METHOD FOR BLAST-FURNACE SMELTING ON MAGNESIA-ALUMINOUS SLAGS

FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to ferrous metallurgy and may be used in blast-furnace production. Method for smelting on magnesia-aluminous slags with content of Al2O3 and MgO from 5 to 20% of each component includes charge loading, insufflation of high...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GIL'MANOV MARAT RIMATOVICH, KUSHNAREV ALEKSEJ VLADISLAVOVICH, BOBROV VLADIMIR PAVLOVICH, SUKHAREV ANATOLIJ GRIGOR'EVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GIL'MANOV MARAT RIMATOVICH
KUSHNAREV ALEKSEJ VLADISLAVOVICH
BOBROV VLADIMIR PAVLOVICH
SUKHAREV ANATOLIJ GRIGOR'EVICH
description FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to ferrous metallurgy and may be used in blast-furnace production. Method for smelting on magnesia-aluminous slags with content of Al2O3 and MgO from 5 to 20% of each component includes charge loading, insufflation of high-temperature combined blast with application of aluminous and magnesia additives. Iron-ore charge is formed with silicon module SiO2/Al2O3 within the limits of 2.2-2.5 and with magnesia index of MgO/(CaO+MgO) within the limits of 0.30-0.35, and as a result low-sulfury cast iron is produced with lowered basicity of slag CaO/SiO2, equal to 0.78-0.92. ^ EFFECT: higher castable and sulfur-absorbing capacity of slag at its reduced basicity. ^ 2 tbl
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2350658C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2350658C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2350658C23</originalsourceid><addsrcrecordid>eNrjZLD1dQ3x8HdRcPMPUnDycQwO0XULDfJzdHZVCPZ19Qnx9HNX8PdT8HV093MN9nTUdfQJ9fX08w8NVgj2cXQP5mFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8UGhRsamBmamFs5GxkQoAQDjjSmo</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR BLAST-FURNACE SMELTING ON MAGNESIA-ALUMINOUS SLAGS</title><source>esp@cenet</source><creator>GIL'MANOV MARAT RIMATOVICH ; KUSHNAREV ALEKSEJ VLADISLAVOVICH ; BOBROV VLADIMIR PAVLOVICH ; SUKHAREV ANATOLIJ GRIGOR'EVICH</creator><creatorcontrib>GIL'MANOV MARAT RIMATOVICH ; KUSHNAREV ALEKSEJ VLADISLAVOVICH ; BOBROV VLADIMIR PAVLOVICH ; SUKHAREV ANATOLIJ GRIGOR'EVICH</creatorcontrib><description>FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to ferrous metallurgy and may be used in blast-furnace production. Method for smelting on magnesia-aluminous slags with content of Al2O3 and MgO from 5 to 20% of each component includes charge loading, insufflation of high-temperature combined blast with application of aluminous and magnesia additives. Iron-ore charge is formed with silicon module SiO2/Al2O3 within the limits of 2.2-2.5 and with magnesia index of MgO/(CaO+MgO) within the limits of 0.30-0.35, and as a result low-sulfury cast iron is produced with lowered basicity of slag CaO/SiO2, equal to 0.78-0.92. ^ EFFECT: higher castable and sulfur-absorbing capacity of slag at its reduced basicity. ^ 2 tbl</description><language>eng ; rus</language><subject>CHEMISTRY ; MANUFACTURE OF IRON OR STEEL ; METALLURGY ; METALLURGY OF IRON</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090327&amp;DB=EPODOC&amp;CC=RU&amp;NR=2350658C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090327&amp;DB=EPODOC&amp;CC=RU&amp;NR=2350658C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GIL'MANOV MARAT RIMATOVICH</creatorcontrib><creatorcontrib>KUSHNAREV ALEKSEJ VLADISLAVOVICH</creatorcontrib><creatorcontrib>BOBROV VLADIMIR PAVLOVICH</creatorcontrib><creatorcontrib>SUKHAREV ANATOLIJ GRIGOR'EVICH</creatorcontrib><title>METHOD FOR BLAST-FURNACE SMELTING ON MAGNESIA-ALUMINOUS SLAGS</title><description>FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to ferrous metallurgy and may be used in blast-furnace production. Method for smelting on magnesia-aluminous slags with content of Al2O3 and MgO from 5 to 20% of each component includes charge loading, insufflation of high-temperature combined blast with application of aluminous and magnesia additives. Iron-ore charge is formed with silicon module SiO2/Al2O3 within the limits of 2.2-2.5 and with magnesia index of MgO/(CaO+MgO) within the limits of 0.30-0.35, and as a result low-sulfury cast iron is produced with lowered basicity of slag CaO/SiO2, equal to 0.78-0.92. ^ EFFECT: higher castable and sulfur-absorbing capacity of slag at its reduced basicity. ^ 2 tbl</description><subject>CHEMISTRY</subject><subject>MANUFACTURE OF IRON OR STEEL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLD1dQ3x8HdRcPMPUnDycQwO0XULDfJzdHZVCPZ19Qnx9HNX8PdT8HV093MN9nTUdfQJ9fX08w8NVgj2cXQP5mFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8UGhRsamBmamFs5GxkQoAQDjjSmo</recordid><startdate>20090327</startdate><enddate>20090327</enddate><creator>GIL'MANOV MARAT RIMATOVICH</creator><creator>KUSHNAREV ALEKSEJ VLADISLAVOVICH</creator><creator>BOBROV VLADIMIR PAVLOVICH</creator><creator>SUKHAREV ANATOLIJ GRIGOR'EVICH</creator><scope>EVB</scope></search><sort><creationdate>20090327</creationdate><title>METHOD FOR BLAST-FURNACE SMELTING ON MAGNESIA-ALUMINOUS SLAGS</title><author>GIL'MANOV MARAT RIMATOVICH ; KUSHNAREV ALEKSEJ VLADISLAVOVICH ; BOBROV VLADIMIR PAVLOVICH ; SUKHAREV ANATOLIJ GRIGOR'EVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2350658C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2009</creationdate><topic>CHEMISTRY</topic><topic>MANUFACTURE OF IRON OR STEEL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><toplevel>online_resources</toplevel><creatorcontrib>GIL'MANOV MARAT RIMATOVICH</creatorcontrib><creatorcontrib>KUSHNAREV ALEKSEJ VLADISLAVOVICH</creatorcontrib><creatorcontrib>BOBROV VLADIMIR PAVLOVICH</creatorcontrib><creatorcontrib>SUKHAREV ANATOLIJ GRIGOR'EVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GIL'MANOV MARAT RIMATOVICH</au><au>KUSHNAREV ALEKSEJ VLADISLAVOVICH</au><au>BOBROV VLADIMIR PAVLOVICH</au><au>SUKHAREV ANATOLIJ GRIGOR'EVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR BLAST-FURNACE SMELTING ON MAGNESIA-ALUMINOUS SLAGS</title><date>2009-03-27</date><risdate>2009</risdate><abstract>FIELD: technological processes; metallurgy. ^ SUBSTANCE: invention is related to ferrous metallurgy and may be used in blast-furnace production. Method for smelting on magnesia-aluminous slags with content of Al2O3 and MgO from 5 to 20% of each component includes charge loading, insufflation of high-temperature combined blast with application of aluminous and magnesia additives. Iron-ore charge is formed with silicon module SiO2/Al2O3 within the limits of 2.2-2.5 and with magnesia index of MgO/(CaO+MgO) within the limits of 0.30-0.35, and as a result low-sulfury cast iron is produced with lowered basicity of slag CaO/SiO2, equal to 0.78-0.92. ^ EFFECT: higher castable and sulfur-absorbing capacity of slag at its reduced basicity. ^ 2 tbl</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2350658C2
source esp@cenet
subjects CHEMISTRY
MANUFACTURE OF IRON OR STEEL
METALLURGY
METALLURGY OF IRON
title METHOD FOR BLAST-FURNACE SMELTING ON MAGNESIA-ALUMINOUS SLAGS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T06%3A16%3A05IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GIL'MANOV%20MARAT%20RIMATOVICH&rft.date=2009-03-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2350658C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true