METHOD OF LITHIATED COBALTOUS OXIDE SYNTHESIS

FIELD: chemistry. ^ SUBSTANCE: initial mixture is added with at least dopant as MgO, TiO2 and Al2O3 in total within 0.5 to 5.0% (wt) in ratio to initial mixture weight. Annealing is two-staged: the first stage includes annealing of initial mixture at temperature 600-800°C; then produced furnace feed...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ROZHKOV VLADIMIR VLADIMIROVICH, REZVOV SERGEJ ANATOL'EVICH, MUKHIN VIKTOR VASIL'EVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: chemistry. ^ SUBSTANCE: initial mixture is added with at least dopant as MgO, TiO2 and Al2O3 in total within 0.5 to 5.0% (wt) in ratio to initial mixture weight. Annealing is two-staged: the first stage includes annealing of initial mixture at temperature 600-800°C; then produced furnace feed is mixed and annealed at temperature 800-1000°C. ^ EFFECT: lower power inputs and improved synthesis process. ^ 6 dwg, 4 ex