соотношении 1:(1,09-1,18):(0,27-0,33):(0,08-0,09) соответственно, в количестве 126-146% от массы титанового шлака, далее смешивают и проплавляют основную часть шихты, состоящую из железорудного концентрата, извести и алюминиевого порошка в соотношении 1:(0,1-0,29):(0,43-0,46) соответственно, в количестве 15-25% от массы титанового шлака. В качестве титаносодержащего сырья используют жидкий титановый шлак с содержанием 85-95% % TiO2 при температуре 1700-1850°С. Изобретение позволяет снизить расход алюминия на плавку за счет использования жидкого титанового шлака, а также получить титан и глиноземистый полупродукт для выплавки синтетических шлаков. 1 з.п. ф-лы, 1 табл. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2351678C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2351678C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2351678C23</originalsourceid><addsrcrecordid>eNrjZJD3dfUJ8fRzV_B1DfHwd1Hwd1Nwcw0K8g_xDHH08wz15WFgTUvMKU7lhdLcDED5EGcP3dSC_PjU4oLE5NS81JL4oFAjY1NDM3MLZyNjIpQAAKGeIYc</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MELTING METHOD OF FERROTITANIUM</title><source>esp@cenet</source><creator>KORZUN VIKTOR KAZIMIROVICH ; TREGUBENKO VIKTOR VASIL'EVICH ; BOBKOV LEONID NIKOLAEVICH ; KONOTOPCHIK KONSTANTIN UL'JANOVICH</creator><creatorcontrib>KORZUN VIKTOR KAZIMIROVICH ; TREGUBENKO VIKTOR VASIL'EVICH ; BOBKOV LEONID NIKOLAEVICH ; KONOTOPCHIK KONSTANTIN UL'JANOVICH</creatorcontrib><description>FIELD: metallurgy. ^ SUBSTANCE: invention relates to metallurgy field. Particularly it relates to production of ferroalloys by aluminothermy process. In the method in the capacity of titanium-bearing raw material it is used liquid titanic slag, it is mixed metallothermic part of charge, consisting of iron-ore concentrates, aluminium powder, lime and ferrosilicium in relation 1:(1.09-1.18):(0.27-0.33):(0.08-0.09) agreeably, in amount 126-146% of titanium slag mass, then it is mixed and penetrate main part of charge, consisting of iron-ore concentrate, lime and aluminium powder in relation 1:(0.1-0.29):(0.43-0.46) agreeably, in amount 15-25% of titanium slag mass. In the capacity of titanium-bearing raw material it is used liquid titanic slag with content 85-95% % TiO2 at temperature 1700-1850C. ^ EFFECT: reduction of aluminium consumption for melting ensured by usage of liquid titanic slag, and also receiving of titanium and aluminous semi-product for melting of synthetic slag. ^ 2 cl, 1 tbl
Изобретение относится к области металлургии, в частности к производству ферросплавов алюминотермическим процессом. В способе в качестве титаносодержащего сырья используют жидкий титановый шлак, смешивают металлотермическую часть шихты, состоящую из железорудного концентрата, алюминиевого порошка, извести и ферросилиция в соотношении 1:(1,09-1,18):(0,27-0,33):(0,08-0,09) соответственно, в количестве 126-146% от массы титанового шлака, далее смешивают и проплавляют основную часть шихты, состоящую из железорудного концентрата, извести и алюминиевого порошка в соотношении 1:(0,1-0,29):(0,43-0,46) соответственно, в количестве 15-25% от массы титанового шлака. В качестве титаносодержащего сырья используют жидкий титановый шлак с содержанием 85-95% % TiO2 при температуре 1700-1850°С. Изобретение позволяет снизить расход алюминия на плавку за счет использования жидкого титанового шлака, а также получить титан и глиноземистый полупродукт для выплавки синтетических шлаков. 1 з.п. ф-лы, 1 табл.</description><language>eng ; rus</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090410&DB=EPODOC&CC=RU&NR=2351678C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090410&DB=EPODOC&CC=RU&NR=2351678C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KORZUN VIKTOR KAZIMIROVICH</creatorcontrib><creatorcontrib>TREGUBENKO VIKTOR VASIL'EVICH</creatorcontrib><creatorcontrib>BOBKOV LEONID NIKOLAEVICH</creatorcontrib><creatorcontrib>KONOTOPCHIK KONSTANTIN UL'JANOVICH</creatorcontrib><title>MELTING METHOD OF FERROTITANIUM</title><description>FIELD: metallurgy. ^ SUBSTANCE: invention relates to metallurgy field. Particularly it relates to production of ferroalloys by aluminothermy process. In the method in the capacity of titanium-bearing raw material it is used liquid titanic slag, it is mixed metallothermic part of charge, consisting of iron-ore concentrates, aluminium powder, lime and ferrosilicium in relation 1:(1.09-1.18):(0.27-0.33):(0.08-0.09) agreeably, in amount 126-146% of titanium slag mass, then it is mixed and penetrate main part of charge, consisting of iron-ore concentrate, lime and aluminium powder in relation 1:(0.1-0.29):(0.43-0.46) agreeably, in amount 15-25% of titanium slag mass. In the capacity of titanium-bearing raw material it is used liquid titanic slag with content 85-95% % TiO2 at temperature 1700-1850C. ^ EFFECT: reduction of aluminium consumption for melting ensured by usage of liquid titanic slag, and also receiving of titanium and aluminous semi-product for melting of synthetic slag. ^ 2 cl, 1 tbl
Изобретение относится к области металлургии, в частности к производству ферросплавов алюминотермическим процессом. В способе в качестве титаносодержащего сырья используют жидкий титановый шлак, смешивают металлотермическую часть шихты, состоящую из железорудного концентрата, алюминиевого порошка, извести и ферросилиция в соотношении 1:(1,09-1,18):(0,27-0,33):(0,08-0,09) соответственно, в количестве 126-146% от массы титанового шлака, далее смешивают и проплавляют основную часть шихты, состоящую из железорудного концентрата, извести и алюминиевого порошка в соотношении 1:(0,1-0,29):(0,43-0,46) соответственно, в количестве 15-25% от массы титанового шлака. В качестве титаносодержащего сырья используют жидкий титановый шлак с содержанием 85-95% % TiO2 при температуре 1700-1850°С. Изобретение позволяет снизить расход алюминия на плавку за счет использования жидкого титанового шлака, а также получить титан и глиноземистый полупродукт для выплавки синтетических шлаков. 1 з.п. ф-лы, 1 табл.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJD3dfUJ8fRzV_B1DfHwd1Hwd1Nwcw0K8g_xDHH08wz15WFgTUvMKU7lhdLcDED5EGcP3dSC_PjU4oLE5NS81JL4oFAjY1NDM3MLZyNjIpQAAKGeIYc</recordid><startdate>20090410</startdate><enddate>20090410</enddate><creator>KORZUN VIKTOR KAZIMIROVICH</creator><creator>TREGUBENKO VIKTOR VASIL'EVICH</creator><creator>BOBKOV LEONID NIKOLAEVICH</creator><creator>KONOTOPCHIK KONSTANTIN UL'JANOVICH</creator><scope>EVB</scope></search><sort><creationdate>20090410</creationdate><title>MELTING METHOD OF FERROTITANIUM</title><author>KORZUN VIKTOR KAZIMIROVICH ; TREGUBENKO VIKTOR VASIL'EVICH ; BOBKOV LEONID NIKOLAEVICH ; KONOTOPCHIK KONSTANTIN UL'JANOVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2351678C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2009</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>KORZUN VIKTOR KAZIMIROVICH</creatorcontrib><creatorcontrib>TREGUBENKO VIKTOR VASIL'EVICH</creatorcontrib><creatorcontrib>BOBKOV LEONID NIKOLAEVICH</creatorcontrib><creatorcontrib>KONOTOPCHIK KONSTANTIN UL'JANOVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KORZUN VIKTOR KAZIMIROVICH</au><au>TREGUBENKO VIKTOR VASIL'EVICH</au><au>BOBKOV LEONID NIKOLAEVICH</au><au>KONOTOPCHIK KONSTANTIN UL'JANOVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MELTING METHOD OF FERROTITANIUM</title><date>2009-04-10</date><risdate>2009</risdate><abstract>FIELD: metallurgy. ^ SUBSTANCE: invention relates to metallurgy field. Particularly it relates to production of ferroalloys by aluminothermy process. In the method in the capacity of titanium-bearing raw material it is used liquid titanic slag, it is mixed metallothermic part of charge, consisting of iron-ore concentrates, aluminium powder, lime and ferrosilicium in relation 1:(1.09-1.18):(0.27-0.33):(0.08-0.09) agreeably, in amount 126-146% of titanium slag mass, then it is mixed and penetrate main part of charge, consisting of iron-ore concentrate, lime and aluminium powder in relation 1:(0.1-0.29):(0.43-0.46) agreeably, in amount 15-25% of titanium slag mass. In the capacity of titanium-bearing raw material it is used liquid titanic slag with content 85-95% % TiO2 at temperature 1700-1850C. ^ EFFECT: reduction of aluminium consumption for melting ensured by usage of liquid titanic slag, and also receiving of titanium and aluminous semi-product for melting of synthetic slag. ^ 2 cl, 1 tbl
Изобретение относится к области металлургии, в частности к производству ферросплавов алюминотермическим процессом. В способе в качестве титаносодержащего сырья используют жидкий титановый шлак, смешивают металлотермическую часть шихты, состоящую из железорудного концентрата, алюминиевого порошка, извести и ферросилиция в соотношении 1:(1,09-1,18):(0,27-0,33):(0,08-0,09) соответственно, в количестве 126-146% от массы титанового шлака, далее смешивают и проплавляют основную часть шихты, состоящую из железорудного концентрата, извести и алюминиевого порошка в соотношении 1:(0,1-0,29):(0,43-0,46) соответственно, в количестве 15-25% от массы титанового шлака. В качестве титаносодержащего сырья используют жидкий титановый шлак с содержанием 85-95% % TiO2 при температуре 1700-1850°С. Изобретение позволяет снизить расход алюминия на плавку за счет использования жидкого титанового шлака, а также получить титан и глиноземистый полупродукт для выплавки синтетических шлаков. 1 з.п. ф-лы, 1 табл.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; rus |
recordid | cdi_epo_espacenet_RU2351678C2 |
source | esp@cenet |
subjects | ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | MELTING METHOD OF FERROTITANIUM |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T06%3A32%3A14IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KORZUN%20VIKTOR%20KAZIMIROVICH&rft.date=2009-04-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2351678C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |