METHOD OF IODIDE REFINING OF HAFNIUM

FIELD: iodide refining of hafnium. ^ SUBSTANCE: interaction of iodine with black metal is carried out at temperature of 250-350°C. Sedimentation of refined hafnium is carried out at temperature of 1200-1600°C on heater (filament) made from molybdenum or zirconium wire in form of one or several loops...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SINEGRIBOV VIKTOR ANDREEVICH, MORENKO OL'GA GRIGOR'EVNA, SHTUTSA MIKHAIL GEORGIEVICH, POGADAEV VLADIMIR ARKAD'EVICH, JUDINA TAT'JANA BORISOVNA, INDYK SERGEJ IVANOVICH, SOTSKOV KONSTANTIN VJACHESLAVOVICH, PIMENOV JURIJ VLADIMIROVICH, KOTSAR' MIKHAIL LEONIDOVICH, CHEREMNYKH GENNADIJ SERGEEVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:FIELD: iodide refining of hafnium. ^ SUBSTANCE: interaction of iodine with black metal is carried out at temperature of 250-350°C. Sedimentation of refined hafnium is carried out at temperature of 1200-1600°C on heater (filament) made from molybdenum or zirconium wire in form of one or several loops connected to electrode end-pieces. Heater is formed in iodide refining apparatus in such way that lower part of each wire loop is suspended above insulator surface at clearance equal to 1/3-1/2 of final thickness of bar. Proposed method may be used for production of iodide hafnium bars more than 17 mm in diameter at height of heater loop more than 0.8 m. ^ EFFECT: enhanced purity by admixtures. ^ 4 cl, 1 tbl, 3 ex