METHOD OF PRODUCING THERMALLY OXIDISED FIBRE FROM POLYACRYLONIRILE AND ITS CO-POLYMERS

FIELD: chemistry. ^ SUBSTANCE: invention relates to technology of producing thermally oxidised fibres from polyacrylonitrile and its co-polymers, which can be used, for instance, as semi-product for their further processing into carbon fibres. Method includes passing polymer solution in organic solv...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MASHCHENKO VLADIMIR IGOREVICH, MALAKHO ARTEM PETROVICH, UDRA SERGEJ ALEKSANDROVICH, OLENIN ALEKSANDR VLADIMIROVICH, SELEZNEV ANATOLIJ NIKOLAEVICH, GERASIMOV VASILIJ IVANOVICH, SHASHKEEV KONSTANTIN ALEKSANDROVICH, AVDEEV VIKTOR VASIL'EVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MASHCHENKO VLADIMIR IGOREVICH
MALAKHO ARTEM PETROVICH
UDRA SERGEJ ALEKSANDROVICH
OLENIN ALEKSANDR VLADIMIROVICH
SELEZNEV ANATOLIJ NIKOLAEVICH
GERASIMOV VASILIJ IVANOVICH
SHASHKEEV KONSTANTIN ALEKSANDROVICH
AVDEEV VIKTOR VASIL'EVICH
description FIELD: chemistry. ^ SUBSTANCE: invention relates to technology of producing thermally oxidised fibres from polyacrylonitrile and its co-polymers, which can be used, for instance, as semi-product for their further processing into carbon fibres. Method includes passing polymer solution in organic solvent through spinneret with further stages of fibre stretching, removal solvent from it and thermal oxidation in presence of oxidant with heating. Before passing polymer through spinneret, at least one cyclic alkylenecarbonate is introduced into solution, in amount 0.2-20 wt % from solution weight. Obtained solution is heated, at least during 6 min within temperature range from 80°C to temperature of solvent boiling. Fibre stretching stage can be carried out after removal of solvent from fibre, as well as before removal solvent from fibre and after its removal. ^ EFFECT: reduction of duration of fibre thermal oxidation stage 8-15 min with preservation of high operational characteristics of produced fibre. ^ 6 ex
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2338015C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2338015C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2338015C13</originalsourceid><addsrcrecordid>eNqNykEKwjAQQNFuXIh6h7lAwRoEtzWZmIGkU6ZpMatSJK5EC_X-iOABXP3F--tiCBgdG2ALrbDpNTUXiA4l1N4n4CsZ6tCApbMgWOEALftUa0meGxLyCHVjgGIHmsuvBZRuW6zu02PJu183BViM2pV5fo15madbfub3KP1BqdO-OupK_bF8AFTSMK8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF PRODUCING THERMALLY OXIDISED FIBRE FROM POLYACRYLONIRILE AND ITS CO-POLYMERS</title><source>esp@cenet</source><creator>MASHCHENKO VLADIMIR IGOREVICH ; MALAKHO ARTEM PETROVICH ; UDRA SERGEJ ALEKSANDROVICH ; OLENIN ALEKSANDR VLADIMIROVICH ; SELEZNEV ANATOLIJ NIKOLAEVICH ; GERASIMOV VASILIJ IVANOVICH ; SHASHKEEV KONSTANTIN ALEKSANDROVICH ; AVDEEV VIKTOR VASIL'EVICH</creator><creatorcontrib>MASHCHENKO VLADIMIR IGOREVICH ; MALAKHO ARTEM PETROVICH ; UDRA SERGEJ ALEKSANDROVICH ; OLENIN ALEKSANDR VLADIMIROVICH ; SELEZNEV ANATOLIJ NIKOLAEVICH ; GERASIMOV VASILIJ IVANOVICH ; SHASHKEEV KONSTANTIN ALEKSANDROVICH ; AVDEEV VIKTOR VASIL'EVICH</creatorcontrib><description>FIELD: chemistry. ^ SUBSTANCE: invention relates to technology of producing thermally oxidised fibres from polyacrylonitrile and its co-polymers, which can be used, for instance, as semi-product for their further processing into carbon fibres. Method includes passing polymer solution in organic solvent through spinneret with further stages of fibre stretching, removal solvent from it and thermal oxidation in presence of oxidant with heating. Before passing polymer through spinneret, at least one cyclic alkylenecarbonate is introduced into solution, in amount 0.2-20 wt % from solution weight. Obtained solution is heated, at least during 6 min within temperature range from 80°C to temperature of solvent boiling. Fibre stretching stage can be carried out after removal of solvent from fibre, as well as before removal solvent from fibre and after its removal. ^ EFFECT: reduction of duration of fibre thermal oxidation stage 8-15 min with preservation of high operational characteristics of produced fibre. ^ 6 ex</description><language>eng ; rus</language><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS ; CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS ; NATURAL OR ARTIFICIAL THREADS OR FIBRES ; SPINNING ; TEXTILES</subject><creationdate>2008</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20081110&amp;DB=EPODOC&amp;CC=RU&amp;NR=2338015C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20081110&amp;DB=EPODOC&amp;CC=RU&amp;NR=2338015C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MASHCHENKO VLADIMIR IGOREVICH</creatorcontrib><creatorcontrib>MALAKHO ARTEM PETROVICH</creatorcontrib><creatorcontrib>UDRA SERGEJ ALEKSANDROVICH</creatorcontrib><creatorcontrib>OLENIN ALEKSANDR VLADIMIROVICH</creatorcontrib><creatorcontrib>SELEZNEV ANATOLIJ NIKOLAEVICH</creatorcontrib><creatorcontrib>GERASIMOV VASILIJ IVANOVICH</creatorcontrib><creatorcontrib>SHASHKEEV KONSTANTIN ALEKSANDROVICH</creatorcontrib><creatorcontrib>AVDEEV VIKTOR VASIL'EVICH</creatorcontrib><title>METHOD OF PRODUCING THERMALLY OXIDISED FIBRE FROM POLYACRYLONIRILE AND ITS CO-POLYMERS</title><description>FIELD: chemistry. ^ SUBSTANCE: invention relates to technology of producing thermally oxidised fibres from polyacrylonitrile and its co-polymers, which can be used, for instance, as semi-product for their further processing into carbon fibres. Method includes passing polymer solution in organic solvent through spinneret with further stages of fibre stretching, removal solvent from it and thermal oxidation in presence of oxidant with heating. Before passing polymer through spinneret, at least one cyclic alkylenecarbonate is introduced into solution, in amount 0.2-20 wt % from solution weight. Obtained solution is heated, at least during 6 min within temperature range from 80°C to temperature of solvent boiling. Fibre stretching stage can be carried out after removal of solvent from fibre, as well as before removal solvent from fibre and after its removal. ^ EFFECT: reduction of duration of fibre thermal oxidation stage 8-15 min with preservation of high operational characteristics of produced fibre. ^ 6 ex</description><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</subject><subject>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</subject><subject>NATURAL OR ARTIFICIAL THREADS OR FIBRES</subject><subject>SPINNING</subject><subject>TEXTILES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2008</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNykEKwjAQQNFuXIh6h7lAwRoEtzWZmIGkU6ZpMatSJK5EC_X-iOABXP3F--tiCBgdG2ALrbDpNTUXiA4l1N4n4CsZ6tCApbMgWOEALftUa0meGxLyCHVjgGIHmsuvBZRuW6zu02PJu183BViM2pV5fo15madbfub3KP1BqdO-OupK_bF8AFTSMK8</recordid><startdate>20081110</startdate><enddate>20081110</enddate><creator>MASHCHENKO VLADIMIR IGOREVICH</creator><creator>MALAKHO ARTEM PETROVICH</creator><creator>UDRA SERGEJ ALEKSANDROVICH</creator><creator>OLENIN ALEKSANDR VLADIMIROVICH</creator><creator>SELEZNEV ANATOLIJ NIKOLAEVICH</creator><creator>GERASIMOV VASILIJ IVANOVICH</creator><creator>SHASHKEEV KONSTANTIN ALEKSANDROVICH</creator><creator>AVDEEV VIKTOR VASIL'EVICH</creator><scope>EVB</scope></search><sort><creationdate>20081110</creationdate><title>METHOD OF PRODUCING THERMALLY OXIDISED FIBRE FROM POLYACRYLONIRILE AND ITS CO-POLYMERS</title><author>MASHCHENKO VLADIMIR IGOREVICH ; MALAKHO ARTEM PETROVICH ; UDRA SERGEJ ALEKSANDROVICH ; OLENIN ALEKSANDR VLADIMIROVICH ; SELEZNEV ANATOLIJ NIKOLAEVICH ; GERASIMOV VASILIJ IVANOVICH ; SHASHKEEV KONSTANTIN ALEKSANDROVICH ; AVDEEV VIKTOR VASIL'EVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2338015C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2008</creationdate><topic>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</topic><topic>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</topic><topic>NATURAL OR ARTIFICIAL THREADS OR FIBRES</topic><topic>SPINNING</topic><topic>TEXTILES</topic><toplevel>online_resources</toplevel><creatorcontrib>MASHCHENKO VLADIMIR IGOREVICH</creatorcontrib><creatorcontrib>MALAKHO ARTEM PETROVICH</creatorcontrib><creatorcontrib>UDRA SERGEJ ALEKSANDROVICH</creatorcontrib><creatorcontrib>OLENIN ALEKSANDR VLADIMIROVICH</creatorcontrib><creatorcontrib>SELEZNEV ANATOLIJ NIKOLAEVICH</creatorcontrib><creatorcontrib>GERASIMOV VASILIJ IVANOVICH</creatorcontrib><creatorcontrib>SHASHKEEV KONSTANTIN ALEKSANDROVICH</creatorcontrib><creatorcontrib>AVDEEV VIKTOR VASIL'EVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MASHCHENKO VLADIMIR IGOREVICH</au><au>MALAKHO ARTEM PETROVICH</au><au>UDRA SERGEJ ALEKSANDROVICH</au><au>OLENIN ALEKSANDR VLADIMIROVICH</au><au>SELEZNEV ANATOLIJ NIKOLAEVICH</au><au>GERASIMOV VASILIJ IVANOVICH</au><au>SHASHKEEV KONSTANTIN ALEKSANDROVICH</au><au>AVDEEV VIKTOR VASIL'EVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF PRODUCING THERMALLY OXIDISED FIBRE FROM POLYACRYLONIRILE AND ITS CO-POLYMERS</title><date>2008-11-10</date><risdate>2008</risdate><abstract>FIELD: chemistry. ^ SUBSTANCE: invention relates to technology of producing thermally oxidised fibres from polyacrylonitrile and its co-polymers, which can be used, for instance, as semi-product for their further processing into carbon fibres. Method includes passing polymer solution in organic solvent through spinneret with further stages of fibre stretching, removal solvent from it and thermal oxidation in presence of oxidant with heating. Before passing polymer through spinneret, at least one cyclic alkylenecarbonate is introduced into solution, in amount 0.2-20 wt % from solution weight. Obtained solution is heated, at least during 6 min within temperature range from 80°C to temperature of solvent boiling. Fibre stretching stage can be carried out after removal of solvent from fibre, as well as before removal solvent from fibre and after its removal. ^ EFFECT: reduction of duration of fibre thermal oxidation stage 8-15 min with preservation of high operational characteristics of produced fibre. ^ 6 ex</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2338015C1
source esp@cenet
subjects APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS
CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS
NATURAL OR ARTIFICIAL THREADS OR FIBRES
SPINNING
TEXTILES
title METHOD OF PRODUCING THERMALLY OXIDISED FIBRE FROM POLYACRYLONIRILE AND ITS CO-POLYMERS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-12T12%3A13%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MASHCHENKO%20VLADIMIR%20IGOREVICH&rft.date=2008-11-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2338015C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true