METHOD FOR THREE-STAGE DRYING OF PELLETS IN CALCINING CONVEYOR MACHINE

FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to the field of iron-ore raw materials preparation in ferrous metallurgy, in particular to production of iron-ore pellets. Method for three-stage drying includes the first stage of drying with filtration of coolant with te...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NEVOLIN VLADIMIR NIKOLAEVICH, EVSTJUGIN SERGEJ NIKOLAEVICH, SOLODUKHIN ANDREJ ALEKSANDROVICH, KLEJN VIKTOR IVANOVICH, ABZALOV VADIM MANNAFOVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NEVOLIN VLADIMIR NIKOLAEVICH
EVSTJUGIN SERGEJ NIKOLAEVICH
SOLODUKHIN ANDREJ ALEKSANDROVICH
KLEJN VIKTOR IVANOVICH
ABZALOV VADIM MANNAFOVICH
description FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to the field of iron-ore raw materials preparation in ferrous metallurgy, in particular to production of iron-ore pellets. Method for three-stage drying includes the first stage of drying with filtration of coolant with temperature of 250-400°C bottom-up and two stages of drying with filtration of coolant bottom-up. At the first stage of drying, drying time makes 30-40 % from the total time of drying at filtration rate of 1.3-1.5 m/sec, and at the second and third stages of drying at every stage - by 30-35 % from total time of drying at the rate of filtration of 0.8-1.0 m/sec. Coolant temperature at the second and third stages makes 250-400°C and 500-800°C accordingly. ^ EFFECT: intensification of pellets layer drying process in three stages with maximum possible coolant parameters, optimal distribution of drying time at every stage depending on initial humidity of pellets and height of layer.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2350664C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2350664C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2350664C13</originalsourceid><addsrcrecordid>eNrjZHDzdQ3x8HdRcPMPUgjxCHJ11Q0OcXR3VXAJivT0c1fwd1MIcPXxcQ0JVvD0U3B29HH29AOJO_v7hblGAvX4Ojp7ePq58jCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQI2NTAzMzE2dDYyKUAABArCvW</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR THREE-STAGE DRYING OF PELLETS IN CALCINING CONVEYOR MACHINE</title><source>esp@cenet</source><creator>NEVOLIN VLADIMIR NIKOLAEVICH ; EVSTJUGIN SERGEJ NIKOLAEVICH ; SOLODUKHIN ANDREJ ALEKSANDROVICH ; KLEJN VIKTOR IVANOVICH ; ABZALOV VADIM MANNAFOVICH</creator><creatorcontrib>NEVOLIN VLADIMIR NIKOLAEVICH ; EVSTJUGIN SERGEJ NIKOLAEVICH ; SOLODUKHIN ANDREJ ALEKSANDROVICH ; KLEJN VIKTOR IVANOVICH ; ABZALOV VADIM MANNAFOVICH</creatorcontrib><description>FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to the field of iron-ore raw materials preparation in ferrous metallurgy, in particular to production of iron-ore pellets. Method for three-stage drying includes the first stage of drying with filtration of coolant with temperature of 250-400°C bottom-up and two stages of drying with filtration of coolant bottom-up. At the first stage of drying, drying time makes 30-40 % from the total time of drying at filtration rate of 1.3-1.5 m/sec, and at the second and third stages of drying at every stage - by 30-35 % from total time of drying at the rate of filtration of 0.8-1.0 m/sec. Coolant temperature at the second and third stages makes 250-400°C and 500-800°C accordingly. ^ EFFECT: intensification of pellets layer drying process in three stages with maximum possible coolant parameters, optimal distribution of drying time at every stage depending on initial humidity of pellets and height of layer.</description><language>eng ; rus</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090327&amp;DB=EPODOC&amp;CC=RU&amp;NR=2350664C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090327&amp;DB=EPODOC&amp;CC=RU&amp;NR=2350664C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NEVOLIN VLADIMIR NIKOLAEVICH</creatorcontrib><creatorcontrib>EVSTJUGIN SERGEJ NIKOLAEVICH</creatorcontrib><creatorcontrib>SOLODUKHIN ANDREJ ALEKSANDROVICH</creatorcontrib><creatorcontrib>KLEJN VIKTOR IVANOVICH</creatorcontrib><creatorcontrib>ABZALOV VADIM MANNAFOVICH</creatorcontrib><title>METHOD FOR THREE-STAGE DRYING OF PELLETS IN CALCINING CONVEYOR MACHINE</title><description>FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to the field of iron-ore raw materials preparation in ferrous metallurgy, in particular to production of iron-ore pellets. Method for three-stage drying includes the first stage of drying with filtration of coolant with temperature of 250-400°C bottom-up and two stages of drying with filtration of coolant bottom-up. At the first stage of drying, drying time makes 30-40 % from the total time of drying at filtration rate of 1.3-1.5 m/sec, and at the second and third stages of drying at every stage - by 30-35 % from total time of drying at the rate of filtration of 0.8-1.0 m/sec. Coolant temperature at the second and third stages makes 250-400°C and 500-800°C accordingly. ^ EFFECT: intensification of pellets layer drying process in three stages with maximum possible coolant parameters, optimal distribution of drying time at every stage depending on initial humidity of pellets and height of layer.</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHDzdQ3x8HdRcPMPUgjxCHJ11Q0OcXR3VXAJivT0c1fwd1MIcPXxcQ0JVvD0U3B29HH29AOJO_v7hblGAvX4Ojp7ePq58jCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQI2NTAzMzE2dDYyKUAABArCvW</recordid><startdate>20090327</startdate><enddate>20090327</enddate><creator>NEVOLIN VLADIMIR NIKOLAEVICH</creator><creator>EVSTJUGIN SERGEJ NIKOLAEVICH</creator><creator>SOLODUKHIN ANDREJ ALEKSANDROVICH</creator><creator>KLEJN VIKTOR IVANOVICH</creator><creator>ABZALOV VADIM MANNAFOVICH</creator><scope>EVB</scope></search><sort><creationdate>20090327</creationdate><title>METHOD FOR THREE-STAGE DRYING OF PELLETS IN CALCINING CONVEYOR MACHINE</title><author>NEVOLIN VLADIMIR NIKOLAEVICH ; EVSTJUGIN SERGEJ NIKOLAEVICH ; SOLODUKHIN ANDREJ ALEKSANDROVICH ; KLEJN VIKTOR IVANOVICH ; ABZALOV VADIM MANNAFOVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2350664C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2009</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>NEVOLIN VLADIMIR NIKOLAEVICH</creatorcontrib><creatorcontrib>EVSTJUGIN SERGEJ NIKOLAEVICH</creatorcontrib><creatorcontrib>SOLODUKHIN ANDREJ ALEKSANDROVICH</creatorcontrib><creatorcontrib>KLEJN VIKTOR IVANOVICH</creatorcontrib><creatorcontrib>ABZALOV VADIM MANNAFOVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NEVOLIN VLADIMIR NIKOLAEVICH</au><au>EVSTJUGIN SERGEJ NIKOLAEVICH</au><au>SOLODUKHIN ANDREJ ALEKSANDROVICH</au><au>KLEJN VIKTOR IVANOVICH</au><au>ABZALOV VADIM MANNAFOVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR THREE-STAGE DRYING OF PELLETS IN CALCINING CONVEYOR MACHINE</title><date>2009-03-27</date><risdate>2009</risdate><abstract>FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to the field of iron-ore raw materials preparation in ferrous metallurgy, in particular to production of iron-ore pellets. Method for three-stage drying includes the first stage of drying with filtration of coolant with temperature of 250-400°C bottom-up and two stages of drying with filtration of coolant bottom-up. At the first stage of drying, drying time makes 30-40 % from the total time of drying at filtration rate of 1.3-1.5 m/sec, and at the second and third stages of drying at every stage - by 30-35 % from total time of drying at the rate of filtration of 0.8-1.0 m/sec. Coolant temperature at the second and third stages makes 250-400°C and 500-800°C accordingly. ^ EFFECT: intensification of pellets layer drying process in three stages with maximum possible coolant parameters, optimal distribution of drying time at every stage depending on initial humidity of pellets and height of layer.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2350664C1
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title METHOD FOR THREE-STAGE DRYING OF PELLETS IN CALCINING CONVEYOR MACHINE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-26T18%3A51%3A32IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NEVOLIN%20VLADIMIR%20NIKOLAEVICH&rft.date=2009-03-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2350664C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true