METHOD OF LITHIATED COBALTOUS OXIDE SYNTHESIS
FIELD: chemistry. ^ SUBSTANCE: initial mixture is added with at least dopant as MgO, TiO2 and Al2O3 in total within 0.5 to 5.0% (wt) in ratio to initial mixture weight. Annealing is two-staged: the first stage includes annealing of initial mixture at temperature 600-800°C; then produced furnace feed...